For how these tolerances integrate with overall insert geometry, materials, and structural styles, see the insert tolerances overview.

Tolerance Specifications by Fit Zone

Fit Zone Material / Condition Target Clearance or Interference Governing Physical Factors
Outer-wall to box interior Rigid paperboard or molded tray +1.5 to +2.5 mm (+0.059 to +0.098 in) width/length; +1.5 to +3 mm (+0.059 to +0.118 in) height Greyboard thickness (1.5 / 2 / 2.5 / 3 mm or 0.059 / 0.079 / 0.098 / 0.118 in) and 15–20 mm (0.591–0.787 in) wrap margins
Outer-wall to box interior Compressible foam block 0 to +1.0 mm (0 to +0.039 in) slip, or light friction Must not bow rigid greyboard walls or lift the lid
Card well (width & length) Unsleeved or sleeved deck in rigid well +1.5 to +2.5 mm (+0.059 to +0.098 in) over finished card or sleeve trim Card corner radius (R3–R3.5 mm / 0.118–0.138 in) and well corner fillets
Card well (stack depth) Full deck stack +1.5 to +3 mm (+0.059 to +0.118 in) over calculated stack height Card stock caliper plus double-sided film (+0.03–0.05 mm / +0.0012–0.0020 in per card)
Foam cavity Rigid components vs. paper decks Slight negative interference for dense pieces; neutral-to-light slip for cards Foam compression resistance without bowing card or tile edges
Divider-to-well Paperboard or plastic divider in card well Positive side slip within the +1.5 to +2.5 mm (+0.059 to +0.098 in) well allowance; tab below lid plane Divider caliper (typically 300–400 gsm Cover-weight stock) and slot/rail alignment

Outer-Wall (Insert-to-Box) Fit

An insert's outer perimeter is sized from the true internal cavity of the assembled box, not the external box dimensions. Rigid boxes built from 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in) greyboard lose internal width and height to board thickness plus the 15–20 mm (0.591–0.787 in) wrap margin folded over the rim. Maintaining 1.5–2.5 mm (0.059–0.098 in) of total slip clearance across width and height prevents the insert from scraping the interior wrap during insertion while keeping lateral rattle minimal. Vertically, reserving 1.5–3 mm (0.059–0.118 in) above the top of the insert and its contents ensures the lid seats flush without resting on divider tabs or booklet spines.

Compartment (Well-to-Content) Fit

Compartment width and length follow the finished trim of the largest item assigned to that well plus 1.5–2.5 mm (0.059–0.098 in) of finger-and-slip clearance. When a card well uses molded or routed rounded corners, the well's corner radius must exceed the card's R3–R3.5 mm (0.118–0.138 in) corner radius so corner fillets do not pinch card tips.

Stack depth must be calculated from actual stock caliper and surface finish rather than nominal gsm alone:

Well depth = ((card caliper + film allowance) * card count) + vertical clearance

Reference component thicknesses used in stack calculations:

  • Card stocks: 300 gsm art or blue core at 0.28–0.31 mm (0.011–0.012 in), 310 gsm black-core linen at 0.30–0.32 mm (0.012–0.013 in), 330 gsm black core at 0.32–0.34 mm (0.013–0.013 in), 350 gsm art stock at 0.34–0.38 mm (0.013–0.015 in), 400 gsm at 0.40–0.44 mm (0.016–0.017 in), and PVC at 0.30 mm (0.012 in).
  • Lamination buildup: Double-sided film adds 0.03–0.05 mm (0.0012–0.0020 in) per card, which shifts total stack height noticeably across multi-hundred-card decks.
  • Booklets and leaflets: Interior sheets at 80–120 gsm add roughly 0.08–0.13 mm (0.003–0.005 in) per sheet, paired with 200–300 gsm covers.
  • Punchboard stacks: Punchboard components follow greyboard core thicknesses (1.5–3 mm / 0.059–0.118 in) with 3–4 mm (0.118–0.157 in) die gaps on the uncut sheet; wells holding unpunched boards or punched tokens require the full 1.5–3 mm (0.059–0.118 in) vertical allowance to absorb edge burrs and curl.

