Uncoated writing stocks (80–120 gsm) absorb liquid compound faster than coated stocks, which narrows the margin against deep wicking. Thicker pads carry more stack weight in kg/lb and require firmer shear adhesion at the head, whereas pads using a perforated stub rather than direct head-peeling shift the mechanical release load from the glue film to the perforation rule.
Specifications and Tolerance Targets
| Tolerance Area | Governing Variables | Target Physical Condition |
|---|---|---|
| Adhesive edge penetration | Compound viscosity, clamping pressure, sheet porosity | 1 to 2 mm (0.04 to 0.08 in) max wicking from head edge; clear of ≥3 mm (0.118 in) safety zone |
| Backing-board flushness | Jogging squareness, board caliper, guillotine clamp pressure | Flush head and trimmed edges across sheets and backing board; zero step or recess |
| Perforation cut-to-tie ratio | Sheet gsm/caliper, pad weight in kg/lb, grain direction | Clean single-sheet tear along the rule without ripping the grid or splitting in transit |
Paper Weights, Calipers, and Backing Boards
- Interior scorepad sheets: 80–120 gsm (about 0.08–0.13 mm, or 0.003–0.005 in, per sheet). In US basis weights, this corresponds to roughly 54–81 lb Text (measured on a 25 × 38 in / 635 × 965 mm basis sheet).
- Cardstock backing: 200–300 gsm (roughly 74–111 lb Cover, measured on a 20 × 26 in / 508 × 660 mm basis sheet, distinct from Text LB).
- Rigid greyboard backing: 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in) caliper when the pad doubles as a standalone writing surface.
- Stack weight and handling: Heavy multi-pad cartons (measured in kg/lb) and thick 50- to 100-sheet pads place higher shear stress on the head bond and perforation ties during shipping.
Prepress and Layout Margins
- Supply print files as PDF/X-1a or PDF/X-4 (from AI/PDF/PSD) with outlined or embedded fonts, CMYK plus any spot layers, and ≥300 DPI resolution.
- Include 3 mm (0.118 in) bleed on trimmed edges and keep all score grids, numbers, and rules at least ≥3 mm (0.118 in) inside the trim and perforation line so 1 to 2 mm (0.04 to 0.08 in) adhesive wicking never reaches printed ink.
- Use 100% K for fine grid lines and small score text; keep rich black (C40–60 M30–40 Y30–40 K100) and total area coverage (TAC ≤280%–300%) away from the glued head edge so heavy ink does not repel the padding compound.
Production Steps
- Print and perforate sheets: Print sheets with grain running parallel to the tear direction where possible, and apply inline or offline micro-perforation rules clear of the ≥3 mm (0.118 in) safety margin.
- Collate and jog with backing: Place the 200–300 gsm cover backing or 1.5–3 mm (0.059–0.118 in) greyboard under the sheet stack and jog all lifts square against the head stop.
- Clamp under weight: Compress the stack evenly at the head edge so air gaps between sheets close before gluing; uneven clamping lets liquid compound wick past 2 mm (0.08 in).
- Apply padding compound: Brush or roll flexible padding adhesive across the compressed head edge in controlled passes, bridging the top sheet through the bottom sheet and onto the backing-board edge.
- Cure and three-side trim: Allow the adhesive film to cure fully before cutting pads apart and trimming the three unglued sides flush on a guillotine, keeping the backing board aligned with the paper block.
Sign-Off Criteria
- Head penetration check: Peel sheets from the top, middle, and bottom of a sample pad and measure adhesive penetration from the head edge; wicking must stay within 1 to 2 mm (0.04 to 0.08 in) and remain outside the printable score grid.
- Flushness inspection: Run a finger across all four edges of the finished pad; the backing board must sit flush with the sheet stack at the glued head and trimmed sides, with the bottom sheet firmly anchored.
- Tear and retention check: Tear individual sheets from multiple depths in the stack. Direct-peel sheets must release cleanly without leaving paper fibers on the spine or pulling adjacent sheets loose; perforated sheets must separate cleanly along the rule while the stub remains bonded.
Concrete Failure Modes
- Deep adhesive wicking (>2 mm / >0.08 in): Caused by low-viscosity compound, loose stack clamping, or highly absorbent uncoated 80–120 gsm stock. Results in stiffened corners, torn top margins, or glue-stained score boxes.
- Unbonded bottom sheets: Caused by a recessed backing board or incomplete adhesive coverage across the bottom edge of the stack. Results in the last few sheets detaching before use.
- Backing-board step or lip: Caused by shifting during final guillotine trimming when soft 80–120 gsm sheets compress more than rigid 1.5–3 mm (0.059–0.118 in) greyboard. Creates an overhang that snags during box packing.
- Zipper-tearing or transit splitting: A cut-to-tie ratio with ties too long for 100–120 gsm stock forces the tear path into the printed grid; ties too short for 80 gsm stock or heavy cartons (kg/lb) cause sheets to split prematurely in transit.
Parent guide Booklet Binding, Spine, and Box-Fit Tolerances