Core Storage Box vs. Expansion Pack BOMs
An expandable fixed-set line splits its bill of materials between a durable core container built to house future releases and lean, fixed-sequence expansion packs engineered for identical card handling.
| Component / Parameter | Core Storage Box BOM | Fixed-Content Expansion Pack BOM |
|---|---|---|
| Primary Card Format & Die | Single line-locked card footprint with R3–R3.5 mm (0.118–0.138 in) corners | Identical footprint, cutting die profile, and corner radius R3–R3.5 mm (0.118–0.138 in) |
| Card Stock & Core | 300–350 gsm (~111–129 lb US Cover, 20 x 26 in basis) blue-core or black-core stock, or 0.30 mm (0.012 in) PVC | Exact stock weight, core color, and coating specification locked to the core BOM |
| Collation Method | Fixed-sequence deck bricks (one or more predetermined stacks) | Fixed-sequence pack collation (no randomization or variable rarity slots) |
| Outer Container | Rigid greyboard box (1.5 / 2 / 2.5 / 3 mm; 0.059 / 0.079 / 0.098 / 0.118 in) with 15–20 mm (0.591–0.787 in) wrap margin | Tuck box, sealed poly/foil flow-wrap, or folding carton sized to a single pack stack |
| Internal Organization | Card dividers, wells, or vacuum-formed/folded inserts sized for core + planned expansion stack height | None, or simple folded paperboard sleeve/band to hold fixed sequence |
| Rules & Extras | Bound rulebook (saddle stitch 12–40 pages; perfect bound 28+; sewn 80–100+ pages) and optional 3–4 mm (0.118–0.157 in) die-gap punchboards | 4-, 6-, or 8-panel folded leaflet (rule updates, card list, or scenario sheet) |
| Run Minimums | Boxed games and custom tooling follow project and component minimums | Standard offset card decks start at 200 decks (usual tiers: 200 / 300 / 500 / 1,000+) |
Card Stock, Finish, and Physical Specifications
Card Deck Press produces custom card and tabletop components through specialist offset and tabletop manufacturing partners, requiring every expansion to match the physical caliper and tactile finish of the core set. Because different game lines use different card footprints, lock the exact trim dimensions at the line level before tooling and reuse that same die across every expansion rather than assuming a default size.
Card Stock, Caliper, and Basis Weight
Distinguish US Cover LB (calculated on a 20 x 26 in basis sheet) from US Text LB (calculated on a 25 x 38 in basis sheet) when specifying card stocks versus rulebook interiors:
- 300 gsm art / blue core (~111 lb US Cover, 20 x 26 in basis): 0.28–0.31 mm (0.011–0.012 in) caliper.
- 310 gsm black-core linen (~115 lb US Cover, 20 x 26 in basis): 0.30–0.32 mm (0.012–0.013 in) caliper; suits frequent shuffling with reduced light show-through.
- 330 gsm black core (~122 lb US Cover, 20 x 26 in basis): 0.32–0.34 mm (0.013 in) caliper.
- 350 gsm art stock (~129 lb US Cover, 20 x 26 in basis): 0.34–0.38 mm (0.013–0.015 in) caliper.
- 400 gsm heavy stock (~148 lb US Cover, 20 x 26 in basis): 0.40–0.44 mm (0.016–0.017 in) caliper; suited to oversized reference cards or dividers rather than standard shuffle decks.
- PVC: 0.30 mm (0.012 in) caliper for waterproof or high-wear lines.
- Double-sided film lamination: Adds 0.03–0.05 mm (0.001–0.002 in) per card to total stack height.
Surface Finishes
- Dark card backs: Specify anti-scuff matte lamination or varnish on dark artwork to prevent edge whitening and surface marring during unsleeved play.
- Gilded edges: Avoid thick film lamination when specifying gilded edges, as heavy film thickness conflicts with edge-gilding adhesion and foil cleanly shearing at the card edge.
Rigid Core Boxes, Inserts, and Rulebooks
- Box clearance: Allow 1.5–2.5 mm (0.059–0.098 in) clearance across card width and height inside wells or tuck boxes, and 1.5–3 mm (0.059–0.118 in) clearance on stack height. When calculating core box stack capacity, sum the card caliper plus lamination (0.03–0.05 mm / 0.001–0.002 in per card) across both the core deck and all planned expansion packs, plus divider thickness.
