How the Calculation Works

Enter a weight in gsm, US Text lb, or US Cover lb. Each US basis weight is the mass of 500 sheets at its own reference sheet size. Multiply pounds by the corresponding factor to convert back to gsm.

US Cover lb = gsm ÷ 2.7048 · US Text lb = gsm ÷ 1.4805

Worked Examples

  • 300 gsm equals 110.9139 lb US Cover (20 × 26 in) or 202.6342 lb US Text (25 × 38 in).
  • 100 lb US Cover equals 270.48 gsm.