All specifications, dimensional baselines, and browser calculators published on Card Deck Press are open to creators, publishers, and buyers preparing files for any offset printing provider. For specification inquiries or technical errata, reach us at hello@carddeckpress.com.
Because card format and trim dimensions vary by project, sheet imposition, corner-rounding dies (R3–R3.5 mm / 0.118–0.138 in), and box cavity sizing follow the locked BOM rather than a single default trim. Deck count, stock caliper, and double-sided film thickness determine stack height, which in turn sets tuck or rigid box dimensions and insert tolerances.
Complete Bill of Materials & Component Specifications
Paper Weight Basis & Unit Conventions
Specify paper and board weights in grams per square meter (gsm), paired with metric (mm) and imperial (in) calipers. When converting or referencing US pound weights (LB), distinguish grades by basis sheet size:
- US Text LB: Measured on a
25 x 38 in(635 x 965.2 mm) basis sheet. Used for booklet interiors and thin paper extras. - US Cover LB: Measured on a
20 x 26 in(508 x 660.4 mm) basis sheet. Used for card stocks, booklet covers, and box wraps. An identicalLBnumber in Cover weight is substantially thicker and heavier ingsmthan the sameLBnumber in Text weight.
Track finished component and carton weights in both kilograms (kg) and pounds (lb) using 1 kg = 2.2046 lb to verify shipping cartons and component BOM totals.
Card Stocks, Cores & Finishes
| Component / Stock | Weight | Approximate Caliper (mm) |
Approximate Caliper (in) |
Typical Application & Constraints |
|---|---|---|---|---|
| Art paper / Blue core | 300 gsm |
0.28–0.31 mm |
0.0110–0.0122 in |
Standard promotional and entry-level playing or game decks |
| Black-core linen | 310 gsm |
0.30–0.32 mm |
0.0118–0.0126 in |
Textured shuffle-grade decks requiring high opacity |
| Black core | 330 gsm |
0.32–0.34 mm |
0.0126–0.0134 in |
Heavy tournament and tabletop card decks |
| Art stock (heavy) | 350 gsm |
0.34–0.38 mm |
0.0134–0.0150 in |
Thick non-playing cards, dividers, and rigid reference cards |
| Art stock (extra-heavy) | 400 gsm |
0.40–0.44 mm |
0.0157–0.0173 in |
Heavy display cards, tiles, and rigid inserts |
| PVC | — | 0.30 mm |
0.0118 in |
Waterproof, high-flexibility plastic decks |
| Double-sided film lamination | — | +0.03–0.05 mm |
+0.0012–0.0020 in |
Added per card; must be included in stack-height math |
- Finish selection: Anti-scuff matte lamination suits dark artwork where standard matte shows rub marks during handling and transit.
- Edge finishing conflict: Thick lamination (
0.03–0.05 mm/0.0012–0.0020 intotal film buildup) can conflict with gilded edges because heavy film resists clean edge adhesion and trimming.
Boards, Punchboards, Puzzles & Paper Extras
| Component | Material / Spec | Metric (mm) |
Imperial (in) |
Production Requirement |
|---|---|---|---|---|
| Game boards & rigid box walls | Greyboard | 1.5 / 2 / 2.5 / 3 mm |
0.059 / 0.079 / 0.098 / 0.118 in |
Selected by board span and folding/lid rigidity |
| Rigid board & box wraps | Printed wrap paper | 15–20 mm margin |
0.591–0.787 in margin |
Required turn-in allowance around greyboard edges |
| Punchboard token sheets | Greyboard + printed liners | 3–4 mm die gap |
0.118–0.157 in die gap |
Minimum clearance between adjacent die-cut tokens |
| Booster packs, puzzles & paper extras | Custom printed paper/board | Project-specific | Project-specific | Follow partner tooling and kitting minimums |
Boxes, Inserts & Clearance Math
Box cavities and tray inserts must accommodate both manufacturing tolerances and cumulative film thickness. Build clearance directly into the dieline:
- Width and height clearance:
1.5–2.5 mm(0.059–0.098 in) across internal box width and length/height. - Stack height clearance:
1.5–3 mm(0.059–0.118 in) above the resting card deck or component stack.
Calculate total deck stack height before locking box or insert cavity depth:
Deck Stack Height (mm) = Card Count * (Base Card Caliper + Film Thickness per Card)
Inner Cavity Depth (mm) = Deck Stack Height (mm) + 1.5 to 3.0 mm
Partner-sourced game pieces (such as dice, wooden tokens, plastic miniatures, or metal coins) are measured prior to insert tooling so cavity walls hold components securely without exceeding outer box dimensions.
