Concrete Component Selection Rules
- Shuffled decks vs. static cards: Choose 300–330 gsm cored stocks (blue core or black core) for opaque, snap-recovery play decks; step up to 350–400 gsm art stock for non-shuffled reference cards, dividers, or heavy tiles, or 0.30 mm (0.012 in) PVC where waterproof durability outweighs paper grain.
- Paper weight notation: Specify stock in gsm rather than US pound (lb) weights alone. US Text LB and Cover LB use different basis sheet sizes, so an identical pound number represents a much lighter, thinner sheet in Text LB than in Cover LB.
- Board and box rigidity: Match greyboard thickness (1.5–3 mm / 0.059–0.118 in) to span width and packed component weight in kg (lb); heavier board stacks, wooden pieces, or metal tokens require thicker greyboard walls and reinforced trays.
- Booklet binding by signature count: Keep folded leaflets to 4, 6, or 8 panels; format bound rulebooks in multiples of 4 pages, switching from saddle stitch (12–40 pages) to perfect binding (28+ pages) or sewn binding (80–100+ pages recommended) as spine thickness grows.
Material, Core, and Structural Specifications
Card Stocks, Cores, and Finishes
| Stock / Core | Weight | Approximate Caliper | Primary Application & Finish Notes |
|---|---|---|---|
| Art / Blue-Core Card Stock | 300 gsm | 0.28–0.31 mm (0.011–0.012 in) | Standard promotional and light-play decks; opaque blue adhesive layer. |
| Black-Core Linen Stock | 310 gsm | 0.30–0.32 mm (0.012–0.013 in) | Textured shuffling decks; linen emboss reduces surface friction. |
| Black-Core Card Stock | 330 gsm | 0.32–0.34 mm (0.013 in) | High-opacity tournament and tabletop decks; strong snap recovery. |
| Art Card Stock | 350 gsm | 0.34–0.38 mm (0.013–0.015 in) | Reference cards, dividers, and light game cards without heavy shuffling. |
| Heavy Art Stock | 400 gsm | 0.40–0.44 mm (0.016–0.017 in) | Rigid tokens, dividers, and standee cards. |
| PVC Plastic | — | 0.30 mm (0.012 in) | Waterproof, tear-resistant decks. |
- Lamination & coating buildup: Double-sided film lamination adds 0.03–0.05 mm (0.001–0.002 in) per card. Calculate total deck stack height after lamination rather than from raw board caliper.
- Surface & edge compatibility: Anti-scuff matte lamination suits dark artwork where gloss or standard matte shows rub marks. Thick film lamination can conflict with gilded edges because edge foil adheres poorly over heavy plastic film edges.
- Corner geometry: Standard die-cut card corners use a R3–R3.5 mm (0.118–0.138 in) radius; square corners or custom die shapes require dedicated tooling.
Boards, Punchboards, Boxes, and Inserts
- Greyboard calipers: 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), and 3 mm (0.118 in).
- Wrap margin: 15–20 mm (0.591–0.787 in) printed paper wrap turn-in around greyboard edges for game boards and rigid setup boxes.
- Punchboard die gap: Maintain 3–4 mm (0.118–0.157 in) minimum clearance between adjacent punchable token dies and from sheet edges so the waste matrix stays intact until punch-out.
- Box and insert clearance:
- Width and height clearance: 1.5–2.5 mm (0.059–0.098 in)
- Stack height clearance: 1.5–3 mm (0.059–0.118 in)
- Sizing formula:
Box Interior Width = Component Width + (1.5 to 2.5 mm)andBox Interior Depth = Total Stack Height + (1.5 to 3 mm)(add 0.059–0.098 in in width/height and 0.059–0.118 in in depth).
- Boosters, puzzles, and paper extras: Foil or paper booster packs, die-cut jigsaw puzzles, player mats, and scorepads follow the same bleed, caliper, and box-clearance rules so stacked extras do not bow lid walls.
Rulebooks, Booklets, and Leaflets
- Leaflets: 4, 6, or 8 panels (bi-fold, tri-fold, or accordion/gatefold).
- Bound booklets (multiples of 4 pages):
- Saddle stitch: 12–40 pages
- Perfect binding: 28+ pages
- Sewn binding: 80–100+ pages recommended for flat-lay durability under repeated table use
- Paper stocks: 80–120 gsm interior pages at approximately 0.08–0.13 mm (0.003–0.005 in) per sheet; 200–300 gsm covers.
- Spine allowance:
Booklet Stack Thickness = (Page Count / 2) * Sheet Caliper + (2 * Cover Caliper)before adding box depth clearance.
Partner-Sourced Non-Paper Game Pieces
Wooden meeples and cubes, injection-molded plastic or resin miniatures, metal coins, acrylic markers, dice, and custom trays are sourced through specialist manufacturing partners. Because non-paper pieces carry process-specific shrinkage, draft angles, and dimensional tolerances, verify actual sample dimensions and combined component weight in kg (lb) before locking insert cavities and rigid box wall thickness.
