Choosing the exact template and stock parameters shifts under three physical conditions:

  • Bordered vs. full-bleed card backs: Printed borders require a 4–5 mm (0.157–0.197 in) safe zone instead of the standard 3 mm (0.118 in) inset so normal die-cut variance does not create visibly uneven margins.
  • Deck card count and lamination: Moving from a 32-card Skat deck to a 48-card Doppelkopf deck adds 4.5 to 7.8 mm (0.18 to 0.31 in) to total stack height across 300–400 gsm stocks including double-sided film lamination, altering the required internal box cavity.
  • Dark artwork and edge gilding: Heavy dark backgrounds require anti-scuff matte coating and controlled total area coverage (TAC), whereas gilded edges conflict with thick film lamination.

Exact Specifications and 300 DPI Pixel Canvas

All inch values below are derived from the 59 × 91 mm trim at 25.4 mm per inch, and pixel dimensions are calculated at 300 DPI. For comparisons across other standard formats in this category, see the playing card sizes overview. Other deck formats use their own dedicated die-line dimensions rather than scaling a Skat template, because proportional scaling distorts corner radii and index clearances.

Parameter Millimetres (mm) Inches (in) 300 DPI Pixels (px) Notes
Trim Size (Finished Card) 59 × 91 mm 2.32 × 3.58 in 697 × 1075 px Standard Skat / Doppelkopf cut line
Bleed Canvas (+3 mm / side) 65 × 97 mm 2.56 × 3.82 in 768 × 1146 px 3 mm (0.118 in) bleed on all four sides
Safe Zone (Borderless) 53 × 85 mm 2.09 × 3.35 in 626 × 1004 px ≥3 mm (0.118 in) inset from trim
Safe Zone (Bordered Backs, 4 mm) 51 × 83 mm 2.01 × 3.27 in 602 × 980 px Minimum 4 mm (0.157 in) inset for borders
Safe Zone (Bordered Backs, 5 mm) 49 × 81 mm 1.93 × 3.19 in 579 × 957 px Preferred 5 mm (0.197 in) inset for borders
Corner Radius R3–R3.5 mm R0.118–0.138 in — Keep corner indices clear of arc

Bleed and Pixel Calculator Formulas

Use these plain-text formulas when verifying custom artboards or exporting raster layers for the 59 × 91 mm die-line:

  • Canvas Width (mm) = Trim Width (mm) + (2 × Bleed per side) → 59 + (2 × 3) = 65 mm
  • Canvas Height (mm) = Trim Height (mm) + (2 × Bleed per side) → 91 + (2 × 3) = 97 mm
  • Inches = Millimetres / 25.4 → 65 / 25.4 = 2.56 in; 97 / 25.4 = 3.82 in
  • 300 DPI Pixels = round((Millimetres / 25.4) × 300) → round((65 / 25.4) × 300) = 768 px; round((97 / 25.4) × 300) = 1146 px

Card Stock, Caliper, and Deck Stack Weight

Standard offset playing cards start at 200 decks (usual tiers: 200, 300, 500, and 1,000+ decks), while boxed games and custom tooling follow project and component minimums. When specifying stock, reference gsm (grams per square metre) alongside caliper rather than relying solely on US pound ratings: US Cover LB is measured on a 20 × 26 in (508 × 660 mm) basis sheet, whereas US Text LB is measured on a 25 × 38 in (635 × 965 mm) basis sheet, meaning identical pound numbers represent very different paper weights and stiffnesses.

Stock Option Caliper per Card Characteristics
300 gsm art / blue core 0.28–0.31 mm (0.0110–0.0122 in) Standard promotional and light playing-card stock
310 gsm black-core linen 0.30–0.32 mm (0.0118–0.0126 in) Textured snap and opacity for frequent shuffling
330 gsm black core 0.32–0.34 mm (0.0126–0.0134 in) Higher stiffness and full light-blocking core
350 gsm art stock 0.34–0.38 mm (0.0134–0.0150 in) Rigid uncoated or coated board without black core
400 gsm art stock 0.40–0.44 mm (0.0157–0.0173 in) Heavy rigid board for low-shuffle reference cards
PVC 0.30 mm (0.0118 in) Waterproof plastic stock

Double-sided film lamination adds 0.03–0.05 mm (0.0012–0.0020 in) per card. For a 59 × 91 mm deck (0.005369 m² per card), stack height and net card weight scale as follows:

