An open-ended paperboard sleeve wraps around the four sides of a deck (front, back, and two spines) while leaving the top and bottom edges open, or sits over an inner shrink-wrapped brick. Shrink wrap alone seals the deck in clear film with no paperboard tooling, making the card face or back immediately visible while leaving no printed surface for retail metadata unless a top card or insert carries it.

Decision Comparison: Sleeve Box vs Shrink Wrap Alone

Decision Factor Open-Ended Sleeve Box Shrink Wrap Alone
Primary use case Retail shelves, expansion packs needing spine copy, or branded bundles Booster-style packs, internal game components, or transparent card-back display
Printed surface Front, back, and two spines for branding, barcodes, and legal text None on the film itself; requires a visible face card or loose insert
Edge and corner protection Shields long edges and faces from transit rubbing; ends remain open unless overwrapped Holds cards in a tight brick; minimal resistance against corner impacts
Tooling and minimums Requires a custom cutting die and project/component minimums No paperboard die required; follows standard offset card minimums (200 decks; usual tiers 200/300/500/1,000+)
Unit cost driver Paperboard stock, CMYK/spot printing, lamination, die-cutting, and gluing Film material and heat-tunnel labor only

Specifications and Sizing Rules

Calculating Stack Height Before Sizing

Because an open-ended sleeve relies on controlled friction or a tight outer wrap to keep the deck from sliding out, measure or calculate the exact stack height before locking the sleeve dieline:

Stack height (mm) = (Card count * Single-card caliper) + Booklet or leaflet thickness

Use the actual stock and finish caliper for the deck:

  • 300 gsm art or blue core: 0.28–0.31 mm (0.011–0.012 in) per card
  • 310 gsm black-core linen: 0.30–0.32 mm (0.012–0.013 in) per card
  • 330 gsm black core: 0.32–0.34 mm (0.0126–0.0134 in) per card
  • 350 gsm art stock: 0.34–0.38 mm (0.013–0.015 in) per card
  • 400 gsm stock: 0.40–0.44 mm (0.016–0.017 in) per card
  • PVC: 0.30 mm (0.012 in) per card
  • Double-sided card film: adds 0.03–0.05 mm (0.0012–0.0020 in) per card

If a folded 4-, 6-, or 8-panel leaflet or bound booklet (using 80–120 gsm / 0.08–0.13 mm [0.003–0.005 in] interior sheets and 200–300 gsm covers) sits inside the sleeve alongside the deck, include its folded thickness in the stack-height calculation.

Sleeve Clearance and Paperboard Specs

  • Clearance: Standard box clearance is 1.5–2.5 mm (0.059–0.098 in) across width and height and 1.5–3 mm (0.059–0.118 in) for stack height. For an open-ended sleeve without an outer shrink wrap, coordinate tighter friction-fit tolerances with the manufacturing partner so the deck does not slip out under its own weight.
  • Paperboard weight: Specify sleeve stock in gsm (typically 200–300 gsm for lightweight wraps or 300–400 gsm when higher spine rigidity is needed). When referencing US pound weights, distinguish Cover LB (measured on a 20 × 26 in / 508 × 660.4 mm basis sheet) from Text LB (measured on a 25 × 38 in / 635 × 965.2 mm basis sheet), because the same pound number represents a substantially heavier board in Cover LB.
  • Surface finish: Apply anti-scuff matte lamination on sleeves with dark or solid-ink artwork to prevent rub marks during shipping and shelf handling.

Prepress Requirements for Printed Sleeves

  • File formats: AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
  • Color and resolution: CMYK with separate spot layers for foils or spot varnishes, at least 300 DPI for raster artwork.
  • Bleed and safety: 3 mm (0.118 in) bleed per side and at least 3 mm (0.118 in) safety margin inside all trim and fold lines.
  • Ink density: Use 100% K for fine text and barcodes; use rich black (C40–60 M30–40 Y30–40 K100) for large dark solids while keeping Total Area Coverage (TAC) at or below 280%–300%.

Production Steps and Sign-Off Criteria

  1. Lock the deck specification: Confirm card count, stock gsm, card lamination, and any enclosed leaflet or booklet so the physical brick dimensions are fixed.
  2. Approve the sleeve dieline: Verify width, height, and spine-depth panels against the calculated stack height and intended wrapping method (friction-fit sleeve over bare cards, or sleeve over an already shrink-wrapped deck).
  3. Run prepress and proof checks: Confirm 3 mm (0.118 in) bleed, 100% K barcode and fine-text separation, TAC ≤280%–300%, and fold-panel orientation so spine text reads in the intended direction.
  4. Wrap and assemble: Shrink-wrap the card brick first when moisture protection or loose-card containment is required, slide it into the glued sleeve, and apply an outer shrink overwrap if the open ends must stay sealed in transit.
  5. Inspect against sign-off criteria:
    • The deck slides into the sleeve without bowing the spine or crushing card corners, and does not fall out when held vertically.
    • Barcodes scan cleanly in 100% K without rich-black misregistration.
    • Shrink-wrap seams sit flat away from the barcode scan zone and do not warp thin card stacks.

Regulatory and Labeling Considerations

Packaging format changes what surface area is available for statutory marks and how packaging fractions are reported:

  • Germany (VerpackG): Placing packaged decks on the German market involves registration and packaging data reporting with Zentrale Stelle Verpackungsregister (VerpackG), where adding a paperboard sleeve introduces a paper/cardboard fraction alongside or in place of plastic film.
  • France (Triman / Info-tri): Household packaging sold in France is subject to sorting-label procedures described by Info-tri / Triman; an open-ended sleeve provides dedicated print space for sorting instructions that bare shrink wrap lacks without an inserted card or adhesive label.
  • EU Toy Safety (EN 71): Decks marketed as toys or children's games require assessment and testing under EU Toy Safety (EN 71), including applicable labeling and packaging film requirements.

Failure Modes and How to Prevent Them

  • Deck sliding out of open sleeve ends: Occurs when an unsealed sleeve uses standard 1.5–2.5 mm (0.059–0.098 in) carton clearance without an outer overwrap. Prevent this by shrink-wrapping the sleeved unit as a second step or tightening the sleeve dieline to a physical dummy brick.
  • Sleeve bowing or split glue seams: Occurs when the stack-height calculation omits the 0.03–0.05 mm (0.0012–0.0020 in) per-card thickness added by double-sided film or an enclosed leaflet. Always calculate caliper with finishes included.
  • Card edge curl or brick warping under shrink wrap alone: Occurs when heat-tunnel tension pulls too tightly on unboxed decks. Calibrate film gauge and tunnel heat to the deck's stiffness, or add a rigid sleeve when decks will face rough bulk transit.
  • Scuffed dark sleeve panels: Occurs when uncoated or standard gloss sleeves rub in master cartons. Specify anti-scuff matte lamination on dark designs.
  • Unreadable barcodes through shrink seams: Occurs when a shrink-wrap weld line crosses a printed sleeve barcode or an internal top-card barcode. Position barcodes away from expected seam lines during dieline and wrap setup.