Use an L-bar sealer with a heat tunnel for single cartonless decks or retail-facing bundles that require full-perimeter enclosure and clean edge seams. Use a sleeve wrapper with a heat tunnel for multi-pack bricks or bulk transit bundles where an overlap bottom/side weld and higher film tension hold stacked decks together without an outer carton. For alternative pack formats and outer-wrapper choices, see booster and pack structures.
Enclosure Specifications and Physical Fit
Cartonless shrink enclosures rely on the deck itself as the structural form. Because there is no folding carton or rigid box to absorb film tension, film choice, seam placement, and stack geometry directly control edge integrity.
| Parameter | Single Cartonless Deck (L-Bar) | Multi-Pack Brick (Sleeve-Tunnel) | Physical Driver |
|---|---|---|---|
| Enclosure Coverage | Full four-sided perimeter weld | Sleeve wrap with overlap seal or bullseye ends | Single decks need dust/moisture protection; bricks need bundling tension |
| Seam Placement | Mid-edge along card thickness | Centered on broad face or flat stack side | Keeps weld lines off card corners to prevent seam splits |
| Air Evacuation | Micro-perforated vent pinholes | Open ends or spaced vent pinholes | Releases trapped air during tunnel shrink to prevent ballooning |
| Corner Interface | Relies on R3–R3.5 mm (0.118–0.138 in) card corners | Combined stack corners take higher hoop stress | Tighter or square corners concentrate stress and puncture film |
| Opening Feature | Optional tear tape or notched pull | Tear strip or slit-to-open brick wrap | Allows opening without nicking exposed card edges |
Stack Dimensions and Card Caliper Allowance
Shrink-film layflat width and tunnel dwell depend on the finished deck block rather than a single default trim size. For any card format, calculate the uncompressed stack height before setting film width and sealer frame clearance:
Stack height = Card count x (Base card caliper + Film allowance)
Typical card calipers from offset production runs:
- 300 gsm art or blue core: 0.28–0.31 mm (0.011–0.012 in) per card
- 310 gsm black-core linen: 0.30–0.32 mm (0.012–0.013 in) per card
- 330 gsm black core: 0.32–0.34 mm (0.013 in) per card
- 350 gsm art stock: 0.34–0.38 mm (0.013–0.015 in) per card
- 400 gsm art stock: 0.40–0.44 mm (0.016–0.017 in) per card
- PVC stock: 0.30 mm (0.012 in) per card
- Double-sided lamination/film: adds 0.03–0.05 mm (0.001–0.002 in) per card
When decks ship without an outer carton, master-carton weight limits and inner dividers matter because exposed shrink film transfers stacking loads directly to card edges. Keep master-carton gross weights within standard handling limits (such as 15–20 kg / 33–44 lb) with corrugated pads between layers so upper bricks do not dent lower decks.
Regulatory and Labeling Records
When cartonless shrink-wrapped decks are placed on the market as retail units or transport-only bundles, packaging and product compliance records follow the destination market's rules:
- Germany (VerpackG): Producers and first distributors placing packaged goods on the German market register and report packaging volumes through the Central Agency Packaging Register (ZSVR VerpackG system information).
- France (Triman / Info-Tri): Consumer-facing packaging requires sorting signage and material separation instructions printed on the pack or an enclosed/affixed label when no outer carton exists (French Ministry Triman guidance).
- EU Toy Safety (EN 71): Where a deck or its accessible film packaging falls under toy-safety scope, conformity requires applicable EN 71 assessment and testing records (European Commission toy safety framework).
Production Steps
- Deck jogging and collation: Square the finished, corner-rounded cards into a flush block so no single card protrudes past the stack face.
- Pinholing and film feed: Perforate the roll with fine vent pinholes spaced to match the deck footprint, avoiding direct alignment over delicate foil or uncoated paper edges.
- Sealing: Wrap the deck or brick and actuate the L-bar or sleeve sealer so the weld line lands along the flat edge of the stack thickness, clear of all four corners.
- Heat-tunnel shrink: Pass the sealed unit through the heat tunnel at controlled air velocity and dwell time so the film tightens evenly across both broad faces without overheating the outer cards.
- Cooling and pack-out: Let the film cool and set flat on the exit conveyor before stacking decks into master cartons with protective pads.
Sign-Off Criteria
- Seam position: Weld lines sit along the flat stack edge or broad face, never crossing a corner radius.
- Weld continuity: Seams hold under normal handling tension without pinholes tearing open along the seal line.
- Air release: Broad faces lie flat with no trapped air pockets or pillowed edges.
- Card flatness: Top and bottom cards remain flat with no heat-induced curl or bowed edges.
- Edge integrity: Card corners and gilt or dark-printed edges show no film-burn marks, scuffing, or crushed edges.
Failure Modes
- Corner splits and punctures: Weld seams routed across card corners, or film shrunk too tightly over sharp or unrounded corners, tear during packing and transit.
- Ballooning and fish-eyes: Missing, clogged, or poorly spaced vent pinholes trap expanding air in the heat tunnel, leaving loose bubbles or uneven shrink wrinkles.
- Card bowing (potato-chipping): Excessive tunnel dwell time or overly high shrink tension pulls the outer cards inward, curving the deck block.
- Open or brittle welds: Contaminated seal blades, uneven platen pressure, or incorrect seal dwell leave weak seams that pop open when bricks are lifted.
- Surface scuffing on cartonless packs: Exposed decks rubbing directly against rough corrugated master-carton walls abrade the shrink film and wear ink off outer card edges when layer pads or dividers are omitted.