Specifications and Material Selection
| Parameter | Specification | Production Condition |
|---|---|---|
| Stock weight | 200–300 gsm (approx. 74–111 lb Cover; 135–203 lb Text) | Distinguish US Cover LB (20 × 26 in / 508 × 660.4 mm basis sheet) from US Text LB (25 × 38 in / 635 × 965.2 mm basis sheet). |
| Approximate caliper | ~0.20–0.31 mm (0.008–0.012 in) uncoated/art; +0.03–0.05 mm (0.0012–0.0020 in) with double-sided film | 300 gsm art or blue-core board measures 0.28–0.31 mm (0.011–0.012 in) before lamination. |
| Trim construction | Straight guillotine cut or steel-rule die-cut | Guillotine for square corners; die-cut or mechanical corner-rounder for rounded corners. |
| Corner radius | Square (0 mm) or R3–R3.5 mm (0.118–0.138 in) | Rounded corners reduce dog-earing during repeated table handling. |
| Bleed & safety | 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) safety | Increase safety margin to ≥4–5 mm (0.157–0.197 in) for bordered designs. |
| Box-packing clearance | 1.5–2.5 mm (0.059–0.098 in) width/height; 1.5–3 mm (0.059–0.118 in) stack height | Calculated against the interior box wall or insert tray recess. |
| Prepress & color | CMYK + separate spot layers, ≥300 DPI, PDF/X-1a or PDF/X-4 | Outlined or embedded fonts; 100% K for fine text; rich black C40–60 M30–40 Y30–40 K100; TAC ≤280%–300%. |
Single-Sheet Trim Construction and Corner Rounding
Flat reference sheets do not use a fixed default trim dimension; width and height are sized to the game box's inner cavity or card tray minus 1.5–2.5 mm (0.059–0.098 in) of clearance on each axis.
- Guillotine trimming: Press sheets aregang-run or nested on parent sheets and cut on a programmable guillotine. This produces sharp 90-degree corners with minimal tooling cost and suits rectangular formats that sit flush inside a box lid or tray.
- Die-cutting and corner rounding: When R3–R3.5 mm (0.118–0.138 in) corners, thumb notches, or non-rectangular silhouettes are required, sheets are either struck with a custom steel-rule die or passed through a corner-rounding unit after guillotine trimming. Die-cutting holds tighter shape consistency across high-volume runs, while post-trim corner rounding avoids custom die tooling on standard rectangles.
Stiffness-to-Footprint Ratio
A sheet's perceived rigidity drops as its surface area increases, even when stock weight stays constant.
- Compact footprints: Smaller reference sheets maintain snap and lie flat at 200–250 gsm (~74–92 lb Cover, 20 × 26 in basis sheet) without bowing when picked up by one corner.
- Wide or full-box footprints: Larger sheets span more unsupported area and require 280–300 gsm (~104–111 lb Cover) plus double-sided matte or anti-scuff lamination (+0.03–0.05 mm / 0.0012–0.0020 in total caliper) to prevent edge sag and curl.
- Grain direction: Align paper grain parallel to the sheet's longest dimension so the sheet resists flexing across its wider span during table handling.
Flat Box-Packing Placement
Because flat reference sheets add only 0.20–0.36 mm (0.008–0.014 in) per sheet (including optional film), multiple player copies stack cleanly without crowding component wells.
- Top-of-insert placement: Full-footprint sheets sit flat between the rulebook and the inner tray lip, acting as a protective layer over loose tokens or cards.
- Recessed tray placement: Smaller sheets drop into a dedicated card or tile well; verify that total stack height (sheet caliper × player count) leaves 1.5–3 mm (0.059–0.118 in) of vertical clearance under the lid.
Production Steps and Sign-Off Criteria
- Prepress and imposition: Deliver artwork in AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 at ≥300 DPI. Include 3 mm (0.118 in) bleed on all four edges, keep critical text and tables ≥3 mm (0.118 in) inside the trim line (≥4–5 mm / 0.157–0.197 in for bordered layouts), set fine text to 100% K, cap total area coverage at TAC ≤280%–300%, and keep spot finishes on separate vector layers.
- Offset printing and surface finish: Print sheets on 200–300 gsm coated art or blue-core stock with specialist offset and tabletop manufacturing partners. Apply aqueous coating or anti-scuff matte lamination on dark artwork to resist table abrasion.
- Trimming and corner finishing: Guillotine-trim to final dimensions or die-cut to shape. Apply R3–R3.5 mm (0.118–0.138 in) corner rounding where specified.
- Collation and flat box packing: Jog player sets to uniform stacks, verify flat orientation inside the box cavity or insert recess, and pack without bending or creasing corners.
Sign-Off Criteria
- Trim dimensions match the target box-cavity footprint with 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) vertical stack clearance.
- Paper grain runs parallel to the long edge; finished sheets lie flat on a level surface without edge lift.
- Fine text (100% K) and small iconography render crisp without haloing or registration shift, and bordered frames remain visually even after trimming.
- Rounded corners (R3–R3.5 mm / 0.118–0.138 in) are smooth and free of die-nick burrs.
Concrete Failure Modes
- Edge curl and table sag: Caused by selecting 200 gsm stock on an oversized footprint, running paper grain perpendicular to the long edge, or applying single-sided film lamination that pulls the sheet toward the laminated face. Fix by stepping up to 280–300 gsm, aligning grain with the long dimension, and laminating both faces equally.
- Corner dog-earing and delamination: Sharp 90-degree corners on 200–250 gsm sheets fray quickly when slid across playmats or packed tightly against box walls. Fix by specifying R3–R3.5 mm (0.118–0.138 in) corners and maintaining 1.5–2.5 mm (0.059–0.098 in) perimeter clearance.
- Uneven border margins: Narrow borders placed within 3 mm (0.118 in) of the trim line expose slight guillotine draw variance. Fix by keeping bordered designs ≥4–5 mm (0.157–0.197 in) inside the trim edge.
- Surface scuffing on dark solids: Uncoated or standard gloss-varnished dark backgrounds show white friction marks after repeated stacking and sliding. Fix by specifying rich black (C40–60 M30–40 Y30–40 K100) within TAC ≤280%–300% and finishing with anti-scuff matte lamination.
- Box-pinch or warped sheets: Sizing a flat sheet to the exact nominal box interior without subtracting 1.5–2.5 mm (0.059–0.098 in) causes the sheet edges to wedge against corner gussets or trays during automated or manual packing. Fix by enforcing the full clearance allowance on both width and height.
Parent guide Standalone Quick-Reference Sheets