Standard round blanks distribute forming pressure evenly and stack cleanly in any orientation. Moving to polygonal or scalloped outlines, or adding a pierced center hole, changes how metal flows into the die or mold, how parts survive tumbling, and whether finished coins sit flat in a stack. Partner-sourced metal coins require dedicated tooling and follow project and component minimums; for broader silhouette options across materials, see non-paper piece shapes.
Profile and Rim Specifications
Custom Coin Outlines
- Round profiles: Offer uniform perimeter strength, predictable deburring, and consistent rim contact for stacking.
- Polygonal outlines: Require slight corner radii at every vertex. Sharp external points concentrate impact during barrel tumbling and are prone to chipping, plating wear, and snagging on inserts.
- Scalloped outlines: Need smooth, open lobe curves rather than deep, narrow notches. Deeply recessed scallops restrict metal flow toward the outer tips and create weak points along the perimeter.
Center-Hole Wall Minimums
- Rim-to-cutout bridge: The solid metal band between the outer perimeter and the inner pierced bore must remain wide and thick enough to resist bowing, radial cracking, or tearing during forming and ejection.
- Relief placement: Avoid cutting deep recessed fields, heavy texturing, or sharp engraved channels across the narrowest section between the outer rim and the center hole. Keep structural thickness consistent around the entire circumference of the bore, especially on polygonal or scalloped coins where the distance to the outer edge varies.
Stack-Nesting Rim Geometry
- Leveled outer lip: For stable table stacking, the outer rim on both faces must form a flat, continuous ring that sits flush with or slightly proud of all interior relief. If central artwork rises above the outer lip, stacked coins will pivot and topple.
- Nesting steps: Optional stepped or beveled inner rim ledges help stacked coins self-center laterally. Mating ledges require parallel bearing surfaces and consistent clearance so plating buildup does not cause coins to jam together.
Production Steps
- Outline and 3D relief prep: Define the outer silhouette, center-hole aperture, rim width, and relief depth in production artwork. Confirm that the outer lip clears the highest interior detail on both sides.
- Tooling and parting-line setup: Specialist tabletop manufacturing partners cut dedicated dies or molds to match the custom outline and center-hole pin, placing parting lines along the outer edge and inside the center bore rather than across the flat stacking lip.
- Forming (stamping or casting): Strike or cast the alloy so metal fills the outer lobes or corners and wraps cleanly around the center-hole pin without short-shots or uneven density.
- Piercing, deburring, and finishing: Clear any flash from the center hole and outer parting line, tumble/deburr sharp edges without rounding off the flat rim ring, and apply plating or surface washes evenly so finish thickness does not pool inside the center bore or unbalance the stacking lip.
Sign-Off Criteria
- Dimensional and weight checks: Measure diameter, total thickness, rim width, and center-hole opening in both mm and in, and verify unit and batch weights in both kg and lb against approved pre-production samples.
- Flat-surface stack test: Stack a full player set on a level surface; the stack must stand upright without rocking, leaning, or catching on raised central artwork.
- Perimeter and bore inspection: Confirm polygonal corners and scalloped lobes are fully formed and smooth, and verify the center-hole wall is free of burrs, residual flash, hairline cracks, or warping.
- Safety and compliance records: Where metal coins are supplied in games subject to toy or small-parts rules, complete and file applicable assessment and testing documentation (such as EN 71 toy safety records where relevant) as part of production sign-off.
Failure Modes
- Rocking or toppling stacks: Interior relief protrudes past the outer lip, or aggressive tumbling rounds the flat rim contact surface into a dome.
- Cracked or bowed rim-to-cutout bridge: The center hole sits too close to the outer edge or deep recessed artwork, causing the wall to fracture during piercing/ejection or warp during finishing.
- Chipped polygonal corners and snagged scallops: External vertices lack corner radii or scalloped notches are too tight, leading to edge damage during tumbling and transit.
- Unfilled outer tips or center-bore flash: Restricted metal flow around the center pin leaves incomplete outer lobes or leaves sharp, un-deburred flash inside the pierced hole.
Parent guide Non-Paper Component Shapes and Form Factors