The exact gap width changes with four physical conditions:

  • Greyboard caliper: Thicker boards (1.5 mm, 2.0 mm, 2.5 mm, or 3.0 mm / 0.059 in, 0.079 in, 0.098 in, or 0.118 in) displace more material as they rotate, requiring wider channels.
  • Fold angle: The back-to-spine and spine-to-lid hinges typically open to 180° when laid flat, whereas the lid-to-flap hinge bends 90° over the front wall.
  • Wrap and liner thickness: Heavier wrap stocks, double-sided lamination films, and thick inner liners consume radius inside the channel.
  • Grain direction: Wrap paper and greyboard grain running parallel to the hinge channels flexes cleanly; cross-grain fibers resist bending and split along the score.

For overall box construction, magnet placement, and tray attachment, see magnetic hinged boxes.


Specifications and Hinge Sizing

Board Calipers and Box Clearances

Parameter Metric Specification Imperial Equivalent Role in Hinge Geometry
Greyboard caliper options 1.5 / 2.0 / 2.5 / 3.0 mm 0.059 / 0.079 / 0.098 / 0.118 in Sets minimum hinge channel width and lid rigidity
Wrap turn-in margin 15–20 mm 0.591–0.787 in Anchors outer wrap around board edges without lifting
Inner tray width/height clearance 1.5–2.5 mm 0.059–0.098 in Prevents deck or insert bind from distorting the spine
Inner tray stack height clearance 1.5–3.0 mm 0.059–0.118 in Ensures lid sits level so the magnetic flap aligns squarely
Wrap sheet bleed 3 mm per side 0.118 in per side Covers trim and wrap-around variance

Plain-Text Geometry Formulas

Use the greyboard thickness as the baseline for spacing every hinge channel:

  • 90° flap hinge channel: Flap channel width = (1.5 to 2.0) * Board thickness + Wrap and liner allowance
  • 180° spine hinge channels (back-to-spine and spine-to-lid): Spine channel width = (2.0 to 2.5) * Board thickness + Wrap and liner allowance
  • Total outer wrap span (left to right across the spine): Total wrap span = Back panel + Spine channel + Spine board + Spine channel + Front lid + Flap channel + Magnetic flap + (2 * Wrap margin)

As a working rule, stepping up from 1.5 mm (0.059 in) greyboard to 3.0 mm (0.118 in) greyboard roughly doubles the required channel width. When a rigid inner tray is glued flush against the back-to-spine edge, add 0.5–1.0 mm (0.020–0.039 in) to the spine-to-lid channel if the tray wall crowds the fold.

Wrap Paper, Grain, and Prepress Specs

  • Paper weight and basis: Specify wrap sheets in gsm and keep US basis weights distinct by sheet size—US Text LB is measured on a 25 × 38 in (635 × 965 mm) basis sheet, whereas US Cover LB is measured on a 20 × 26 in (508 × 660 mm) basis sheet. Flexible Text-weight wraps conform cleanly into narrow hinge channels; stiff Cover-weight stocks resist tight radii and crack under repeated flexing.
  • Lamination: Double-sided film adds 0.03–0.05 mm (0.001–0.002 in) to sheet thickness. Anti-scuff matte lamination is recommended over dark artwork to prevent burnishing and scuff lines along high-flex hinge channels.
  • File and color setup: Supply AI, PDF, or PSD artwork as PDF/X-1a or PDF/X-4 at ≥300 DPI with 3 mm (0.118 in) bleed per side, outlined or embedded fonts, CMYK plus separate spot layers, 100% K for fine text, rich black at C40–60 M30–40 Y30–40 K100, and total area coverage (TAC) ≤280%–300%.

Production Steps

  1. Select board caliper from box footprint and contents mass: Match 1.5–2.0 mm (0.059–0.079 in) greyboard to compact single-deck boxes (light contents under ~0.5 kg / 1.1 lb) and 2.5–3.0 mm (0.098–0.118 in) greyboard to wide or heavy multi-deck boxes (1.0 kg / 2.2 lb or heavier) so the lid does not bow across the span.
  2. Draft the multi-panel board layout: Plot the back panel, spine, front lid, and magnetic flap on one continuous layout separated by the calibrated hinge channels. Align the board grain parallel to the spine.
  3. Prepare and print the outer wrap sheet: Orient wrap paper grain parallel to the spine channels. Keep TAC ≤280%–300% across hinge zones so heavy ink layers do not crack when folded, and apply anti-scuff matte film on dark wraps.
  4. Cut greyboard panels and mount to the wrap: Die-cut or V-groove/mill the panels cleanly with square edges, then mount them onto the glued wrap sheet in a single registration pass so channel widths stay uniform from head to tail. Fold and press the 15–20 mm (0.591–0.787 in) turn-in margins flat.
  5. Seat magnets and press the inner liner into the channels: Embed magnets flush in the flap and front wall, then apply the inner liner and press it firmly down into each hinge trough before the adhesive sets. Verify 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3.0 mm (0.059–0.118 in) stack height clearance for the inner tray or card stack.

Sign-Off Criteria

  • Flat-open lid travel: The front lid opens 180° onto the work surface without lifting the base tray, straining the spine wrap, or pinching the inner liner.
  • Square magnetic closure: The 90° flap folds cleanly over the front wall and seats flush against the catch magnets without twisting or leaving a gap at either corner.
  • Consistent channel alignment: Hinge gaps measure evenly along the full spine and flap length with no visible board drift or skewed panels.
  • Clean flex surface: Repeated opening and closing produces no white stress lines, film delamination, ink cracking, or liner tenting inside the hinge troughs.

Concrete Failure Modes

  • Channel too narrow for board caliper: Adjacent greyboard edges collide and pinch the outer wrap and inner liner as the lid opens, causing the wrap paper to split or the lamination film to whiten along the spine. Fix: Widen the channel in proportion to the 1.5–3.0 mm (0.059–0.118 in) board thickness and wrap caliper.
  • Channel too wide: Unsupported wrap paper and liner sag or wrinkle inside the gap, leaving the lid sloppy and causing the magnetic flap to miss alignment on the front wall. Fix: Tighten the channel to match the actual board thickness plus wrap/liner allowance.
  • Cross-grain wrap paper: Paper fibers running perpendicular to the spine resist folding and fracture along the hinge line after a few open-close cycles. Fix: Rotate the press sheet imposition so wrap grain runs parallel to the hinge channels.
  • Liner tenting across the hinge: If the inner liner is glued flat while the box is closed without pressing it into the channel trough, opening the lid pulls the liner taut and rips it away from the board edges. Fix: Press the liner into the open channel troughs during assembly and allow adhesive to tack before closing.