Board caliper, companion page count, and retail packaging drive the exact bill of materials. Larger panel counts or heavy table use favor 2.5 mm (0.098 in) greyboard to resist bowing, while compact travel kits or slipcase-housed sets often use 2.0 mm (0.079 in) board to keep folded stack thickness and shipping weight (typically 0.45 to 1.10 kg / 1.0 to 2.4 lb per assembled kit depending on panel dimensions and booklet extent) manageable.
Bill of Materials & Core Specifications
Panel trim dimensions are determined by table height, folded footprint, and slipcase sizing rather than a single fixed standard. Derive inch equivalents from your custom millimetre trim using inches = mm / 25.4.
| Component | Default Specification | Alternatives & Conditions |
|---|---|---|
| Screen Core | 2.0–2.5 mm (0.079–0.098 in) greyboard | 1.5 mm (0.059 in) for ultra-compact screens; 3.0 mm (0.118 in) for oversized tall panels requiring extra rigidity |
| Outer & Inner Wrap | Coated art paper with matte or anti-scuff matte lamination | Anti-scuff matte is recommended for dark artwork; wrap margin 15–20 mm (0.591–0.787 in) turned over board edges |
| Companion Booklet | Saddle-stitched, 12–40 pages (multiples of 4) | Perfect binding for 28+ pages; sewn binding recommended at 80–100+ pages |
| Booklet Interior Stock | 80–120 gsm (approx. 54–81 lb US Text, 25 × 38 in basis sheet) | Caliper approx. 0.08–0.13 mm (0.003–0.005 in) per sheet |
| Booklet Cover Stock | 200–300 gsm (approx. 74–111 lb US Cover, 20 × 26 in basis sheet) | Match lamination to screen finish when bundled in an open-front pack |
| Folded Reference Sheet | 4-, 6-, or 8-panel folded leaflet | Replaces or supplements a booklet when quick-reference tables must lie flat |
| Kit Packaging | Shrink wrap or rigid greyboard slipcase | Slipcase uses 1.5–2.5 mm (0.059–0.098 in) greyboard with 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3.0 mm (0.059–0.118 in) stack-height clearance |
Note on US Paper Weights: Always specify gsm alongside US pound weights and state the basis sheet size. Text LB (25 × 38 in / 635 × 965 mm) and Cover LB (20 × 26 in / 508 × 660 mm) are not interchangeable—for example, 120 gsm equals roughly 81 lb US Text, whereas 220 gsm equals roughly 81 lb US Cover.
Prepress & File Setup
Submit print-ready files in Adobe Illustrator (AI), PDF (PDF/X-1a or PDF/X-4), or Photoshop (PSD) with all fonts outlined or embedded.
- Resolution & Color: Minimum 300 DPI at 100% print size; CMYK color mode with separate named spot layers for any foil, spot UV, or die-line guides.
- Bleed & Safety: 3 mm (0.118 in) bleed per side on all wraps, booklets, and leaflets. Keep critical text, tables, and logos at least 3 mm (0.118 in) inside trim and hinge fold lines, increasing to 4–5 mm (0.157–0.197 in) on bordered panels.
- Black Ink & Coverage: Set fine body text and table rules to 100% K only. Use rich black (
C40–60 M30–40 Y30–40 K100) for large dark backgrounds, and keep Total Area Coverage (TAC) at or below 280%–300%. - Wrap & Hinge Layout: Supply a continuous spread or panel-by-panel wrap mechanical that accounts for the 15–20 mm (0.591–0.787 in) turn-in margins and the hinge gap allowance required for panels to fold flat over one another.
Production Workflow
Rigid GM screen kits follow a multi-stage offset and bindery sequence managed through specialist tabletop manufacturing partners:
- Prepress & Structural Dummy: Verify wrap dielines, hinge spacing, and slipcase clearances against a physical white dummy before committing to plates.
- Offset Printing & Lamination: Print screen wraps, companion booklets/leaflets, and any slipcase wraps. Apply matte or anti-scuff matte film lamination to protect high-touch edges and dark ink coverage.
- Board Cutting & Wrapping: Die-cut or guillotine 2.0–2.5 mm (0.079–0.098 in) greyboard panels, align hinge gaps, wrap outer and inner sheets with 15–20 mm (0.591–0.787 in) turn-ins, and press under weight to cure flat.
- Companion Finishing: Fold 4/6/8-panel reference leaflets, or fold 4-page signatures and saddle-stitch (12–40 pages) / perfect-bind (28+ pages) / sew (80–100+ pages) companion booklets.
- Collation & Pack-Out: Insert the folded screen and printed companion into shrink wrap or a custom rigid slipcase.
Sign-Off Criteria
- Color & Ink: Contract proof matches approved CMYK targets; fine table text prints cleanly in 100% K without registration halos; TAC stays at or below 280%–300%.
- Hinge & Fold Action: Panels fold completely flat in sequence without binding at the spine or lifting the wrap paper along the hinge channel.
- Slipcase Fit: Folded screen plus companion booklet/leaflet slides smoothly into the slipcase with 1.5–2.5 mm (0.059–0.098 in) clearance on width/height and 1.5–3.0 mm (0.059–0.118 in) clearance on total stack thickness:
Slipcase internal depth = (Panel count * Board caliper) + Wrap & hinge allowance + Companion thickness + 1.5 to 3.0 mm clearance
Common Failure Modes & Prevention
- Hinge Cracking or Delamination: Occurs when paper grain runs perpendicular to the fold or rigid film lamination resists tight 180-degree folding. Specify grain direction parallel to the hinges and validate flex endurance on a laminated structural sample.
- Panel Warping: Results from moisture imbalance between a laminated outer wrap and an unlaminated inner liner. Balance outer and inner wrap weights and allow wrapped boards to cure under flat pressure.
- Slipcase Jamming: Caused by calculating internal depth solely from raw greyboard thickness while ignoring turn-in overlaps, hinge cloth/paper buildup, and companion booklet caliper (0.08–0.13 mm / 0.003–0.005 in per interior sheet plus cover). Always measure the full collated stack before finalizing the slipcase die.
- Surface Scuffing on Dark Panels: Standard matte lamination marks easily during transit and repeated table setup. Switch to anti-scuff matte film whenever artwork relies on heavy rich black or dark saturated backgrounds.
- Clipped Tables Near Folds: Tight 3 mm (0.118 in) margins look crowded next to wrapped edges or hinge channels. Enforce 4–5 mm (0.157–0.197 in) safety margins around all bordered reference tables.
Regulatory & Packaging Compliance Records
When distributing kits internationally, maintain documentation matching the destination market's applicable procedures:
- EU Toy Safety (EN 71): If the kit is marketed or intended for use by children under 14 in the European Union, assess applicability and complete required physical, mechanical, and chemical testing under the EU Toy Safety framework (European Commission Toy Safety), retaining test reports and Declarations of Conformity as source records.
- Germany Packaging Act (VerpackG): For packaged kits placed on the German market, register with the Central Agency Packaging Register (ZSVR) in LUCID and maintain volume participation data reporting (Stiftung Zentrale Stelle Verpackungsregister).
- France Sorting Labeling (Triman / Info-Tri): For consumer-facing packaging sold in France, include compliant Triman and Info-Tri sorting instructions on the outer pack or slipcase per official guidelines (French Ministry of Ecological Transition Info-Tri).
Parent guide Custom GM Screen and Reference Kits