Prepress and Production Workflow
Prepress File Specifications
- Formats: AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
- Color & ink limits: CMYK process colors with separate named spot layers for foil, spot UV, embossing, or die lines. Keep fine text at 100% K only. Use rich black (
C40–60 M30–40 Y30–40 K100) for large dark solids, keeping Total Area Coverage (TAC) at ≤280%–300%. - Resolution & geometry: ≥300 DPI for all raster artwork; 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) safety margin from trim, increasing to ≥4–5 mm (0.157–0.197 in) for bordered card backs.
Job-Specific Production Steps
- Component and tooling lock: Finalize card counts, stock calipers, finish combinations, booklet signature counts, and partner-sourced piece samples to establish total stack height and weight in kg (lb).
- Prepress and dieline separation: Verify bleed, safety margins, TAC limits, 100% K fine text, and isolated spot/dieline layers on PDF/X-1a or PDF/X-4 master files.
- Offset printing and curing: Print sheets on calibrated offset presses, apply aqueous, UV, or film lamination (including anti-scuff matte on dark coverage), and cure sheets before mechanical stress.
- Die-cutting, wrapping, and binding: Slit and corner-round cards (R3–R3.5 mm / 0.118–0.138 in), die-cut punchboards with 3–4 mm (0.118–0.157 in) gaps, wrap 1.5–3 mm (0.059–0.118 in) greyboard with 15–20 mm (0.591–0.787 in) turn-ins, and fold or bind booklets in 4-page signatures.
- Kitting and fit verification: Collate decks, boosters, punchboards, booklets, and non-paper pieces into inserts and boxes, verifying lid closure and stack movement.
Sign-Off Criteria
- Caliper and stack height check: Measured laminated card deck height and folded booklet thickness match box interior depth with 1.5–3 mm (0.059–0.118 in) clearance.
- Clearance and wrap check: Cards, boards, and trays slide freely with 1.5–2.5 mm (0.059–0.098 in) lateral clearance; greyboard wraps show 15–20 mm (0.591–0.787 in) adhesion without corner lifting.
- Prepress separation check: Dielines and spot effects sit on non-printing/separate layers, TAC does not exceed 280%–300%, and bordered backs hold ≥4–5 mm (0.157–0.197 in) safety.
- Conditional regulatory and packaging records:
- When a game or component falls under EU toy-safety scope (such as products intended for children or containing small parts), maintain EN 71 assessment and testing records in line with the European Commission Toy Safety framework.
- For packaged goods placed on the German market, complete packaging participation and data reporting per the VerpackG / LUCID information system.
- For packaged goods sold in France, apply sorting and material markings according to France’s Triman / Info-tri rules.
Concrete Failure Modes
| Failure Mode | Physical Cause | Prevention / Fix |
|---|---|---|
| Box lid fails to seat or bows | Deck height calculated from raw gsm caliper without adding 0.03–0.05 mm (0.001–0.002 in) per card for double-sided film. | Sum laminated caliper across the full deck plus 1.5–3 mm (0.059–0.118 in) depth clearance. |
| Off-center borders on card backs | Standard 3 mm (0.118 in) safety margin used on a bordered back design during die-cut registration variance. | Increase bordered-back safety margin to ≥4–5 mm (0.157–0.197 in). |
| Gilded edge foil peels or flakes | Heavy film lamination applied prior to edge gilding blocks foil adhesion along card edges. | Omit thick film lamination on gilded decks or switch to a compatible surface varnish. |
| Punchboard waste tears or tokens pop early | Die-cut gap narrower than 3 mm (0.118 in) weakens the surrounding greyboard matrix. | Enforce 3–4 mm (0.118–0.157 in) spacing between all punchboard dies and sheet borders. |
| Dark card backs show white scuff lines | Standard matte varnish or uncoated ink rubbed during collating and shuffling. | Specify anti-scuff matte lamination and keep TAC ≤280%–300% with rich black (C40–60 M30–40 Y30–40 K100). |
| Booklet spine cracks or pages creep | Saddle stitch forced above 40 pages, or perfect binding used on a high-page-count rulebook opened flat repeatedly. | Move 28+ page books to perfect binding and 80–100+ page books to sewn binding in 4-page signatures. |
| Box corners crush or wraps peel | Greyboard too thin for packed kg (lb) load, or wrap turn-in shorter than 15 mm (0.591 in). | Step up greyboard to 2–3 mm (0.079–0.118 in) and maintain a 15–20 mm (0.591–0.787 in) wrap margin. |
Guides in this section
- Rulebook, Booklet, and Printed Reference Specifications
- Booster Pack and Wrapper Specifications
- Card Box and Game Box Specifications
- Card Stocks, Shapes, and Manufacturing Tolerances
- Game Board and GM Screen Specifications
- Game Box Insert and Divider Specifications
- Non-Paper Tabletop Component Specifications
- Punchboard Construction and Die-Cut Tolerances
- Jigsaw Puzzle and Crowdfunding Paper Extra Specifications