Foam Cavity Interference

Foam inserts behave differently from rigid trays because cavity walls deform under load. Dense, rigid items (such as dice, miniatures, or wooden tokens) require slight negative cavity interference so friction holds them in place when the box is inverted. Paper components (cards, punchboard tiles, and booklets) must not be subjected to tight negative interference; their foam cavities should use neutral-to-light slip clearance or dedicated finger notches so compressed foam does not bow thin card edges or delaminate corner wraps.

Divider-to-Well Clearance

Dividers must fit within the card well's lateral tolerance without catching on side walls, draft angles, or corner radii. When dividers are cut from heavy Cover-weight cardstock (300–400 gsm) or rigid board, their width should match or sit slightly narrower than the finished card width while staying wide enough not to slip past card edges or twist diagonally inside a 1.5–2.5 mm (0.059–0.098 in) oversized well. If the insert uses slotted side walls to lock dividers in place, slot width must match divider caliper plus minimal insertion slip so dividers stay upright under shipping vibration. Divider tab height must remain below the 1.5–3 mm (0.059–0.118 in) vertical lid clearance plane.

Production Steps

  1. Lock component stack-up and physical calipers: Confirm exact card stock gsm, core type, double-sided film finish, corner radius (R3–R3.5 mm / 0.118–0.138 in), punchboard thickness, booklet page count, and whether wells must accommodate sleeves.
  2. Derive true box interior dimensions: Subtract greyboard wall thickness (1.5 / 2 / 2.5 / 3 mm or 0.059 / 0.079 / 0.098 / 0.118 in) and 15–20 mm (0.591–0.787 in) wrap turn-in overlap from the outer box footprint to establish the usable insert envelope.
  3. Assign CAD and dieline clearances: Apply 1.5–2.5 mm (0.059–0.098 in) lateral slip and 1.5–3 mm (0.059–0.118 in) vertical clearance for rigid wells and outer walls; set foam cavity interference by component rigidity; size divider tabs below the lid plane.
  4. Prepare printed insert and divider prepress files: For printed paperboard inserts and dividers, supply AI, PDF, or PSD files in PDF/X-1a or PDF/X-4 with CMYK plus separate spot layers, at least 300 DPI, 3 mm (0.118 in) bleed per side, at least 3 mm (0.118 in) safety (4–5 mm / 0.157–0.197 in for bordered backs), outlined or embedded fonts, 100% K fine text, rich black at C40–60 M30–40 Y30–40 K100, and TAC at or below 280%–300%.
  5. Validate on physical pre-production samples: Assemble full-weight decks, punchboards, booklets, and dividers into the white sample or first tooling sample inside the wrapped rigid box before approving mass production.

Sign-Off Criteria

  • Smooth box seating: The empty and loaded insert slides into the wrapped box without scraping the 15–20 mm (0.591–0.787 in) interior wrap turn-in or bowing the greyboard walls outward.
  • Flush lid closure: With all cards, booklets, punchboards, and dividers loaded, the box lid seats fully down to its intended stop with no upward spring or gap.
  • Bind-free card and divider movement: Decks drop into and lift out of wells smoothly with finger access, and dividers slide or seat into slots without corner pinching or vertical tab contact against the lid.
  • Retention without edge damage: Foam cavities hold rigid items securely during handling and inversion while leaving card corners and tile edges unbent.

Concrete Failure Modes

  • Lid lift or bowed box walls: Occurs when stack height calculations omit the +0.03–0.05 mm (+0.0012–0.0020 in) per-card thickness of double-sided film, when 15–20 mm (0.591–0.787 in) wrap turn-ins reduce the box's internal opening, or when oversized foam outer walls push outward against 1.5–2 mm (0.059–0.079 in) greyboard.
  • Corner pinching and deck binding: Occurs when molded or routed compartment corners have a tighter fillet radius than the deck's R3–R3.5 mm (0.118–0.138 in) card corners, or when lateral well clearance drops below 1.5 mm (0.059 in).
  • Crushed divider tabs or jammed slots: Occurs when divider tab height intrudes into the 1.5–3 mm (0.059–0.118 in) vertical lid clearance zone, or when divider stock caliper exceeds molded slot width.