Card Deck Press coordinates custom dice through specialist tabletop manufacturing partners as part of boxed games and component runs, which follow project and component minimums rather than standard card-deck tiers. For broader component trade-offs, see Game Pieces Comparisons.
When Each Process Wins
| Factor | Engraved & Ink-Filled Faces | Flat Pad- or UV-Printed Faces |
|---|---|---|
| Marking structure | Recessed cavity molded or carved into the die face, then filled with paint | Ink deposited directly onto a flat, uncarved die face via pad transfer or UV inkjet |
| Wear resistance | High; recessed ink sits below the rolling surface and resists edge-to-table abrasion | Lower; exposed surface ink takes direct friction from rolling, shaking, and tray impacts |
| Color & detail | Solid spot colors per cavity; unsuitable for gradients, photographic art, or fine halftones | Supports multi-color artwork, gradients, fine halftones, and tight multi-ink graphics |
| Setup & tooling | Higher upfront setup when custom face cavities require dedicated mold tooling | Lower setup cost because standard blank dice bodies can be fixtured and printed |
| Best fit | High-wear dice, classic pips or bold icons, single- or two-color spot fills | Complex full-color illustrations, small-batch runs, or artwork with frequent revisions |
Artwork and Prepress Specifications
Prepare production files in AI, PDF, or PSD format exported as PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
- Engraved and ink-filled faces: Supply clean, closed vector paths on separate spot layers for each fill color. Avoid hairlines, micro-text, and tight acute angles that trap bubbles or tear during paint wiping. Keep each face's artwork centered within a safe margin away from rounded or beveled die edges so cavities do not break into the chamfer.
- Flat pad- or UV-printed faces: Supply vector art or raster artwork at >=300 DPI. Use CMYK for process artwork with separate spot layers for white underbases or metallic/solid spot inks. Use 100% K for fine dark text, keep rich black within C40-60 M30-40 Y30-40 K100, and cap total area coverage (TAC) at <=280%-300% to prevent over-inking and slow curing.
Production Steps
Engraved and Ink-Filled Workflow
- Tooling and cavity prep: Custom faces are cut into mold inserts (or CNC-engraved on blanks for compatible materials) to create uniform recessed channels.
- Molding and deburring: Dice bodies are molded, cooled, and tumbled or trimmed to smooth parting lines and edge bevels.
- Ink filling: Paint is flooded or injected into each recessed face.
- Surface wiping and curing: Excess paint is wiped flush from the raised face before curing, leaving pigment only inside the recessed cavity.
Flat Pad- or UV-Printed Workflow
- Blank preparation: Standard or custom-colored blank dice are molded, tumbled, and cleaned to remove mold-release residue that blocks ink adhesion.
- Jig fixturing: Dice are seated into multi-up holding jigs so every face sits square to the print head or silicone transfer pad.
- Printing and curing: Pad printing transfers one spot color per plate pass; flat UV printing jets CMYK (plus white underbase when needed on dark bodies) and cures immediately under UV lamps.
- Optional topcoat: A clear protective coat may be applied over flat-printed faces to slow surface scuffing, though it does not match the physical protection of a recessed cavity.
Sign-Off Criteria
Inspect physical pre-production samples across all six (or more) faces before authorizing mass production:
- Registration and centering: Confirm markings sit centered on each face without drifting toward bevels or showing gaps between adjacent spot colors or white underbases.
- Fill and cure integrity: For engraved dice, verify cavities are completely filled with no pinholes, recessed voids, or paint halos on the surrounding flat surface. For printed dice, verify crisp edges, uniform gloss, and clean ink adhesion across edges.
- Color accuracy: Check filled or printed colors against approved spot targets or CMYK contract proofs under neutral lighting.
- Compliance documentation: Where custom dice form part of a product subject to toy or small-part rules, maintain applicable assessment and testing records—such as EU Toy Safety (EN 71) documentation for mechanical small-part checks and surface-coating requirements—rather than assuming material or ink coverage automatically qualifies.
Concrete Failure Modes
- Incomplete cavity fill or air pockets (Engraved): Narrow strokes or overly deep, steep-walled recesses trap air during flooding, leaving sunken spots or missing pigment in fine corners.
- Wipe-off smearing and halos (Engraved): If the die face has micro-scratches or the paint cures too quickly before wiping, pigment streaks across the flat surface around the glyph.
- Late-stage tooling lock-in (Engraved): Changing a symbol after mold cavities are cut requires re-machining inserts, adding cost and schedule delay.
- Edge chipping and rolling abrasion (Flat Printed): Artwork placed too close to sharp or lightly beveled edges chips first during repeated rolling, exposing the base resin underneath.
- Adhesion failure on slick blanks (Flat Printed): Residual mold release or unprimed acrylic/resin surfaces cause UV or pad ink to flake under fingernail or friction contact.
- Multi-pass misregistration (Flat Printed): Slight play in holding jigs shifts spot layers or white underbases out of alignment, leaving visible white fringes around colored icons.
Parent guide Tabletop Game Piece Comparisons