For outer print substrates, barrier layers, and overall web structures, see Foil Laminate Pack Films.
Inner Liner Coating Specifications
| Property | Heat-Seal Inner Layer (PE / CPP) | Pattern-Applied Cold-Seal Cohesive |
|---|---|---|
| Sealing mechanism | Thermal melt under heated jaw pressure and dwell, followed by cooling | Pressure-only cohesive bond (cohesive-to-cohesive) at ambient temperature |
| Coating coverage | Full-width continuous inner sealant film | Pattern-coated strictly to longitudinal fin and transverse end-seal zones |
| Thermal transfer risk | High if heated jaws contact or dwell close to the card stack | None during sealing; zero heat applied at the crimping station |
| Card cavity surface | Smooth, non-tacky PE or CPP across the entire interior | Uncoated film in the card pocket; cohesive restricted to seal margins |
| Roll storage sensitivity | Stable at standard ambient warehouse conditions; low blocking risk | Sensitive to elevated temperature, humidity, and excessive rewind tension |
| Outer-web requirement | Heat-resistant outer print or overprint varnish to prevent jaw sticking | Release lacquer (OPV) on the outer face where it contacts cohesive wraps |
Sealing Constraints by Card Stock
- Heat-seal headspace clearance: Thermal jaws must clamp and dwell strictly in the empty pouch margin beyond the card stack. If the pouch length is tight, conductive and radiant heat transfers into the cards during jaw dwell, which can soften double-sided card film (0.03–0.05 mm / 0.0012–0.0020 in per card) or cause edge curl in 300–400 gsm paper cores and 0.30 mm (0.012 in) PVC cards.
- Cold-seal zero-heat advantage: Because cold-seal cohesive bonds solely under nip pressure, the card stack can sit closer to the crimp line without thermal distortion, and line stops do not leave cards resting under heated jaws.
- Slip and surface energy: PE and CPP inner layers rely on controlled slip additives so cards slide smoothly during insertion without scuffing, whereas cold-seal webs keep the interior card pocket uncoated and friction-free while confining tackiness to the outer perimeter.
Production Steps
- Select the sealant system against card sensitivity and line type: Match PE or CPP continuous sealant webs to thermal form-fill-seal equipment with sufficient headspace margin; assign pattern-applied cold-seal cohesive to pressure-only lines or heat-sensitive card builds.
- Define seal-zone geometry and pattern registration:
- For heat-seal, set pouch cut-off length and card-stop tolerances so the heated transverse jaws close completely clear of the card edge.
- For cold-seal, generate a dedicated pattern-coat separation aligned strictly to the longitudinal fin seal and transverse end-seal bands, leaving the entire interior card cavity uncoated.
- Convert and wind the roll stock:
- Lamination bonds the continuous PE or CPP film to the barrier web, or applies the cold-seal cohesive in register over the inner web while pairing the outer print surface with a compatible release lacquer.
- Wind finished rolls under controlled tension; cold-seal rolls require lower, uniform rewind tension and climate-controlled storage to prevent wrap-to-wrap blocking.
- Form, fill, and seal pouches:
- Heat-seal lines: Balance jaw temperature, dwell time, and jaw pressure so the inner PE/CPP layer melts cleanly without scorching the outer laminate.
- Cold-seal lines: Set rotary or linear nip pressure and line speed to activate the cohesive-to-cohesive bond across both flat seals and the fin T-junction.
Sign-Off Criteria
- Continuous perimeter seal: Longitudinal fin and transverse end seals fuse uniformly across the full width, including the overlapping T-junction, with no open micro-channels.
- Clean card surfaces: Enclosed cards show zero thermal warping, edge softening, film blocking, or cohesive adhesive transfer after sealing.
- In-register cold-seal pattern: Pattern-coated cohesive remains confined to the designated fin and end-seal zones with clean, adhesive-free margins around the card pocket.
- Clean roll unwind: Stored rolls unwind smoothly without cohesive pick-off, outer-ink lifting, or wrap-to-wrap blocking.
Failure Modes
- Thermal card marking or edge curl (Heat-seal): Heated jaws closing too close to the card stack, or excessive dwell during line slowdowns, transfers heat into the pouch and warps 300–400 gsm paper stocks, deforms 0.30 mm (0.012 in) PVC cards, or softens double-sided card lamination.
- Roll blocking in storage (Cold-seal): High warehouse temperatures, high humidity, excessive rewind tension, or an incompatible outer release lacquer causes the pattern-applied cohesive to bond to the back of the next wrap, tearing outer graphics or starving the seal zone on unwind.
- Cohesive residue inside the card pocket (Cold-seal): Misregistered pattern coating extends past the crimp margin into the interior cavity, causing cards to stick to the inner liner during insertion or removal.
- T-junction channel leaks (Heat-seal and Cold-seal): Insufficient nip pressure at the step change where the longitudinal fin folds over the transverse seal leaves a narrow unsealed tunnel, allowing moisture ingress or premature pouch opening.
- Inner-liner delamination or outer-web burn-through (Heat-seal): Jaw temperatures set above the outer film's thermal limit scorch the exterior print, while over-heated or over-pressured PE/CPP layers squeeze out from the seal zone and delaminate from the barrier layer.
Parent guide Foil and Metalized Booster Pack Laminates