For most custom decks, choose full-bleed artwork with a 3 mm (0.118 in) bleed and >= 3 mm (0.118 in) safety margin when using guillotine trimming plus corner rounding, or step up to die-punching and >= 4–5 mm (0.157–0.197 in) safety margins when the design relies on thin printed borders, custom shapes, or tight card-to-card size uniformity. This choice changes with run volume (standard offset cards start at 200 decks, with usual tiers at 200, 300, 500, and 1,000+), stock caliper, lamination thickness, and whether the deck uses a rectangular trim or a custom die-cut profile. For broader card tolerance context across caliper, warp, and box fit, see Card Tolerances.

Centering Drift vs. Dimensional Repeatability

Cut quality splits into two separate physical tolerances that behave differently on press and in finishing:

  1. Print-to-cut centering drift (graphic alignment): The combined shift between where ink lands on the press sheet and where the blade or die cuts that sheet. Even when every card in a deck is cut to the exact same size, centering drift makes printed borders look wider on one side than the opposite side.
  2. Card-to-card dimensional repeatability (size uniformity): How closely individual cards match each other in width, height, squareness, and corner radius across a deck and across decks. High repeatability keeps stacked edges flush and preserves predictable fit inside boxes built with 1.5–2.5 mm (0.059–0.098 in) width/height clearance.

In plain terms, total graphic shift at any card edge follows:

Total Edge Shift = Press-Sheet Registration Variance + Cut-Position Alignment Variance

Because these two variances can add together in the same direction on a given sheet, safety margins must absorb the combined shift rather than just one step.

Specifications and Design Allowances

Use the following prepress and physical allowances to keep centering drift invisible and card dimensions repeatable across standard offset and tabletop card stocks:

Parameter Specification (Metric / Imperial) Production Role
Perimeter bleed 3 mm (0.118 in) per side Prevents unprinted white slivers when cut position shifts outward
Standard safety margin >= 3 mm (0.118 in) inside trim Protects text, indices, and icons from inward cut drift
Bordered-back safety margin >= 4–5 mm (0.157–0.197 in) inside trim Masks visible asymmetry from press and cut registration drift
Corner radius R3–R3.5 mm (0.118–0.138 in) Standard rounded card corner; removes extra area at corner arcs
Box width/height clearance 1.5–2.5 mm (0.059–0.098 in) Absorbs minor card-size variance without binding or rattling
Box stack-height clearance 1.5–3 mm (0.059–0.118 in) Absorbs cumulative card caliper and film-lamination variance

Stock thickness and surface film directly affect blade drag and clamp compression during cutting:

  • 300 gsm art / blue core: 0.28–0.31 mm (0.011–0.012 in) caliper
  • 310 gsm black-core linen: 0.30–0.32 mm (0.012–0.013 in) caliper
  • 330 gsm black core: 0.32–0.34 mm (0.013–0.013 in) caliper
  • 350 gsm art stock: 0.34–0.38 mm (0.013–0.015 in) caliper
  • 400 gsm stock: 0.40–0.44 mm (0.016–0.017 in) caliper
  • PVC stock: 0.30 mm (0.012 in) caliper
  • Double-sided film lamination: Adds 0.03–0.05 mm (0.001–0.002 in) per card

When specifying paper weight, gsm measures grams per square meter directly, whereas US Cover LB (based on a 20 × 26 in / 508 × 660 mm basis sheet) and US Text LB (based on a 25 × 38 in / 635 × 965 mm basis sheet) refer to different basis sheet sizes and cannot be compared without conversion. Prepare print files as PDF/X-1a or PDF/X-4 (from AI, PDF, or PSD sources) at >= 300 DPI in CMYK with separate non-printing spot layers for trim and die lines, outlined or embedded fonts, 100% K for fine text, and rich black (C40–60 M30–40 Y30–40 K100, TAC <= 280%–300%).

Production Steps: Guillotine Trimming vs. Die-Punching

  1. Press-sheet printing and registration: Offset cards print multiple-up on parent sheets with registration targets. Sheet-to-sheet feed variance and multi-color plate alignment establish the baseline graphic registration before cutting begins.
  2. Cutting method selection:
    • Guillotine trimming + corner rounding: Parent sheets are stacked into lifts, clamped, sliced into strips, and chopped into individual rectangles before a separate corner-rounding pass forms the R3–R3.5 mm (0.118–0.138 in) corners. Because the perimeter cut and corner cut happen on different stations, alignment between straight edges and corner arcs depends on careful stop setup and controlled lift heights.
    • Die-punching: A matched-metal or steel-rule die punches the card perimeter and R3–R3.5 mm (0.118–0.138 in) corners in a single stroke. Die-punching locks card-to-card dimensional repeatability and corner symmetry together, making it the standard choice for high uniformity and required for non-rectangular shapes.
  3. Other deck formats: For non-standard or custom-shaped deck formats, tooling and cut tolerances follow the custom die geometry and project minimums rather than a fixed default trim size. Maintain the 3 mm (0.118 in) outer bleed and >= 3 mm (0.118 in) (>= 4–5 mm / 0.157–0.197 in for bordered backs) safety clearance from the active cut path.

Sign-Off Criteria

  • Prepress sign-off: Confirm 3 mm (0.118 in) bleed extends cleanly beyond the trim box on all sides, no critical text or border line sits closer than 3 mm (0.118 in) (4–5 mm / 0.157–0.197 in for bordered backs), and die/cut paths sit on a separate non-printing spot layer.
  • Dimensional and visual cut check: Inspect cards sampled from the top, middle, and bottom of cut lifts (or across die cavities). Verify uniform card-to-card width and height when squared as a deck, smooth transitions where R3–R3.5 mm (0.118–0.138 in) corners meet straight edges, and even border balance on bordered backs.
  • Box-fit check: Confirm the finished deck slides into its paired box cleanly within the 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) stack-height clearance.

Concrete Failure Modes

  • Visibly uneven card borders: Caused by narrow printed borders amplifying normal press-sheet registration and cut-position drift. Fix: Move critical border lines inward to >= 4–5 mm (0.157–0.197 in) from trim or use full-bleed artwork.
  • White edge slivers after trimming: Caused by bleed stopping short of 3 mm (0.118 in) when the cut shifts outward. Fix: Extend all background colors, textures, and artwork to the full 3 mm (0.118 in) bleed boundary.
  • Stepped nibs at corner transitions: Caused by misalignment between guillotine straight cuts and a secondary corner-rounding station, or blade deflection on thick 350–400 gsm and laminated stock. Fix: Switch to single-stroke die-punching or recalibrate corner-rounder stops on smaller lifts.
  • Top-to-bottom size taper (blade draw): Caused by guillotine blade drag through overly tall lifts of slick laminated or 0.30 mm (0.012 in) PVC sheets, creating uneven deck edges and tight box fit. Fix: Reduce guillotine lift height, adjust clamp pressure, or move to die-punching.
  • Clipped corner indices or pips: Caused by placing elements 3 mm (0.118 in) from the straight edge without accounting for the inward curve of the R3–R3.5 mm (0.118–0.138 in) corner radius. Fix: Measure corner safety clearance from the corner arc rather than the theoretical sharp corner.