Conditions that change this default specification:
- Double-sided film lamination: Adding double-sided film increases card thickness by 0.03–0.05 mm (0.001–0.002 in) per card, adding 0.66–1.10 mm (0.026–0.043 in) across 22 cards and pushing a 400 gsm deck to the top of the 8–10 mm (0.315–0.394 in) range or slightly above.
- Gilded edges: Thick lamination can conflict with gilded edges and cause edge peeling or adhesion failure; use thinner coatings or uncoated finishes when edge gilding is specified.
- Frequent riffle shuffling: If the deck is built for heavy mechanical shuffling rather than single-card pulls, step down from 400 gsm art stock (0.40–0.44 mm / 0.016–0.017 in) to 330 gsm black core (0.32–0.34 mm / 0.013 in) or 310 gsm black-core linen (0.30–0.32 mm / 0.012–0.013 in) to reduce stiffness.
- Guidebook length: A 4-, 6-, or 8-panel folded leaflet keeps the shallow box profile intact; a 12–40 page saddle-stitched booklet adds measurable thickness and requires increasing the box depth allowance.
Bill of Materials and Default Specifications
Standard offset card runs start at 200 decks (usual tiers: 200, 300, 500, 1,000+), while boxed games and custom tooling follow project and component minimums. When specifying paper weights, always state gsm alongside US basis weights: US Text LB is measured on a 25 x 38 in (635 x 965 mm) basis sheet, whereas US Cover LB is measured on a 20 x 26 in (508 x 660 mm) basis sheet, so the same gsm produces a higher Text LB number than Cover LB number.
Card Stock and Caliper
| Component | Default Specification | Alternative Options | Physical Caliper / Dimension |
|---|---|---|---|
| Card stock (22 cards) | 400 gsm art stock | 350 gsm art stock; 330 gsm black core; 310 gsm black-core linen; 300 gsm art/blue core; PVC | 400 gsm: 0.40–0.44 mm (0.016–0.017 in); 350 gsm: 0.34–0.38 mm (0.013–0.015 in); 330 gsm: 0.32–0.34 mm (0.013 in); 310 gsm: 0.30–0.32 mm (0.012–0.013 in); 300 gsm: 0.28–0.31 mm (0.011–0.012 in); PVC: 0.30 mm (0.012 in) |
| Surface finish | Anti-scuff matte (for dark artwork) | Standard matte/gloss film or varnish | Double-sided film adds 0.03–0.05 mm (0.001–0.002 in) per card |
| Corner radius | Rounded corners | — | R3–R3.5 mm (0.118–0.138 in) |
Plain-text stack and mass formulas (using 1 in = 25.4 mm and 1 kg = 2.205 lb):
Card stack height (mm) = 22 * (base stock caliper in mm + film thickness in mm)
Card stack height (in) = Card stack height (mm) / 25.4
Deck card mass (kg) = 22 * card width (m) * card height (m) * (gsm / 1000)
Deck card mass (lb) = Deck card mass (kg) * 2.205
Press-Sheet Imposition Efficiency
A 22-card Major Arcana deck occupies roughly one-third to one-half of the press-sheet area required by a full 78-card deck at the same card trim. Because fewer press sheets are needed per deck, print setup and sheet waste drop proportionally across 200–1,000+ deck tiers. If the chosen card trim leaves open slots on the press-sheet grid, those spare positions can hold a title card, spread reference card, or spare blank without adding another press sheet.
Shallow Box Sizing (Tuck or Rigid Box)
| Packaging Element | Specification | Notes |
|---|---|---|
| Width & height clearance | 1.5–2.5 mm (0.059–0.098 in) over card trim | Applies to both tuck boxes and two-piece rigid boxes |
| Stack height clearance | 1.5–3 mm (0.059–0.118 in) over combined stack | Combined stack = 22 cards + booklet or leaflet |
| Rigid greyboard | 1.5 mm or 2 mm (0.059 in or 0.079 in) | Standard options are 1.5, 2, 2.5, and 3 mm (0.059, 0.079, 0.098, 0.118 in); thinner board keeps shallow boxes proportional |
| Rigid wrap margin | 15–20 mm (0.591–0.787 in) | Required turn-in allowance around greyboard edges |
Because an 8–10 mm (0.315–0.394 in) card stack is shallow, a folding tuck box is often simpler to form cleanly at low depth than a deep-walled two-piece rigid box. When a rigid box is chosen for presentation, 1.5 mm (0.059 in) or 2 mm (0.079 in) greyboard prevents the outer box walls from looking oversized relative to the 22-card stack.
