When a boxed game ships with unpunched sheets above the insert and transitions to loose or bagged components after first opening, the compartment cannot be sized from flat sheet thickness alone. The required allowance shifts based on four physical conditions:
- Piece geometry: Irregular silhouettes, L-shaped tiles, and slotted standees bridge against well walls and each other at random angles, creating larger air voids than uniform round or square tokens.
- Bagging vs. loose fill: Polybags add film thickness, folded gussets, and trapped air, increasing the settled height beyond loose-dumped pieces unless bags are vented or flattened.
- Board caliper: Thicker greyboard cores (2.5 mm / 0.098 in or 3 mm / 0.118 in vs. 1.5 mm / 0.059 in or 2 mm / 0.079 in) amplify the height penalty when pieces tilt on edge rather than lying flat.
- Frame disposal: Discarding the outer punchboard skeleton frees perimeter volume; if the insert is designed to reclaim that space—part of dual-state punchboard storage—less extra well depth is needed.
Compartment & Material Specifications
| Parameter | Metric | Imperial | Role in Loose-Fill Allowance |
|---|---|---|---|
| Greyboard core thickness | 1.5 / 2 / 2.5 / 3 mm | 0.059 / 0.079 / 0.098 / 0.118 in | Sets baseline flat sheet stack height and edge-tilt height of settled tokens |
| Punchboard die gap | 3–4 mm | 0.118–0.157 in | Material removed or left as waste skeleton around pieces on the sheet |
| Compartment X/Y clearance | 1.5–2.5 mm | 0.059–0.098 in | Prevents tight wall binding that forces tiles to wedge above the well floor |
| Stack-height clearance | 1.5–3 mm | 0.059–0.118 in | Minimum vertical margin below the lid plane or upper tray lip |
Volume Allocation Relationships
In the pre-punch state, components occupy solid sheet volume:
Pre-punch stack height = (Sheet count * Board caliper) + Liner/wrap thickness
Once punched, the waste frame is removed, but random orientation and air gaps expand the effective bulk height of the pieces:
Post-punch settled height = Theoretical solid piece volume / Well footprint + Void & bridging height + Bag fold/air allowance
To keep the lid flush without crushing components:
Required well depth >= Post-punch settled height + 1.5–3 mm (0.059–0.118 in) stack clearance
If the box height is fixed, reclaim the volume of the discarded punchboard sheets by removing a temporary spacer or routing tokens into the cavity previously occupied by the unpunched boards.
Production & Sizing Steps
- Lock sheet caliper and piece count: Confirm the exact greyboard thickness (1.5 / 2 / 2.5 / 3 mm; 0.059 / 0.079 / 0.098 / 0.118 in) and total token, tile, and standee count before finalizing insert cavity depths.
- Separate flat-stacking tiles from loose-fill tokens: Give large uniform tiles dedicated flat wells sized with 1.5–2.5 mm (0.059–0.098 in) X/Y clearance so they stack predictably rather than tumbling.
- Assign loose-fill wells or discard-spacer reclaim: For small tokens and standees, either deepen the dedicated tray wells beyond the flat-sheet height or place a removable spacer under the insert that is discarded when the punchboard skeletons are thrown away.
- Account for polybag bulk: When pieces are sorted into multiple polybags, size the well width and depth to accept folded bag seams and residual air pockets without forcing the user to press the lid down to expel air.
- Verify the lid plane in both states: Check total vertical stack-up with unpunched sheets on top of the tray, and again with all tokens punched, settled, or bagged inside their assigned compartments.
Sign-Off Criteria
- Dual-state lid closure: The box lid closes flush with 1.5–3 mm (0.059–0.118 in) vertical clearance in both the unpunched shipping configuration and the post-punch loose or bagged configuration.
- No forced compression: Settled tokens and bagged standees sit below the compartment rim under gravity alone without manual flattening or lid pressure.
- Wall clearance compliance: Stacked tiles drop freely into their wells with 1.5–2.5 mm (0.059–0.098 in) lateral clearance so edges do not catch and bridge diagonally.
- Adjacent component protection: Loose-fill overflow does not spill over dividers into card wells, board channels, or booklet recesses.
Concrete Failure Modes
- Post-punch lid lift: Sizing a tray strictly to the flat punchboard thickness causes punched, randomly settled tokens to mound above the tray rim, bowing or lifting the box lid after first play.
- Bagged-air overflow: Pieces that fit loose in a well exceed the well height once divided into multiple polybags because folded seams and trapped air add unbudgeted vertical stack.
- Diagonal tile bridging: Narrow compartments without sufficient 1.5–2.5 mm (0.059–0.098 in) lateral clearance or rounded corners trap square and irregular tiles at steep angles, creating hollow voids underneath that push the top layer above the lid plane.
- Insufficient spacer reclaim: Relying on punchboard disposal to free space fails if the discarded waste skeleton was thin (e.g., 1.5 mm / 0.059 in) or shared across a shallow tray that still lacks the vertical depth for tumbled standees.
Parent guide Dual-State Unpunched and Punched Insert Storage