Booklets & Leaflets
| Format | Page / Panel Structure | Interior Stock | Cover Stock | Binding / Folding Notes |
|---|---|---|---|---|
| Folded leaflets | 4, 6, or 8 panels |
80–120 gsm (0.08–0.13 mm / 0.0031–0.0051 in per sheet) |
Self-cover | Scored folds; fits inside compact tuck or rigid boxes |
| Saddle-stitched booklets | 12–40 pages (multiples of 4) |
80–120 gsm (0.08–0.13 mm / 0.0031–0.0051 in per sheet) |
200–300 gsm |
Wire-stitched spine; outer pages must account for creep |
| Perfect-bound rulebooks | 28+ pages (multiples of 4) |
80–120 gsm (0.08–0.13 mm / 0.0031–0.0051 in per sheet) |
200–300 gsm |
Milled and glued spine; requires spine-width calculation |
| Sewn-bound rulebooks | 80–100+ pages recommended (multiples of 4) |
80–120 gsm (0.08–0.13 mm / 0.0031–0.0051 in per sheet) |
200–300 gsm |
Smyth-sewn signatures for flat lay and heavy table use |
Prepress & File Preparation Standards
Prepare all print-ready artwork in Adobe Illustrator (AI), PDF, or Adobe Photoshop (PSD), exported to PDF/X-1a or PDF/X-4 standards:
- Color mode & spot channels:
CMYKprocess build with separate named spot layers for foil, spot UV, embossing, or die-lines. - Resolution:
>=300 DPIat 100% print size for all raster images and flattened effects. - Bleed & safety margins:
- Bleed:
3 mm(0.118 in) per side beyond trim. - Standard safety margin:
>=3 mm(>=0.118 in) inside trim for text and critical graphics. - Bordered card backs:
>=4–5 mm(0.157–0.197 in) safety margin to absorb sheet-to-die registration variance.
- Bleed:
- Corner radius:
R3–R3.5 mm(0.118–0.138 in) for rounded card corners. - Typography & black builds:
- Outline all fonts or embed full font subsets.
- Fine text and rules:
100% Konly (no CMYK rich black on small type). - Rich black solids:
C40–60 M30–40 Y30–40 K100. - Total Area Coverage (TAC):
<=280%–300%across all channels.
Production Steps & Sign-Off Criteria
- BOM Lock & Dieline Engineering: Confirm component list, card stock
gsmand core, board thickness (1.5–3 mm/0.059–0.118 in), partner-sourced pieces, and exact cavity clearances (1.5–2.5 mm/0.059–0.098 inwidth/height;1.5–3 mm/0.059–0.118 instack height).- Sign-off: Master BOM and CAD dielines approved against measured stack-height calculations and partner piece dimensions.
- Prepress & Color Proofing: Preflight
PDF/X-1aorPDF/X-4files for>=300 DPIresolution,3 mm(0.118 in) bleed, spot layer separation,100% Kfine text, and<=280%–300%TAC.- Sign-off: Digital imposition proof and color proof approved before plate making.
- Offset Printing, Finishing & Die-Cutting: Print card sheets, booklet signatures, and board wraps; apply anti-scuff matte or specified coatings; die-cut cards (
R3–R3.5 mm/0.118–0.138 incorners) and punchboards (3–4 mm/0.118–0.157 indie gaps).- Sign-off: Sheet registration, coating cure, and clean die release verified on press samples.
- Board Wrapping, Binding & Kitting: Wrap greyboard using
15–20 mm(0.591–0.787 in) turn-in margins; bind booklets in multiples of4; collate cards, boosters, puzzles, paper extras, and partner-sourced pieces into inserts and boxes.- Sign-off: White-sample or pre-production assembly check confirming smooth card draw, lid fit, zero rattle or crush, and complete BOM kitting.
Regulatory & Market Compliance Procedures
Compliance requirements depend on target market, age grading, and packaging materials. Maintain source records and test documentation for each applicable jurisdiction without assuming blanket coverage:
- EN 71 / EU Toy Safety Assessment and Testing: Products marketed or classified for children's play in the EU require age-grade assessment, chemical/mechanical testing against applicable EN 71 parts, technical documentation, and Declaration of Conformity records per the European Commission Toy Safety framework.
- VerpackG (Germany Packaging Act): Placing packaged goods onto the German market triggers producer registration, system participation, and packaging weight data reporting (
kg/lbby material fraction) through the Stiftung Zentrale Stelle Verpackungsregister (ZSVR). - Triman & Info-tri (France): Consumer-facing packaging distributed in France requires Triman marking and material-specific sorting instructions following the French Ministry of Ecology Info-tri guidelines.
Concrete Failure Modes
- Visible border skew on card backs: Occurs when bordered backs use
<4–5 mm(<0.157–0.197 in) safety margins and normal press/die-cutting registration variance shifts one edge narrower than the opposite side. - Box lid binding or crushed corners: Occurs when inner box dimensions omit
1.5–2.5 mm(0.059–0.098 in) width/height clearance or1.5–3 mm(0.059–0.118 in) stack-height clearance, or when+0.03–0.05 mm(+0.0012–0.0020 in) per card for double-sided film is left out of stack-height math. - Gilded edge peeling or flaking: Occurs when thick lamination is paired with metallic edge gilding, preventing clean foil adhesion along the trimmed card edge.
- Scuffing and ink set-off on dark cards: Occurs when dark
CMYKartwork exceeds280%–300%TAC or uses standard matte instead of anti-scuff matte lamination. - Delaminated wrap edges on rigid boards: Occurs when greyboard wraps use
<15–20 mm(<0.591–0.787 in) turn-in margins, leaving insufficient glue surface on1.5–3 mm(0.059–0.118 in) greyboard. - Punchboard tearing or crushed token edges: Occurs when token layouts place die-cut blades closer than
3–4 mm(0.118–0.157 in), collapsing the greyboard bridge between adjacent pieces. - Booklet spine cracking or blank pages: Occurs when page counts are not multiples of
4, saddle stitching is pushed past40pages, or perfect binding is forced below28pages.