Both finishes cure a clear gloss polymer over a matte-laminated surface to create contrast against dark or muted artwork, as part of the broader finishes comparison. The decision comes down to stack geometry, surface flexing, and edge contact:
- Use flat spot UV on playing cards, game cards, card backs, and any component stacked in bulk or flexed during shuffling. Flat spot UV adds negligible height, keeping the deck stack flat under cutting clamps and preventing tactile tells or catching edges during play.
- Use raised spot UV on rigid box lids, slipcases, tuck box front/back panels, and flat display covers where tactile relief adds shelf presence without affecting stack height or crossing a fold line.
- Switch from raised to flat (or omit spot UV) when artwork crosses tuck-box creases, wraps around rigid-box edges, or sits on cards that will receive gilded edges. Thick raised polymer cracks along score lines and interferes with edge-gilding clamps.
Specifications and Comparison
| Attribute | Flat Spot UV | Raised Spot UV |
|---|---|---|
| Tactile profile | Flush to very slight sheen step; negligible stack build | Noticeable 3D relief; builds cumulative height across stacks |
| Visual contrast | Crisp gloss-on-matte contrast | High gloss-on-matte contrast plus light-catching edge bevel |
| Primary applications | Card faces, card backs, flat inserts, fine-detail highlights | Rigid box lids, tuck box panels, display covers |
| Stacking & cutting behavior | Lies level in bulk stacks; safe for guillotine and die-cutting | Causes uneven stack height, rocking, and clamp-mark distortion on cards |
| Fold & crease tolerance | Tolerates gentle flexing when kept clear of sharp creases | Cracks, chips, or peels if placed over score lines or wrap corners |
| Base lamination | Matte or anti-scuff matte film (0.03–0.05 mm / 0.001–0.002 in double-sided on cards) | Matte or anti-scuff matte film on box wraps and covers |
| Typical substrates | 300–330 gsm card cores (approx. 111–122 lb Cover, 20 × 26 in basis; 0.28–0.34 mm / 0.011–0.013 in caliper) | 350–400 gsm tuck/cover stock (approx. 130–148 lb Cover, 20 × 26 in basis; 0.34–0.44 mm / 0.013–0.017 in) or 1.5–3 mm (0.059–0.118 in) greyboard wraps |
Prepress and File Requirements
- File format & color: Supply print-ready AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4. Build base artwork in CMYK at ≥300 DPI with all fonts outlined or embedded.
- Spot UV mask layer: Place the spot UV mask on a separate, clearly named vector spot layer set to 100% K (black) overprint. Keep the spot layer separate from CMYK ink channels.
- Black & ink density: Use 100% K for fine text. For dark backgrounds beneath spot UV highlights, use rich black (C40–60 M30–40 Y30–40 K100) while keeping total area coverage (TAC) at ≤280%–300%.
- Bleed & safety margins: Include 3 mm (0.118 in) bleed per side on CMYK artwork. Keep spot UV elements inside the ≥3 mm (0.118 in) safety margin—and ≥4–5 mm (0.157–0.197 in) on bordered card backs—so cured polymer does not reach the trim line or R3–R3.5 mm (0.118–0.138 in) rounded corners.
- Clearance on packaging: Keep raised spot UV off all tuck-box score lines, glue flaps, and the 15–20 mm (0.591–0.787 in) wrap margins of greyboard rigid boxes.
Production Steps
- Prepress Separation and Trapping Verify that the spot UV vector mask aligns cleanly with the CMYK layer, sits clear of trim edges and die-cut scores, and excludes fine hairlines or tiny knockouts that can bridge during coating.
- Offset Printing and Base Lamination Print CMYK sheets at standard offset minimums (200+ decks for cards; project-specific minimums for boxes and components). Allow inks to cure, then apply matte or anti-scuff matte film lamination—especially on dark artwork—to prevent scuffing and create a uniform surface for UV adhesion and contrast.
- Spot UV Coating and Curing
- Flat spot UV: Apply a thin, even coat through a fine screen or coating plate, then cure under UV lamps so the gloss layer bonds flush to the matte film.
- Raised spot UV: Deposit a higher-build UV polymer via thick-mesh screen or digital inkjet UV head, then cure immediately so the raised edges hold their profile without slumping.
- Cutting, Creasing, and Box Assembly
- Cards: Die-cut or guillotine-cut flat-UV sheets and round corners (R3–R3.5 mm / 0.118–0.138 in). Flat profiles keep stacks level under cutting clamps.
- Packaging: Die-cut and crease tuck boxes, or wrap cured lid sheets onto 1.5–3 mm (0.059–0.118 in) greyboard. Verify internal box clearance of 1.5–2.5 mm (0.059–0.098 in) across width and height and 1.5–3 mm (0.059–0.118 in) for stack height.
Sign-Off Criteria
Before approving full production from a physical proof or pre-production sample, verify:
- Registration: Spot UV aligns accurately to the underlying CMYK artwork with no visible halo or offset shift.
- Stack flatness (cards): A full deck sits level on a flat surface with no doming, rocking, or edge flare, and fits within the planned box stack-height clearance.
- Crease integrity (packaging): Folded tuck-box panels and wrapped greyboard corners show zero cracking, whitening, or lifting along the edges of the cured UV.
- Surface bond and contrast: Cured gloss adheres cleanly to the matte or anti-scuff matte lamination without flaking under fingernail or rub pressure, and delivers clean visual separation against dark backgrounds.
Concrete Failure Modes
- Deck doming and uneven cutting: Applying raised spot UV to cards—especially in concentrated central emblems—creates thicker zones in the middle of the sheet. Stacked decks bow or rock under the cutter clamp, shifting trim alignment and causing cards to stick or catch during shuffling.
- Marked card backs: Extending either flat or raised spot UV to the trim edge or into the 4–5 mm (0.157–0.197 in) safety zone on bordered card backs creates specular glints or tactile ridges that make specific cards identifiable from the side or by touch.
- Cracking and peeling on folds: Running raised spot UV across a tuck-box score line or onto a rigid-box wrap turn-in causes the rigid cured polymer to fracture when folded, leaving jagged flakes along the crease.
- Misregistration on fine type: Pairing raised spot UV with small body text or thin rules makes minor press-to-screen registration tolerances visibly obvious as a clear ridge sitting beside the ink rather than on top of it.
- Poor adhesion or low contrast: Applying spot UV over uncoated stock or gloss lamination rather than matte/anti-scuff matte film reduces visual contrast and can cause the UV layer to fish-eye or peel.
Parent guide Coating, Decoration, and Edge Finish Comparisons