Both constructions are produced with specialist offset and tabletop manufacturing partners, and the right choice depends on how the screen is used, packed, and transported. When comparing structural options across boards and mats comparisons, the deciding factors are panel height, fold frequency, available box depth, and unit weight targets.
Choose mounted (paper-wrapped) grayboard when:
- The screen stands upright for multi-hour sessions without clips, weighted bases, or table clamps.
- The screen is opened and folded repeatedly across a campaign, requiring flexible paper-wrapped hinges rather than scored fibers.
- Tall or wide multi-panel layouts must resist bowing from ambient humidity or table drafts.
- The screen is sold as a standalone hardcover-style accessory or inside a deep rigid box.
Choose heavy cardstock when:
- The screen must pack flat inside a thin game box, zine sleeve, or starter set with tight stack-height limits.
- Lower unit cost and lighter parcel weight (
kg/lb) matter more than rigid self-standing bulk. - The screen uses compact panel heights or a three-panel footprint that stands reliably at a shallow angle.
- Tooling and setup budgets favor single-sheet die-cutting and creasing over multi-part board wrapping.
Head-to-Head Specifications
| Specification | Mounted Grayboard GM Screen | Heavy Cardstock GM Screen |
|---|---|---|
| Core substrate | Rigid grayboard: 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in) |
Solid art or core cardstock: 300–400 gsm |
| Typical single-panel caliper | Core thickness plus wrap and liner (~1.7–3.3 mm / ~0.067–0.130 in total) |
350 gsm art stock: 0.34–0.38 mm (0.013–0.015 in); 400 gsm: 0.40–0.44 mm (0.016–0.017 in) |
| US basis weight class | Wrap/liner: 80–120 gsm (25 × 38 in / 635 × 965 mm Text LB basis) |
Main sheet: 300–400 gsm (20 × 26 in / 508 × 660 mm Cover LB basis) |
| Hinge mechanism | Separated board panels joined by continuous wrapped outer sheet and inner liner | Die-scored creases pressed directly into the laminated cardstock sheet |
| Lamination allowance | 0.03–0.05 mm (0.001–0.002 in) for outer wrap film |
0.03–0.05 mm (0.001–0.002 in) for double-sided film per sheet |
| Folded stack height (3–4 panels) | High (~6–13 mm / ~0.236–0.512 in depending on board caliper) |
Low (~1.2–2.0 mm / ~0.047–0.079 in) |
| Boxed clearance requirement | 1.5–2.5 mm (0.059–0.098 in) width/height; 1.5–3 mm (0.059–0.118 in) stack height |
1.5–2.5 mm (0.059–0.098 in) width/height; 1.5–3 mm (0.059–0.118 in) stack height |
| Tooling & minimums | Project/component minimums for board cutting, grooving/spacing, and casing-in | Project/component minimums for custom die-cutting and creasing |
Distinguishing US Text LB vs. Cover LB
Paper basis weights cannot be compared by pound number alone because US mills use different basis sheet sizes:
- US Text LB is weighed on a
25 × 38 in(635 × 965 mm) basis sheet. Wrap and liner papers (80–120 gsm,0.08–0.13 mm/0.003–0.005 inper sheet) fall into this class. - US Cover LB is weighed on a
20 × 26 in(508 × 660 mm) basis sheet. Heavy cardstock screens (300–400 gsm) fall into this class, delivering roughly twice the caliper of a Text stock with the same numeric pound label.
Material and Prepress Specifications
Both screen types share offset prepress standards, though their structural tolerances differ at the edges and folds:
- File formats and color: Supply print-ready
PDF/X-1aorPDF/X-4exported fromAI,PDF, orPSDwith all fonts outlined or embedded. Build artwork inCMYKwith separate spot layers for foil or spot UV, at≥300 DPI. - Black ink and coverage: Set fine reference tables and small body text to
100% Kfor crisp legibility. Use rich black (C40–60 M30–40 Y30–40 K100) for large dark panels while keeping Total Area Coverage (TAC) at≤280%–300%. - Bleed and safety margins:
- Heavy cardstock: Include
3 mm(0.118 in) bleed per side and keep text/tables at least3 mm(0.118 in) inside the trim and score lines (≥4–5 mm/0.157–0.197 infor bordered layouts). - Mounted grayboard: Include a
15–20 mm(0.591–0.787 in) wrap margin around the outer perimeter of the front wrap sheet so the paper turns cleanly over the grayboard edges onto the back face before the inner liner is applied.
- Heavy cardstock: Include
- Lamination: Specify anti-scuff matte film on dark artwork to prevent rub marks during shipping and table handling. Film adds
0.03–0.05 mm(0.001–0.002 in) to the total thickness of a double-sided cardstock sheet.
