Specifications and Panel Geometry

Leaflets are produced in 4-, 6-, or 8-panel configurations. Standard leaflet interior stock runs 80–120 gsm (approximately 0.08–0.13 mm / 0.003–0.005 in per sheet), which corresponds to US Text LB weights measured on a 25 × 38 in basis sheet. Heavier 200–300 gsm cover stocks—measured as US Cover LB on a 20 × 26 in basis sheet—increase fold bulk and require mechanical creasing before folding.

Panel-Width Compensation

Every nested fold adds paper thickness at the hinge, pushing the inner panel outward toward the opposite crease. Subtract 2 to 3 mm (0.08 to 0.12 in) from each successive tucked panel so the leading edge stops short of the outer fold wall:

Structure Panel Count Panel Width Formula (Plain Text) Closure Constraint
6-panel roll fold 6 (3 per side) Outer = W; Center = W; Inner flap = W - (2 to 3 mm) Inner flap tucks cleanly inside outer cover without hitting the spine hinge.
8-panel roll fold 8 (4 per side) Panel 1 = W; Panel 2 = W; Panel 3 = W - (2 to 3 mm); Panel 4 = W - (4 to 6 mm) Cumulative step-down prevents double-layer bulk from bowing the outer cover.
Double-gate fold 8 (4 per side) Inner spread = 2 × W; Each gate flap = W - (2 to 3 mm) Left and right flaps leave a center gap so they do not collide when folded in half.

Prepress and Print Tolerances

  • File formats: AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
  • Color and resolution: CMYK with separate spot layers for fold/score guides; ≥300 DPI for all raster artwork.
  • Bleed and safety: 3 mm (0.118 in) bleed on all outer trim edges; ≥3 mm (0.118 in) safety margin from both trim edges and fold creases.
  • Black and ink density: 100% K for fine text; rich black C40–60 M30–40 Y30–40 K100 for solid areas; total area coverage (TAC) ≤280%–300% to prevent ink cracking along fold lines.
  • Boxed pack clearance: When a folded leaflet sits inside a card box or game box, keep the folded footprint within 1.5–2.5 mm (0.06–0.10 in) clearance across width and height, and reserve 1.5–3 mm (0.06–0.12 in) for total stack height.

Production Steps

  1. Panel imposition: Build the flat spread using the stepped panel widths above rather than equal grid divisions. Place fold and crease lines on a non-printing spot layer outside the 3 mm (0.118 in) bleed zone.
  2. Grain alignment: Orient the paper grain parallel to the primary fold axes so fibers bend smoothly along the hinge and resist spring-back.
  3. Offset printing: Print CMYK and any spot layers at ≤280%–300% TAC. Allow sufficient drying or curing before mechanical folding so wet ink does not set off onto adjacent panels under roller pressure.
  4. Scoring and folding: Score stocks above 120 gsm prior to folding. For roll folds, feed the narrowest tucked panel into the first buckle plate so it nests inside the wider panels; for double-gate folds, fold the two outer gate flaps inward first, then make the final center spine fold under controlled nip compression.

Sign-Off Criteria

  • Nested clearance: With the leaflet closed, the leading edge of every tucked panel stops 2 to 3 mm (0.08 to 0.12 in) short of the opposing fold crease.
  • Closure compression: The closed leaflet lies flat under light stack weight without the outer cover bowing or springing open.
  • Crease integrity: Folded edges show no fiber cracking, white paper exposure, or ink flaking across dark solids.
  • Safety alignment: All text, borders, and key graphics remain ≥3 mm (0.118 in) clear of every fold line and trim edge.

Failure Modes

  • Edge telescoping and buckling: Setting all panels to equal width forces the inner tucked panel against the outer fold wall, causing the flap to buckle outward or push the cover open.
  • Center spine pinching (double-gate fold): Making each gate flap equal to half the inner spread causes the two flap edges to butt together in the center, creating a rigid ridge that resists the final half-fold and cracks the spine.
  • Fold cracking: Running TAC above 300% over a fold line or folding perpendicular to the paper grain fractures the ink film and paper fibers along the crease.
  • Typography trapped in the hinge: Placing text or ruled borders closer than 3 mm (0.118 in) to a fold line pulls copy into the shadow of the gutter and distorts alignment across panels.
  • Box interference: Underestimating the stacked thickness of a 6- or 8-panel fold consumes the 1.5–3 mm (0.06–0.12 in) stack height clearance in a box, preventing the lid or tuck flap from closing cleanly.