  • 32-card Skat deck on 310 gsm black-core linen:
    • Unlaminated stack height: 9.6–10.2 mm (0.38–0.40 in); with double-sided film: 10.6–11.8 mm (0.42–0.46 in).
    • Net card weight: 0.053 kg (0.117 lb).
  • 48-card Doppelkopf deck on 310 gsm black-core linen:
    • Unlaminated stack height: 14.4–15.4 mm (0.57–0.61 in); with double-sided film: 15.8–17.8 mm (0.62–0.70 in).
    • Net card weight: 0.080 kg (0.176 lb).
  • 48-card Doppelkopf deck on 330 gsm black core:
    • Unlaminated stack height: 15.4–16.3 mm (0.61–0.64 in); with double-sided film: 16.8–18.7 mm (0.66–0.74 in).
    • Net card weight: 0.085 kg (0.187 lb).

For tuck boxes or two-piece rigid boxes housing Skat decks, add 1.5–2.5 mm (0.06–0.10 in) clearance across card width and height (targeting a 60.5–61.5 × 92.5–93.5 mm internal cavity) and 1.5–3 mm (0.06–0.12 in) clearance on top of the finished stack height.

Prepress Setup and Production Steps

  1. Build the artboard at 65 × 97 mm (2.56 × 3.82 in): Set the document trim box to 59 × 91 mm (2.32 × 3.58 in) and extend all background artwork, textures, and edge-to-edge rules all the way to the 65 × 97 mm outer edge.
  2. Position corner indices inside the safe zone: Keep card pips, corner numbers, and key illustrations inside the 53 × 85 mm (2.09 × 3.35 in) safe box, and pull them slightly inward near the four corners to clear the R3–R3.5 mm (0.118–0.138 in) die-cut radius. For bordered backs, hold the inner edge of the border frame at least 4–5 mm (0.157–0.197 in) from the trim line.
  3. Prepare CMYK and spot-finish layers: Work in CMYK at ≥300 DPI. Set fine text and thin linework to 100% K only so registration shifts do not blur small typography. Build large dark solids using rich black (C40–60 M30–40 Y30–40 K100) while keeping total area coverage (TAC) at or below 280%–300%. Place metallic foil, spot UV, and die-line guides on separate named spot layers set to overprint where required.
  4. Match coating to artwork and edge treatment: Specify anti-scuff matte coating when cards carry heavy dark artwork to reduce rub marks during collation and play. Avoid combining thick lamination with gilded edges, as thick film interferes with foil adhesion along the trimmed edge.
  5. Export press-ready files: Deliver native AI, PDF, or PSD packages exported to PDF/X-1a or PDF/X-4 with all fonts outlined or embedded and no RGB or unflattened transparency errors.

Sign-Off Criteria and Failure Modes

Sign-Off Criteria

  • Trim box measures exactly 59 × 91 mm (2.32 × 3.58 in) and bleed box measures 65 × 97 mm (2.56 × 3.82 in) across every card face and back.
  • All raster assets are ≥300 DPI at 100% print scale (768 × 1146 px full bleed).
  • Fine text is 100% K, rich black areas fall within C40–60 M30–40 Y30–40 K100, and peak TAC does not exceed 280%–300%.
  • Fonts are outlined or embedded, and spot layers (foil, spot UV, die-lines) are separated from CMYK artwork.
  • Box cavity dimensions account for the actual card count, stock caliper, and 0.03–0.05 mm per-card lamination build-up plus 1.5–2.5 mm width/height and 1.5–3 mm stack clearance.

Concrete Failure Modes

  • Lopsided card-back borders: Using a 3 mm (0.118 in) or narrower inset on bordered backs causes normal press-sheet trim drift to leave one margin visibly thinner than the opposite side. Keep bordered frames ≥4–5 mm (0.157–0.197 in) from trim.
  • Clipped corner indices: Placing Skat or Doppelkopf corner pips too close to the 90-degree artboard corners results in the R3–R3.5 mm corner-rounding die slicing through suit symbols or numbers.
  • Scuffing and ink cracking on dark solids: Exceeding 300% TAC or omitting anti-scuff matte on dark CMYK backs leads to visible rub marks, slow ink drying, and edge chipping during die-cutting.
  • Gilded-edge peeling: Applying edge gilding over thick film lamination causes the metallic edge foil to lift or flake during shuffling.
  • Tight or crushed tuck boxes: Sizing a box cavity from unlaminated card caliper alone causes a 48-card laminated deck to bind in the box or bow the carton walls.