- Punchboard tokens: If the core box includes die-cut counters, maintain a 3–4 mm (0.118–0.157 in) die gap between punchboard pieces.
- Rulebooks and leaflets: Core rulebooks use multiples of four pages with 80–120 gsm interior paper (~54–81 lb US Text, 25 x 38 in basis; about 0.08–0.13 mm / 0.003–0.005 in per sheet) and 200–300 gsm covers (~74–111 lb US Cover, 20 x 26 in basis). Expansion packs typically drop to 4-, 6-, or 8-panel folded leaflets.
- Carton packing: Group finished core boxes and expansion displays into master cartons balanced for safe handling (typically targeting 15–20 kg / 33.1–44.1 lb gross carton weight).
Prepress, Color Lock, and Production Steps
Prepress Requirements
- File formats: Supply print-ready AI, PDF, or PSD files exported to PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
- Color and ink limits: Build artwork in CMYK with separate spot layers for foil, spot UV, or die lines, at ≥300 DPI. Use 100% K for fine text, rich black (C40–60 M30–40 Y30–40 K100) for large dark solids, and keep total area coverage (TAC) at ≤280%–300%.
- Bleed and safety: Include 3 mm (0.118 in) bleed per side and ≥3 mm (0.118 in) safety margin from trim. For bordered card backs, increase the safety margin to ≥4–5 mm (0.157–0.197 in) so minor sheet shift does not expose asymmetric borders between core and expansion runs.
Job-Specific Production Steps
- Lock the master card-back standard: During the core set press run, archive physical wet proofs and press-calibrated color targets for the shared card back. Every subsequent expansion run must be matched against this physical master rather than a digital proof alone.
- Impose fixed-sequence press sheets: Lay out expansion cards on gang-run offset sheets in fixed positions tied to a single collation map, keeping card backs oriented uniformly with the core set's grain direction.
- Cut with matched tooling: Use the same die profile and R3–R3.5 mm (0.118–0.138 in) corner-rounding specification across core and expansion runs so mixed decks align flush.
- Collate and seal in sequence: Collate cards in exact manifest order, verify card count by weight and sequence check, and seal into tuck boxes or flow-wrap packs before cartoning.
Sign-Off Criteria and Failure Modes
Sign-Off Criteria
- Card-back color match: Expansion press sheets match the retained core master back under controlled viewing light without visible hue or density shift.
- Physical uniformity: Measured card caliper (including double-sided film allowance), corner radius, and grain stiffness match the core set BOM.
- Collation accuracy: First-off and periodic line checks confirm exact card count and fixed sequence with zero duplicates or omissions.
- Fit and clearance: Core box wells accommodate the target number of core and expansion cards (plus dividers) within the 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) stack-height tolerances.
Concrete Failure Modes
- Card-back hue drift: Printing an expansion from uncalibrated CMYK values without the core master sheet creates noticeable shade differences on the back, marking expansion cards in a shuffled deck.
- Caliper or corner-radius mismatch: Switching from 310 gsm black-core linen to 330 gsm black core or changing corner radius between runs creates tactile tells when cutting or shuffling mixed decks.
- Bordered-back trim shift: Using less than 4–5 mm (0.157–0.197 in) safety on bordered backs causes uneven border widths on one edge of an expansion sheet, revealing card origin in hand.
- Undersized core box wells: Omitting the 0.03–0.05 mm (0.001–0.002 in) per-card film thickness or future expansion stack height causes the rigid lid to bow or crushes divider tabs.
- Scuffed dark backs: Running dark solid card backs with standard matte varnish instead of anti-scuff matte leads to visible abrasion rings after minimal play.
Regulatory and Packaging Compliance Records
When distributing core boxes and expansion packs into regulated markets, maintain product-level technical files and packaging registrations based on destination rules and age grading:
- EU Toy Safety (EN 71): Where a game's target age grading or physical components bring it under toy safety scope, conduct applicable EN 71 mechanical, flammability, and chemical assessment and testing and retain the technical documentation referenced by the European Commission Toy Safety framework.
- Germany Packaging Act (VerpackG): Before placing packaged core boxes or retail expansion packs on the German market, complete producer registration and data reporting through Stiftung Zentrale Stelle Verpackungsregister (LUCID).
- France Sorting Signage (Triman): Apply applicable sorting instructions and Triman markings to consumer packaging sold in France in accordance with French Ministry of Ecological Transition Info-Tri guidance.