For broader component trade-offs across custom jigsaw formats, see the puzzle comparisons overview.

When to Switch Construction

  • Choose unmounted cardstock when the puzzle ships inside an envelope, magazine, or flat-pack carton where total thickness must stay near 0.34–0.44 mm (0.013–0.017 in) and unit mass per piece must remain low in both kg and lb.
  • Choose mounted grayboard when players handle pieces repeatedly on a table, expect a crisp interlocking snap, and need rigid 1.5–3 mm (0.059–0.118 in) pieces that resist bending or curling during assembly.
  • Switch from unmounted to mounted if piece count or finished puzzle area requires lateral stiffness to move assembled sections without buckling.
  • Switch from mounted to unmounted if tooling and boxing minimums for rigid board exceed project scope, or if postage tiers penalize bulky cartons.

Specifications

Unmounted puzzles print directly onto heavy single-ply cover stock, whereas mounted puzzles print onto a lighter text-weight face sheet that is laminated to rigid grayboard. When comparing paper weights, US Text LB is measured on a 25 x 38 in (635 x 965 mm) basis sheet, while US Cover LB is measured on a 20 x 26 in (508 x 660 mm) basis sheet—making Cover LB roughly twice as dense as the same numerical Text LB.

Specification Unmounted Cardstock Mounted Grayboard
Core / Backing Single-ply 350 gsm (~130 lb Cover, 20 x 26 in) or 400 gsm (~148 lb Cover, 20 x 26 in) art stock Rigid greyboard at 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in)
Face Sheet Printed directly on the cardstock ply 80–120 gsm (~54–81 lb Text, 25 x 38 in) coated paper, 0.08–0.13 mm (0.003–0.005 in) thick
Total Caliper 0.34–0.38 mm (0.013–0.015 in) for 350 gsm; 0.40–0.44 mm (0.016–0.017 in) for 400 gsm Combined greyboard + face sheet + adhesive (typically 1.60–3.15 mm / 0.063–0.124 in)
Film Lamination Double-sided film adds 0.03–0.05 mm (0.001–0.002 in) Face-side film adds ~0.015–0.025 mm (0.0006–0.001 in); anti-scuff matte suits dark artwork
Shipping & Weight Profile Compact flat packs; lower shipping weight (kg / lb) per unit Bulkier boxed packs; substantially higher shipping weight (kg / lb) per unit
Packaging Fit Fits flat mailers or tight sleeves Boxed games follow project minimums with 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) stack-height clearance

Prepress & Artwork Requirements

  • File format: Supply AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
  • Resolution & color: >=300 DPI in CMYK with separate spot layers for custom inks or finishes. Keep fine text at 100% K, build rich black at C40–60 M30–40 Y30–40 K100, and cap total area coverage (TAC) at <=280%–300%.
  • Bleed & safety: Include 3 mm (0.118 in) bleed per side and keep critical text or border elements at least >=3 mm (0.118 in) inside the outer trim edge.
  • Dark coverage: Specify anti-scuff matte lamination on dark artwork to prevent rub marks during die-cutting and packing.

Production Steps

Card Deck Press coordinates production with specialist offset and tabletop manufacturing partners using two distinct workflows:

  1. Unmounted Cardstock Workflow

    • Offset printing: Print CMYK and any spot layers directly onto 350–400 gsm art stock (single-sided or two-sided).
    • Surface finishing: Apply aqueous coating or film lamination (adding 0.03–0.05 mm / 0.001–0.002 in if double-sided) to protect piece edges.
    • Steel-rule die-cutting: Die-cut the single-ply sheet in one pass through a custom puzzle die, then strip waste and pack flat or bag loose pieces.
  2. Mounted Grayboard Workflow

    • Face sheet printing & finishing: Print the 80–120 gsm (~54–81 lb Text, 25 x 38 in) face sheet via offset and apply the protective film (such as anti-scuff matte) before mounting.
    • Board mounting & curing: Laminate the printed face sheet onto 1.5 mm, 2 mm, 2.5 mm, or 3 mm greyboard with uniform adhesive pressure, allowing 15–20 mm (0.591–0.787 in) wrap or trim margin around the press sheet before final sizing, then cure under weight to stabilize moisture.
    • High-tonnage die-cutting: Cut the mounted board through a heavy-duty puzzle steel-rule die, break apart or bag the pieces, and pack into rigid boxes with 1.5–2.5 mm (0.059–0.098 in) width/height clearance.

Sign-Off Criteria

  • Prepress proof: Verify CMYK separation, <=280%–300% TAC, 3 mm (0.118 in) outer bleed, >=3 mm (0.118 in) safety margin, and crisp 100% K fine text.
  • Physical caliper & flatness: Confirm unmounted sheets measure within 0.34–0.44 mm (0.013–0.017 in) and mounted boards match the specified 1.5–3 mm (0.059–0.118 in) greyboard gauge without bowing on a flat surface.
  • Die-cut separation: Inspect interlocking tabs for clean cuts without crushed greyboard fibers, paper tearing, or hanging burrs.
  • Surface durability: Rub-test dark solid areas to confirm anti-scuff matte or varnish prevents ink transfer.
  • Regulatory documentation (conditional):

Concrete Failure Modes

  • Board warp and curl (Mounted Grayboard): Uneven moisture absorption between the adhesive, the 80–120 gsm face sheet, and the 1.5–3 mm greyboard causes pieces to dish or curl if boards are die-cut before adhesive curing finishes.
  • Edge delamination (Mounted Grayboard): Dull die blades or insufficient adhesive tack near sheet edges cause the printed face sheet to peel away from the greyboard when players separate or interlock pieces.
  • Tab bending and creasing (Unmounted Cardstock): Thin 350–400 gsm interlocking knobs bend permanently during rough separation or repeated assembly, reducing piece fit.
  • Scuffing on dark solids (Both): High-ink-coverage artwork (near 280%–300% TAC) without anti-scuff matte lamination marks and scratches when loose pieces rub inside bags or mailers.
  • Crushed edges and fuzzy cuts (Mounted Grayboard): Cutting 2.5–3 mm (0.098–0.118 in) greyboard with inadequate die pressure or worn ejection rubber leaves compressed, beveled edges and fibrous dust in the bag.