Booklet and Leaflet Options
| Guide Format | Page / Panel Count | Paper Stock | Thickness Impact |
|---|---|---|---|
| Folded leaflet | 4, 6, or 8 panels | 80–120 gsm interior-grade sheet | ~0.08–0.13 mm (0.003–0.005 in) per sheet layer; minimal box depth impact |
| Saddle-stitched booklet | 12–40 pages (multiples of 4) | Interior: 80–120 gsm (US Text LB, 25 x 38 in / 635 x 965 mm basis); Cover: 200–300 gsm (US Cover LB, 20 x 26 in / 508 x 660 mm basis) | Adds ~0.5–3 mm (0.020–0.118 in) depending on page count; verify in box dummy |
Perfect binding (28+ pages) and sewn binding (80–100+ pages recommended) require thicker spines and deeper rigid boxes, so they are normally excluded from shallow 22-card Major Arcana sets unless the packaging is deepened specifically for a companion book.
Prepress and Production Steps
- Prepare print files: Supply artwork in AI, PDF, or PSD format, exported as PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
- Set color and ink limits: Build artwork in CMYK at ≥300 DPI, placing foil, spot UV, or gilding masks on separate spot layers. Use 100% K for fine text, rich black (
C40–60 M30–40 Y30–40 K100) for large dark solids, and keep total area coverage (TAC) at ≤280%–300%. - Apply bleed and safety margins: Add 3 mm (0.118 in) bleed per side on all cards, box wraps, and booklet pages. Keep critical text and borders at ≥3 mm (0.118 in) inside the trim line, increasing to ≥4–5 mm (0.157–0.197 in) for bordered card backs.
- Impose the 22-card grid: Lay out the 22 cards on the offset press sheet according to your chosen trim size, confirming whether extra grid slots will carry bonus/title cards or remain blank.
- Proof and build a physical dummy: Verify color on press/digital proofs and assemble an unprinted physical dummy using the actual 400 gsm stock, double-sided film (if used), and booklet/leaflet to confirm the 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) stack height clearance.
- Print, laminate, die-cut, and pack: Run offset sheets, apply anti-scuff matte or selected lamination, die-cut and round corners to R3–R3.5 mm (0.118–0.138 in), apply any edge gilding, assemble into the tuck or rigid box, and pack master cartons within shipping weight targets (for example, keeping carton gross weight around 15 kg / 33 lb or under carrier limits).
Sign-Off Criteria
Before releasing the job to mass production, verify these measurable checkpoints:
- Dummy stack fit: The 22 laminated cards plus the folded leaflet or saddle-stitched booklet slide into the box with 1.5–2.5 mm (0.059–0.098 in) lateral clearance and 1.5–3 mm (0.059–0.118 in) vertical clearance, without bowing the tuck flap or lifting the rigid lid.
- Ink and text check: Fine text prints cleanly in 100% K, rich black solids fall within
C40–60 M30–40 Y30–40 K100, and TAC does not exceed 280%–300%. - Border symmetry: Bordered card backs maintain ≥4–5 mm (0.157–0.197 in) safety margin from the trim edge on all four sides after die-cutting.
- Finish compatibility: Dark-ground artwork shows no scuffing under handling, and any edge gilding adheres cleanly without lifting the surface coating.
- Booklet signature count: Any saddle-stitched booklet uses an exact multiple of 4 pages (12–40 pages).
Concrete Failure Modes
- Box lid binding or tuck-flap pop-open: Calculating box depth from nominal 400 gsm caliper (0.40 mm / 0.016 in) without adding +0.03–0.05 mm (0.001–0.002 in) per card for double-sided film or the thickness of a saddle-stitched booklet eliminates the 1.5–3 mm (0.059–0.118 in) height clearance.
- Gilded edge peeling: Applying thick film lamination before edge gilding prevents the metallic foil from bonding evenly to the card edge, causing flaking during first use.
- Visible off-center borders: Setting bordered card-back safety margins below 4–5 mm (0.157–0.197 in) exposes normal die-cutting tolerance as uneven border widths.
- Scuffed dark artwork: Using standard gloss or unsealed matte coating on heavy dark-ink solids (TAC near 280%–300%) leads to rub marks during collating and box insertion; specify anti-scuff matte instead.
- Wasted press-sheet capacity or awkward booklet bulk: Leaving unallocated press-sheet positions unreviewed or pairing a 22-card shallow box with a 28+ page perfect-bound booklet forces unnecessary tooling or oversized packaging depth.
Regulatory and Packaging Compliance
Where a deck is marketed to children or falls under toy safety rules in the European Union, EN 71 assessment and testing procedures apply according to the European Commission Toy Safety framework. For retail packaging distributed in Germany or France, producer registration, packaging weight reporting (in kg / lb), and sorting-mark obligations follow VerpackG and Triman requirements.
Parent guide Custom Tarot and Oracle Deck Printing