Specifications and Template Parameters
Standard offset card runs with specialist manufacturing partners start at 200 decks (usual production tiers: 200, 300, 500, and 1,000+ decks), while custom tooling and boxed sets follow component minimums.
Format Envelope and Reference Dimensions
Inch equivalents are derived at 25.4 mm per inch, and 300 DPI pixel counts reflect the full bleed canvas.
| Format Reference | Trim (mm) | Trim (in) | Bleed Canvas (+6 mm) | 300 DPI Bleed Pixels | Corner Radius |
|---|---|---|---|---|---|
| Standard Tarot (lower bound) | 70 × 120 mm | 2.76 × 4.72 in | 76 × 126 mm (2.99 × 4.96 in) | 898 × 1488 px | R3–R3.5 mm (0.118–0.138 in) |
Standard Oracle (assigned trim W × H) |
Wider than 70 mm, smaller than 88 × 126 mm | (W / 25.4) × (H / 25.4) in |
(W + 6) × (H + 6) mm |
((W + 6) / 25.4) * 300 × ((H + 6) / 25.4) * 300 px |
R3–R3.5 mm (0.118–0.138 in) |
| Large Oracle (upper bound) | 88 × 126 mm | 3.46 × 4.96 in | 94 × 132 mm (3.70 × 5.20 in) | 1110 × 1559 px | R3–R3.5 mm (0.118–0.138 in) |
Bleed, Safe-Area, and Pixel Formulas
Use plain-text calculations when configuring any assigned Standard Oracle trim (W = trim width in mm, H = trim height in mm):
- Bleed margin: 3 mm (0.118 in) per edge, adding 6 mm (0.236 in) to both width and height.
- Full bleed width (mm):
W + 6 - Full bleed height (mm):
H + 6 - 300 DPI pixel width:
round(((W + 6) / 25.4) * 300) - 300 DPI pixel height:
round(((H + 6) / 25.4) * 300) - Standard safe area (borderless art):
>= 3 mm(0.118 in) inward from every trim edge; live printable area is(W - 6) × (H - 6)mm. - Bordered back safe area:
>= 4–5 mm(0.157–0.197 in) inward from every trim edge; critical inner elements sit inside(W - 8) × (H - 8)mm to(W - 10) × (H - 10)mm.
Prepress, Color, Stock, and Clearance Specs
- Accepted file formats: AI, PDF, or PSD, exported for print as PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
- Resolution and color space: Minimum 300 DPI for all raster artwork; CMYK color mode with separate spot layers for foil, spot UV, or metallic inks.
- Black ink builds and coverage: Use 100% K (
C0 M0 Y0 K100) for fine text and thin linework; use rich black (C40–60 M30–40 Y30–40 K100) for large dark solids; keep Total Area Coverage (TAC) at<= 280%–300%. - Cardstock gsm, basis weight, and caliper: Cardstocks are specified in grams per square meter (gsm), which measures sheet mass directly, whereas US pound ratings depend on basis sheet size—US Cover LB uses a 20 × 26 in (508 × 660 mm) basis sheet, while US Text LB uses a 25 × 38 in (635 × 965 mm) basis sheet. Common card calipers:
- 300 gsm art / blue core: 0.28–0.31 mm (0.011–0.012 in)
- 310 gsm black-core linen: 0.30–0.32 mm (0.012–0.013 in)
- 330 gsm black core: 0.32–0.34 mm (0.013–0.0134 in)
- 350 gsm art stock: 0.34–0.38 mm (0.013–0.015 in)
- 400 gsm art stock: 0.40–0.44 mm (0.016–0.017 in)
- PVC: 0.30 mm (0.012 in)
- Finish and box clearance: Double-sided film lamination adds 0.03–0.05 mm (0.001–0.002 in) per card. Anti-scuff matte suits dark oracle artwork, while thick lamination can conflict with gilded edges. Pair the finished deck with 1.5–2.5 mm (0.059–0.098 in) box clearance across width and height and 1.5–3 mm (0.059–0.118 in) clearance for total stack height.
Production Steps
- Lock the trim inside the Standard Oracle band: Select a trim wider than 70 × 120 mm (2.76 × 4.72 in) and smaller than 88 × 126 mm (3.46 × 4.96 in) that fits the illustration proportions and press sheet layout.
- Build the template layers: Set the document canvas to
(W + 6) × (H + 6)mm at 300 DPI, mark theW × Hmm trim box, and place non-printing guides for the R3–R3.5 mm (0.118–0.138 in) corners and the 3 mm (0.118 in) or 4–5 mm (0.157–0.197 in) safe zone. - Extend artwork and separate spot layers: Pull background colors, textures, and full-bleed art all the way to the outer bleed edge. Place any foil or spot UV masks on dedicated overprint spot layers rather than flattening them into CMYK.
- Verify ink density and typography: Convert fine body copy and captions to 100% K, set dark solids to rich black (
C40–60 M30–40 Y30–40 K100), cap TAC at<= 280%–300%, and outline or embed all fonts. - Export and match packaging tolerances: Export to PDF/X-1a or PDF/X-4. Calculate total deck stack thickness (
card count * (stock caliper + film thickness)) before finalizing tuck or rigid box dimensions so the 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) stack clearances hold.
Sign-Off Criteria
- Bleed extends a full 3 mm (0.118 in) beyond the trim box on all four edges with no white canvas gaps.
- Text, titles, and frame borders sit at least 3 mm (0.118 in) inside the trim, or 4–5 mm (0.157–0.197 in) inside the trim on bordered card backs.
- Corner elements clear the R3–R3.5 mm (0.118–0.138 in) die-cut arc.
- Raster images resolve at
>= 300 DPIat 100% print scale, with CMYK builds capped at<= 280%–300%TAC and fine text in 100% K. - Spot finishes sit on separate named spot layers, and fonts are outlined or embedded in PDF/X-1a or PDF/X-4 output.
Concrete Failure Modes
- Uneven or clipped back borders: Placing a thin border within 1–2 mm (0.039–0.079 in) of the trim causes visible off-center framing when normal die-cut registration shifts; enforce the 4–5 mm (0.157–0.197 in) safe margin on bordered backs.
- White edge slivers after die-cutting: Stopping background art at the trim line instead of extending it 3 mm (0.118 in) into the bleed exposes unprinted stock along card edges.
- Corner-radius clipping: Positioning card numbers, corner ornaments, or sharp frame corners inside the R3–R3.5 mm (0.118–0.138 in) corner arc results in severed details during round-cornering.
- Scuffing, ink set-off, or gilding delamination: Exceeding 300% TAC on dark oracle spreads slows ink drying and causes sheet-to-sheet marking, while omitting anti-scuff matte leaves dark matte surfaces prone to rub marks; pairing thick film lamination with gilded edges prevents clean metallic adhesion.
- Tight box fit or crushed deck edges: Sizing a box from bare cardstock caliper without adding 0.03–0.05 mm (0.001–0.002 in) per card for double-sided film—or omitting the 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) stack clearances—leaves the finished deck binding inside the box.
Parent guide Tarot and Oracle Card Sizes and Templates