Production Steps
Mounted Grayboard Workflow
- Offset printing and lamination: Print the outer wrap sheet (typically
80–120 gsmcoated art paper) and the inner reference liner on separate sheets, then apply protective film to the outer wrap. - Board cutting: Cut the
1.5–3 mm(0.059–0.118 in) grayboard panels to the exact panel dimensions specified by the project dieline. - Gluing and wrapping: Apply adhesive to the outer wrap, position the grayboard panels with uniform hinge gaps between them, and fold the
15–20 mm(0.591–0.787 in) wrap margins cleanly around all four edges. - Lining and pressing: Mount the inner reference sheet over the back face to bridge the hinge gaps and seal the turn-in margins, then press the assembled screen flat under controlled weight while the adhesive cures.
Heavy Cardstock Workflow
- Two-sided offset printing: Print the player-facing art and GM-facing reference tables duplex onto
300–400 gsmcardstock (such as350 gsmart stock at0.34–0.38 mm/0.013–0.015 inor400 gsmat0.40–0.44 mm/0.016–0.017 in). - Double-sided lamination: Apply matte or anti-scuff matte film to both sides to seal the ink and reinforce the surface across the fold lines.
- Die-cutting and creasing: Run the laminated sheets through a custom steel-rule die that trims the outer perimeter and presses channel scores along each panel fold.
- Pre-folding and packing: Fold along the scored hinges and pack flat into cartons or boxed game inserts.
Sign-Off Criteria
Before approving a production run, verify the physical white dummy or wet proof against these criteria:
- Standing stability: Open the screen to its intended table angle and confirm panels stand without bowing, creeping open, or tipping under light air movement.
- Hinge cycle check: Fold and unfold every hinge completely in both directions (folded flat for storage, opened to standing angle) to verify zero paper tearing on grayboard or film lifting on cardstock.
- Warp and curl tolerance: Lay the folded screen on a flat surface; mounted grayboard panels must sit flat without cup or twist caused by uneven glue moisture.
- Wrap and corner finish (grayboard): Inspect all four corners and the
15–20 mm(0.591–0.787 in) turn-in margins for tight adhesion, clean miters, and zero exposed raw grayboard. - Box and carton fit: If the screen packs inside a game box, confirm
1.5–2.5 mm(0.059–0.098 in) clearance across width and height and1.5–3 mm(0.059–0.118 in) clearance for folded stack height. Verify master carton gross weight inkgandlbagainst fulfillment limits. - Regulatory documentation (when applicable): If the screen is part of a product requiring regional compliance records, retain material test and assessment records for EN 71 toy safety where relevant, alongside packaging participation records for VerpackG or Triman sorting marks on outer packaging.
Concrete Failure Modes
- Panel warping (Mounted Grayboard):
- Cause: Applying wet adhesive to only one face of
1.5 mm(0.059 in) grayboard or omitting a balanced inner liner. - Fix: Use balanced outer wrap and inner liner paper weights (
80–120 gsm), press flat during curing, or step up to2 mm(0.079 in) or2.5 mm(0.098 in) grayboard for tall panels.
- Cause: Applying wet adhesive to only one face of
- Hinge tearing or binding (Mounted Grayboard):
- Cause: Hinge gap between grayboard panels is too narrow for the board thickness, pinching the wrap and liner paper when folded 180 degrees.
- Fix: Size the hinge gap proportionally to the selected board caliper (
1.5–3 mm/0.059–0.118 in) so the paper bridges smoothly without tension.
- Cracking along score lines (Heavy Cardstock):
- Cause: Folding
350–400 gsmcardstock against the paper grain direction or scoring with insufficient channel width over heavy ink coverage. - Fix: Align the sheet grain parallel to the vertical fold lines, keep
TAC ≤280%–300%, and laminate both sides before die-creasing.
- Cause: Folding
- Tip-over or panel sag (Heavy Cardstock):
- Cause: Tall panels made from
300 gsm(0.28–0.31 mm/0.011–0.012 in) stock lack enough stiffness when opened wide. - Fix: Upgrade to
400 gsm(0.40–0.44 mm/0.016–0.017 in) cardstock, shorten panel height, or switch to2 mm(0.079 in) mounted grayboard.
- Cause: Tall panels made from
- Box-fit binding:
- Cause: Calculating box depth from raw board or paper caliper without adding
0.03–0.05 mm(0.001–0.002 in) per laminated sheet or accounting for folded hinge bulk. - Fix: Measure the physical folded dummy stack and maintain
1.5–2.5 mm(0.059–0.098 in) width/height clearance and1.5–3 mm(0.059–0.118 in) stack height clearance.
- Cause: Calculating box depth from raw board or paper caliper without adding
Parent guide Game Board, GM Screen, and Play Mat Comparisons