For broader structural options across flat, die-cut, and bound sticker formats, see Sticker Sheet Formats.

Specifications and Structural Tolerances

Parameter Folded Panel Booklet Perforated Tear-Out / Saddle-Stitched Notes
Panel / page count 4, 6, or 8 panels Multiples of 4 (12–40 pages if saddle-stitched) Match fold style (accordion, gate, or roll-fold) to panel count
Box & rulebook fit clearance 1.5–2.5 mm (0.059–0.098 in) width/height 1.5–2.5 mm (0.059–0.098 in) width/height Maintain 1.5–3 mm (0.059–0.118 in) stack-height clearance
Bleed 3 mm (0.118 in) per side 3 mm (0.118 in) per side Extend background color past outer trim
Fold-gap & safety clearance >=3 mm (0.118 in) from trim, scores, and perfs >=3 mm (0.118 in) from trim, spine, and perfs Keeps kiss-cut decal edges clear of fold channels
Stock & weight notation Face stock + release liner; specify in gsm 80–120 gsm (0.08–0.13 mm / 0.003–0.005 in) interior; 200–300 gsm covers Express pack weights in kg and lb (1 kg = 2.205 lb)
Print & color CMYK + separate spot layers, >=300 DPI CMYK + separate spot layers, >=300 DPI TAC <=280%–300%; 100% K fine text; rich black C40–60 M30–40 Y30–40 K100
Surface finish Anti-scuff matte for dark artwork Anti-scuff matte for dark artwork Prevents rub marks across folded panels
Production minimums Component and tooling minimums apply Component and tooling minimums apply Custom kiss-cut, score, and perf dies follow project minimums

Paper Weight Notation (gsm vs. US Basis Weight)

Specify sticker face stock, release liner, and any cover wraps in grams per square meter (gsm). When referencing US pound weights, distinguish US Text LB—measured on a 25 × 38 in (635 × 965 mm) basis sheet—from US Cover LB—measured on a 20 × 26 in (508 × 660 mm) basis sheet—because identical pound numbers represent very different paper densities and thicknesses.

Job-Specific Production Steps

  1. Prepress and Spot-Layer Separation

    • Deliver print-ready AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
    • Place outer trim, kiss-cut decal contours, score lines, and perforation lines on separate named spot-color layers so tooling operators can assign distinct blade depths.
    • Confirm every kiss-cut decal sits at least 3 mm (0.118 in) away from outer trim edges, score lines, and perforation lines.
  2. Offset Printing and Surface Protection

    • Print artwork at >=300 DPI in CMYK with total area coverage capped at 280%–300% to prevent ink cracking along fold spines.
    • Apply an anti-scuff matte varnish or film over dark solids so folded panels do not scuff against adjacent decals or box interiors during transit.
  3. Kiss-Cutting, Scoring, and Perforating

    • Kiss-cut the face stock cleanly down to the adhesive layer without scoring or severing the release liner.
    • Register score channels and micro-perforation blades to the panel grid. Keep score channels free of kiss-cut shapes so the sheet folds along the intended crease rather than along a sticker edge.
  4. Folding, Binding, and Pack-Out

    • Fold 4-, 6-, or 8-panel sheets into their closed footprint, or collate 4-page signatures for 12–40 page saddle-stitched booklets.
    • Measure total closed stack thickness against the target card box or rulebook cavity before final pack-out.

Sign-Off Criteria

  • Fold-gap clearance: No kiss-cut contour intersects or touches a score channel, perforation line, or outer trim edge; minimum 3 mm (0.118 in) clearance holds across all panels.
  • Kiss-cut vs. liner integrity: Decals peel smoothly from the release liner without tearing the backing paper or lifting neighboring stickers.
  • Perforation and fold behavior: Perforated panels tear cleanly along the perf line without ripping into adjacent decal shapes; scored panels fold flat without cracking dark ink or delaminating matte film.
  • Box and rulebook fit: Closed booklet dimensions preserve 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) stack-height clearance inside the box.
  • Regulatory documentation (when applicable): For sticker booklets packed inside games or products subject to EU toy safety rules, age-grading and material testing under EN 71 are recorded in the product's compliance file (EU Toy Safety).

Concrete Failure Modes

  • Decal edges lifting or creasing at the fold: Caused by placing kiss-cut shapes too close to a score line, which forces the crease stress onto the sticker edge. Maintain >=3 mm (0.118 in) fold-gap clearance on both sides of every score.
  • Release liner tearing during peel or tear-out: Caused by kiss-cut tooling set too deep or by merging kiss-cut and perforation paths onto the same spot layer. Separate kiss-cut, score, and perf vectors onto distinct spot layers and calibrate cut depth to the liner caliper.
  • Ink cracking or scuffing along dark fold spines: Caused by heavy ink coverage (TAC >300%) or unprotected dark solids rubbing inside the box. Cap TAC at <=280%–300% and specify anti-scuff matte finishing on dark layouts.
  • Closed booklet bowing the box lid: Caused by underestimating the combined caliper of multi-panel release liners and face stock (or thick saddle-stitched signatures). Verify closed stack height in mm and inches and hold 1.5–3 mm (0.059–0.118 in) of vertical box clearance.