Two construction paths change how the tray performs:
- Folded double-wall (roll-over) trays fold a scored paperboard or thin rigid-board flap 180 degrees over the top rim and lock it against the inner tray floor. This creates a smooth, rounded top edge that resists delamination and guides the tray into the sleeve without catching.
- Laminated double-wall rigid trays glue a secondary greyboard or paperboard liner to the interior or exterior of a scored greyboard core. This maximizes compression strength and square 90-degree corners for heavy stacks, but adds glue-line thickness and requires wider outer-sleeve clearance.
Single-wall trays remain sufficient for lightweight single decks with generous sleeve clearance, where doubling the wall thickness would unnecessarily widen the outer sleeve footprint. Boxed games and custom tray tooling follow project and component minimums rather than standard deck tiers.
Structural and Material Specifications
Double-wall trays must balance wall stiffness against the total outer width and height so the tray slides smoothly inside the rigid outer sleeve without rattling or jamming.
| Parameter | Manufacturing Specification | Production Impact |
|---|---|---|
| Rigid Core (Greyboard) | 1.5 mm (0.059 in), 2.0 mm (0.079 in), 2.5 mm (0.098 in), or 3.0 mm (0.118 in) | Sets baseline wall stiffness; double-wall builds double the effective wall thickness minus any V-groove or compression allowance |
| Internal Width & Height Clearance | 1.5–2.5 mm (0.059–0.098 in) across card deck width and height | Prevents decks from wedging against the inner wall and bowing the tray outward |
| Internal Stack Height Clearance | 1.5–3.0 mm (0.059–0.118 in) above total deck height | Leaves finger-access room and prevents top card edges from dragging on the outer sleeve |
| Wrap Margin | 15–20 mm (0.591–0.787 in) turn-in onto interior walls | Anchors printed wrap paper around the double-thickness rim without peeling during repeated sliding |
| Wrap Bleed & Safety | 3 mm (0.118 in) bleed per side; >= 3 mm (0.118 in) safety | Keeps artwork and solid ink coverage continuous across folded or laminated rims |
| Prepress & Color | CMYK with separate spot layers, >= 300 DPI, PDF/X-1a or PDF/X-4, TAC <= 280%–300% | Controls ink load on wrap folds; anti-scuff matte film suits dark artwork subjected to sleeve friction |
Stack Height and Wall-Thickness Sizing
Account for both card caliper and lamination before locking the tray wall height:
- Card caliper range: 300 gsm art or blue-core stock measures 0.28–0.31 mm (0.011–0.012 in) per card, 310 gsm black-core linen measures 0.30–0.32 mm (0.012–0.013 in), 330 gsm black core measures 0.32–0.34 mm (0.013–0.013 in), 350 gsm art stock measures 0.34–0.38 mm (0.013–0.015 in), 400 gsm measures 0.40–0.44 mm (0.016–0.017 in), and PVC measures 0.30 mm (0.012 in). Double-sided film lamination adds 0.03–0.05 mm (0.001–0.002 in) per card.
- Plain-text tray sizing formulas:
Tray Inner Height = (Card Count * Caliper per Card) + 1.5 to 3.0 mm (0.059 to 0.118 in)Tray Outer Width = Deck Width + (2 * Inner Clearance) + (2 * Double-Wall Thickness)
When specifying wrap or liner stocks in US weights, distinguish basis sheet sizes: US Cover LB uses a 20 x 26 in (508 x 660 mm) basis sheet, whereas US Text LB uses a 25 x 38 in (635 x 965 mm) basis sheet. A 100 lb Text sheet is substantially lighter and thinner than a 100 lb Cover sheet; match wrap thickness to the tightest fold radius of the double-wall rim.
For wraps using rich black on dark tray edges, specify C40–60 M30–40 Y30–40 K100 with total area coverage (TAC) at or below 280%–300%, and keep fine text at 100% K with fonts outlined or embedded in AI, PDF, or PSD source files.
Production Steps
- Structural Dieline & Clearance Mapping: Calculate the tray inner cavity from actual deck dimensions plus 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3.0 mm (0.059–0.118 in) stack height clearance. Size the outer sleeve to accommodate the full doubled wall thickness plus sliding tolerance.
- Board Cutting & Scoring / V-Grooving: Die-cut or V-groove the greyboard or heavy paperboard blank. For folded double-wall trays, place twin parallel scores across the top rim width so the inner flap folds flat against the outer wall without bulging.
- Wrap Printing & Surface Protection: Print wrap sheets in CMYK (plus spot layers if specified) at >= 300 DPI with 3 mm (0.118 in) bleed. Apply anti-scuff matte lamination on dark wraps to prevent burnishing where the tray rubs the outer sleeve.
- Wall Doubling & Wrapping:
- Folded method: Wrap the exterior face with a 15–20 mm (0.591–0.787 in) turn-in, then fold the doubled side flaps inward and lock or glue them flush to the tray floor.
- Laminated method: Bond the secondary wall liner to the primary greyboard wall under uniform press pressure before applying the outer wrap, keeping glue spread even to avoid warped panels.
- Tray-to-Sleeve Pairing: Mate finished inner trays with their rigid outer sleeves and cycle the drawer action under full deck weight to confirm smooth travel.
Sign-Off Criteria
- Squareness & Edge Geometry: All four vertical corners hold 90-degree alignment without inward bowing along the top rim or outward splay at the base.
- Sliding Resistance: With a full card stack loaded, the tray slides smoothly into and out of the outer sleeve with consistent light friction and no corner catching.
- Rim & Wrap Integrity: The 15–20 mm (0.591–0.787 in) wrap turn-in lies flat inside the cavity with zero edge lift, bubbling, or cracking along the doubled top fold.
- Deck Fit: Decks drop in and lift out within the 1.5–2.5 mm (0.059–0.098 in) lateral clearance and 1.5–3.0 mm (0.059–0.118 in) height clearance without compressing card corners.
Concrete Failure Modes
- Inward Wall Bowing and Sleeve Binding: If the tray relies on thin board or incomplete lamination across a long span, heavy deck weight pulls the side walls inward or lets the outer sleeve pinch the top rim, causing the drawer to jam mid-pull.
- Thick-Rim Wrap Cracking: Folding heavy Cover-weight wrap stock or high-TAC ink over a tight double-wall top edge fractures the paper fibers and exposes raw greyboard along the rim.
- Delamination at the Doubled Flap: Insufficient adhesive or short turn-in margins (< 15 mm / 0.591 in) allow the inner folded wall to spring back, narrowing the card cavity and snagging deck corners.
- Sleeve Drag from Unaccounted Glue/Wrap Thickness: Sizing the outer sleeve from nominal greyboard thickness without adding adhesive layers and wrap caliper creates an overly tight fit that scuffs dark matte surfaces during sliding.
Parent guide Drawer and Slide Box Structures