Choose the stock by stack weight, artwork coverage, and box clearance:
- Uncoated stock (120–150 gsm / ~80–100 lb Text) suits light-to-medium decks with minimal ink coverage, offering high surface friction that keeps the band from sliding off bare cards.
- Matte-coated stock (150–216 gsm / ~100 lb Text to 80 lb Cover) suits full-bleed color, dark artwork, or fine typography; pair it with an aqueous matte or anti-scuff matte varnish to prevent ink transfer onto the top and bottom cards.
- Kraft paper (120–176 gsm / ~80 lb Text to 65 lb Cover) suits high-tension wraps on thicker or heavier stacks because long unbleached fibers resist tearing along score lines.
For broader component material options, see booster materials. Standard offset card production starts at 200 decks (usual tiers 200/300/500/1,000+), while boxed games and custom band tooling follow project and component minimums.
Paper Stock and Basis-Weight Specifications
Paper belly bands sit between interior text sheets and heavy cover boards. Distinguish US Text LB from US Cover LB by basis sheet size, since identical pound ratings represent different thicknesses and weights:
| Stock Type | Typical Grade (gsm) | US Basis Weight & Sheet Size | Ream Weight (kg / lb per 500 sheets) | Approximate Caliper (mm / in) | Best Fit |
|---|---|---|---|---|---|
| Uncoated offset / bond | 120–150 gsm | 80–100 lb Text (25 × 38 in / 635 × 965 mm) | 36.3–45.4 kg / 80–100 lb | 0.13–0.17 mm / 0.005–0.007 in | Low-ink text bands, high natural friction |
| Matte-coated art | 150–216 gsm | 100 lb Text (25 × 38 in) to 80 lb Cover (20 × 26 in / 508 × 660 mm) | 36.3–45.4 kg / 80–100 lb | 0.13–0.20 mm / 0.005–0.008 in | Full-bleed CMYK, dark solids, barcodes |
| Unbleached / dyed kraft | 120–176 gsm | 80 lb Text (25 × 38 in) to 65 lb Cover (20 × 26 in) | 29.5–36.3 kg / 65–80 lb | 0.14–0.21 mm / 0.006–0.008 in | Heavy stacks, tight corners, plastic-free look |
| Heavy cover (scored) | 250–270 gsm | 92–100 lb Cover (20 × 26 in / 508 × 660 mm) | 41.7–45.4 kg / 92–100 lb | 0.24–0.28 mm / 0.009–0.011 in | Wide bands requiring rigid crease geometry |
Reference conversion formulas (plain text):
gsm = (Text LB * 453.592) / (25 * 38 * 0.00064516) = Text LB * 1.48gsm = (Cover LB * 453.592) / (20 * 26 * 0.00064516) = Cover LB * 2.70inches = mm / 25.4
Grain Orientation and Structural Tolerances
- Grain direction: Align paper grain parallel to the wrap loop (running around the four sides of the card stack, perpendicular to the four fold creases). When grain runs parallel to the loop, the fibers bend cleanly around the stack edges without splitting.
- Inner surface finish: Leave the inside face unprinted whenever possible. If double-sided printing is required, keep the inner face free of heavy ink coverage near the card-contact zone or seal it with a matte aqueous coating.
- Overlap and glue flap: Size the overlap tab to 15–20 mm (0.591–0.787 in) for consistent adhesive contact without pressing a hard step into the card faces.
- Box clearance: Account for the band's double thickness (including the overlap seam) when sizing the outer tuck or rigid box. Standard box clearance is 1.5–2.5 mm (0.059–0.098 in) across width and height and 1.5–3 mm (0.059–0.118 in) for stack height; a 0.20 mm (0.008 in) band adds 0.40 mm (0.016 in) at the single layer and 0.60 mm (0.024 in) at the overlap.
- Card-stack compressibility: Bare card stacks vary slightly in caliper by stock—from 0.28–0.31 mm (0.011–0.012 in) per card on 300 gsm art/blue core up to 0.40–0.44 mm (0.016–0.017 in) on 400 gsm stock, plus 0.03–0.05 mm (0.001–0.002 in) per card when double-sided film is applied. Measure the compressed stack height of the actual production stock before locking the band dieline.
Prepress and Production Steps
- Prepress file setup: Supply artwork in AI, PDF, or PSD format exported as PDF/X-1a or PDF/X-4 at ≥300 DPI. Outline or embed all fonts.
- Bleed and safety margins: Include 3 mm (0.118 in) bleed per side on the band dieline and keep critical text or barcodes ≥3 mm (0.118 in) inside trim and fold lines (≥4–5 mm / 0.157–0.197 in for bordered designs).
- Color and ink limits: Use CMYK with separate spot layers for any Pantone or foil elements. Set fine text to 100% K, use rich black (C40–60 M30–40 Y30–40 K100) for large dark areas, and cap total area coverage (TAC) at ≤280%–300%. Apply anti-scuff matte varnish over dark artwork.
- Grain-aligned imposition: Nest band blanks on the press sheet so the long wrap axis runs parallel to the sheet's grain direction.
- Scoring and die-cutting: Crease stocks ≥176 gsm (65 lb Cover) with a channel score before folding; lighter 120–150 gsm (80–100 lb Text) bands wrap smoothly with light score lines or soft-creased folds.
- Wrapping and closure: Wrap the band snugly around the compressed card stack and bond the overlap tab with hot-melt or cold-set PVA adhesive, keeping glue away from the card edges.
Sign-Off Criteria
Verify the following on pre-production physical samples wrapped around the actual card stock:
- Zero fold cracking: Outer ink and coating remain intact along all four 90-degree stack corners without white fiber show-through.
- Clean inner contact: Rubbing the wrapped band across the top and bottom cards leaves no ink transfer, pigment dusting, or coating scuff.
- Controlled slip resistance: The band holds the stack together when lifted by one end, yet slides off or tears open cleanly without denting card corners.
- Box insertion fit: The banded stack slides into its outer box within the 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) height clearance without catching on the overlap seam.
Failure Modes and Causes
- Corner cracking along folds: Caused by cross-grain imposition (grain running parallel to the fold lines instead of the wrap loop), overly heavy cover stock (≥250 gsm / ≥92 lb Cover) without channel scoring, or brittle UV/thick film lamination on tight 90-degree bends.
- Ink rub onto bare cards: Caused by unsealed CMYK or rich black ink printed on the inside face, high TAC (>300%) on matte-coated stock without anti-scuff varnish, or stacking bands before ink fully cures.
- Band tearing or popping open: Caused by insufficient overlap (<15 mm / 0.591 in), adhesive applied over unvarnished slick coating that fails to bond, or sharp card edges cutting into low-tear uncoated stock under tight wrap tension.
- Stack bowing or box binding: Caused by wrapping too tightly around a tall deck, or failing to deduct the band's double-wall overlap thickness from the outer box's 1.5–3 mm (0.059–0.118 in) stack-height clearance.
Packaging and Regulatory Records
Replacing plastic shrink wrap with paper belly bands affects packaging waste reporting and sorting marks depending on destination markets:
- Germany (VerpackG / LUCID): Paper bands count as sales packaging; producers placing packaged decks on the German market maintain registration and volume reporting records with the Zentrale Stelle Verpackungsregister.
- France (Triman / Info-tri): Paper packaging sold to French consumers requires applicable sorting signage and material-stream records per Info-tri guidance.
- EU Toy Safety (EN 71): When card decks and their paper bands are intended for children, maintain applicable assessment and testing documentation under the EU Toy Safety framework.
Parent guide Booster Pack and Wrapper Materials