For broader board and tile format trade-offs, see punchboard comparisons.

When to Switch

  • Sheet-punched vs. loose delivery: Raw-edge tiles remain held in die-cut carrier sheets by small nicks, which streamlines packing and preserves punch-out presentation. Wrapped-edge tiles cannot be gang-punched from a single mounted sheet and must be wrapped, lined, and packed as loose components.
  • Edge visibility and wear: Raw-edge cuts expose the greyboard core around the perimeter. Wrapped-edge construction folds the printed face sheet over all four edges, concealing the core and resisting edge splitting or fuzzing under repeated handling.
  • Tooling and minimums: Boxed games and custom tooling follow project and component minimums. Wrapped-edge tiles add per-tile wrapping, corner mitering, and back-lining steps compared to single-pass sheet die-cutting.

Specifications Comparison

Specification Raw-Edge (Flush Die-Cut) Wrapped-Edge (Turned-Edge)
Core material Greyboard: 1.5 / 2 / 2.5 / 3 mm (0.059 / 0.079 / 0.098 / 0.118 in) Greyboard: 1.5 / 2 / 2.5 / 3 mm (0.059 / 0.079 / 0.098 / 0.118 in)
Sheet / wrap allowance 3–4 mm (0.118–0.157 in) die gap between tiles on the sheet 15–20 mm (0.591–0.787 in) wrap margin per side folded around the core
Perimeter finish Exposed greyboard core; flush cut edge Face paper wrapped over all edges; separate back liner applied
Delivery format Held in die-cut carrier sheets via nicks Loose individual tiles
Bleed & safety 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) safety 15–20 mm (0.591–0.787 in) wrap extension; ≥3 mm (0.118 in) face safety
Box clearance 1.5–2.5 mm (0.059–0.098 in) width/height; 1.5–3 mm (0.059–0.118 in) stack height 1.5–2.5 mm (0.059–0.098 in) width/height; 1.5–3 mm (0.059–0.118 in) stack height

Prepress & Production Steps

1. Prepress Setup

  • Supply artwork in AI, PDF, or PSD format exported as PDF/X-1a or PDF/X-4 with outlined or embedded fonts.
  • Build files in CMYK at ≥300 DPI, keeping spot finishes on separate spot layers.
  • Set fine text to 100% K. For deep dark solids, use rich black (C40–60 M30–40 Y30–40 K100) and keep total area coverage (TAC) at ≤280%–300%.
  • Use anti-scuff matte lamination on dark artwork to reduce rub marks along edges and stacked surfaces.

2. Raw-Edge Production

  1. Print face and back sheets with 3 mm (0.118 in) bleed per side and ≥3 mm (0.118 in) safety inside the cut line.
  2. Mount both printed sheets to 1.5, 2, 2.5, or 3 mm (0.059, 0.079, 0.098, or 0.118 in) greyboard.
  3. Die-cut the mounted board with a 3–4 mm (0.118–0.157 in) die gap between adjacent tiles, leaving small uncut nicks so tiles stay intact inside the carrier sheet during transit.

3. Wrapped-Edge Production

  1. Die-cut or guillotine bare greyboard cores to final tile dimensions.
  2. Print the face sheet with a 15–20 mm (0.591–0.787 in) wrap margin extending beyond each core edge, keeping critical art ≥3 mm (0.118 in) inside the face perimeter.
  3. Glue and fold the wrap margin around the greyboard edges, mitering or pleating the corners, then bond a trimmed back liner over the turn-ins.

Sign-Off Criteria

  • Registration & safety: Printed borders, icons, and text sit cleanly inside the ≥3 mm (0.118 in) safety zone with no bleed showing on adjacent raw-edge tiles or creeping onto wrapped-edge bevels.
  • Edge & surface integrity: Raw-edge tiles release from carrier nicks without tearing the face paper; wrapped-edge corners lie flat with full adhesive bond and no cracking along the fold.
  • Box & tray fit: Completed tile stacks fit the insert or box cavity within 1.5–2.5 mm (0.059–0.098 in) across width/height and 1.5–3 mm (0.059–0.118 in) for stack height.
  • Compliance records: Where tiles are intended for children's products, verify material and small-part requirements through EN 71 assessment and testing against the final production materials.

Failure Modes

  • Nick tearing (Raw-edge): Oversized nicks or dull steel-rule dies rip the printed face paper when players punch tiles from the sheet.
  • Edge fuzzing & splitting (Raw-edge): Repeated shuffling or damp conditions cause exposed greyboard plies to separate or fray along the cut perimeter.
  • Wrap lifting & dog-ears (Wrapped-edge): Insufficient glue or a wrap margin narrower than 15–20 mm (0.591–0.787 in) causes corner pleats to pop open over time.
  • Fold cracking (Wrapped-edge): Heavy ink coverage above 280%–300% TAC or stiff, thick lamination cracks along the 90-degree turn-in over 2–3 mm (0.079–0.118 in) greyboard.