Alloy Specifications and Blank Properties
Tabletop metal coins are typically produced from die-cast zinc alloy, stamped brass, or stamped iron (mild steel). Typical coin diameters range from 20 mm to 40 mm (0.787 in to 1.575 in) with blank thicknesses from 2.0 mm to 3.5 mm (0.079 in to 0.138 in), depending on whether the design relies on deep sculptural contours or flat stacked rims.
| Property | Zinc Alloy (Cast) | Brass (Stamped) | Iron / Mild Steel (Stamped) |
|---|---|---|---|
| Typical composition | Zinc base with aluminum, magnesium, and copper | Copper-zinc alloy (rolled strip) | Low-carbon iron/steel (rolled strip) |
| Forming method | High-pressure die-casting | Blanking and high-tonnage coining | Blanking and high-tonnage coining |
| Relative density | ~6.6–6.7 g/cm3 (lighter hand-feel) | ~8.4–8.5 g/cm3 (heaviest hand-feel) | ~7.8–7.9 g/cm3 (medium-heavy hand-feel) |
| Flow and fill behavior | High molten fluidity; fills deep 3D cavities and undercuts | Solid-state plastic flow; suited to crisp flat rims and stepped 2D relief | Solid-state flow with higher work-hardening; best for clean flat faces and sharp edges |
| Corrosion behavior | Forms white oxide if unsealed; requires barrier plating | Naturally corrosion-resistant; tarnishes without lacquer | Rusts rapidly without oil protection or full barrier plating |
| Magnetic response | Non-magnetic | Non-magnetic | Ferromagnetic |
| Plating-base readiness | Porous cast skin; requires tumbling and copper strike | Smooth rolled surface; accepts direct activation and plating | Smooth rolled surface; requires descaling and nickel/copper barrier |
Because zinc alloy has lower density than brass or iron, a 1,000-coin batch of 30 mm (1.181 in) diameter, 2.5 mm (0.098 in) thick blanks weighs noticeably less in the hand and in shipping cartons—for example, shifting total component mass by several kilograms (several pounds) per master carton compared with solid brass of the same dimensions. When a heavier coin feel is required on a zinc blank, increasing blank thickness toward 3.0–3.5 mm (0.118–0.138 in) compensates for the lower alloy density.
Plating-Base Readiness and Surface Preparation
Raw blank metallurgy determines the pre-plating steps required to prevent blistering, peeling, or under-film corrosion:
- Zinc alloy: Die-casting produces a dense outer skin over a slightly porous interior, along with sprue gates and a perimeter parting line. Blanks must be sheared, media-tumbled to smooth flash, ultrasonically degreased, lightly acid-activated, and sealed with an alkaline or cyanide-free copper strike before decorative nickel, brass, or antique finishes are applied.
- Brass: Rolled brass blanks have a uniform, non-porous grain structure. After stamping and deburring, alkaline degreasing and light acid pickling prepare the surface for direct electroplating, chemical antiquing, or clear protective lacquering.
- Iron and mild steel: Stamped steel blanks oxidize quickly if exposed to ambient humidity between coining and plating. Blanks require protective oil during staging, followed by thorough descaling, pickling, and a continuous copper or nickel barrier layer before any decorative topcoat is applied.
Production Steps
- Match relief geometry to forming method: Route deep multi-level 3D sculpting, organic textures, and undercut-style contours to cast zinc molds with appropriate draft angles; route crisp raised rims, fine lettering, and flat stackable faces to stamped brass or iron coining dies.
- Form the blanks: Inject molten zinc alloy into steel dies for cast blanks, or punch blanks from rolled strip and strike them under coining presses for brass and iron.
- Shear and tumble: Trim casting gates and sprues on zinc blanks, then run all blanks through ceramic or stainless media tumbling to remove sharp stamped burrs and mold parting-line flash.
- Activate and apply base strike: Degrease, pickle, and apply the alloy-specific base layer—copper strike on zinc, barrier nickel or copper on iron, or direct surface activation on brass—immediately before decorative plating.
- Document material compliance: Where finished games fall under toy-safety scope, coordinate alloy and plating-layer assessment and testing against EN 71 (including heavy-metal migration limits) and keep supplier material declarations in the job record.
Sign-Off Criteria
- Alloy and batch weight: Confirm sample blanks match the specified alloy and fall within the target unit and bulk weight range in kg and lb (for example, verifying a 100-coin sample weight against the expected mass tolerance).
- Dimensions and stack flatness: Measure diameter and thickness in mm and in against approved drawings, and verify that coined rims sit flat enough for stable stacking.
- Edge and parting-line finish: Inspect the perimeter for residual sprue scars, raised mold seams, or sharp stamping burrs without over-tumbling crisp rim edges.
- Base-coat adhesion and surface integrity: Check strike-coated or pre-plated samples for micro-pits, pinholes, blisters, or early rust spots before authorizing full-batch finishing.
Failure Modes and Remedies
- Incomplete relief fill on stamped brass or iron: Deep sculpting or steep vertical walls exceed the metal's cold-coining ductility, leaving rounded or under-filled high points. Reduce relief depth, soften step transitions, or switch to cast zinc alloy.
- Plating blisters or peeling on zinc alloy: Trapped casting gas, open surface porosity, or an insufficient copper strike causes finishes to lift during plating or heat-drying. Adjust die venting and casting temperature, and enforce a full copper-strike barrier before decorative plating.
- Visible parting-line ridge or sprue mark: Worn mold halves or short tumbling cycles leave a sharp seam around the coin edge. Re-machine the mold parting faces and extend ceramic media tumbling time.
- Flash rust or edge pitting on iron blanks: Moisture exposure between stamping and plating—or pinholes in the barrier coat—triggers rust bleed-through. Keep iron blanks oil-protected until the plating line and specify a thicker copper or nickel undercoat.
- Light or hollow hand-feel: Selecting zinc alloy at a thin profile produces a noticeably lighter coin than brass. Increase blank thickness (for example, from 2.0 mm / 0.079 in to 3.0–3.5 mm / 0.118–0.138 in) or switch to stamped brass when maximum weight per unit is required.
Parent guide Non-Paper Tabletop Piece Materials