Default Bill of Materials (BOM) & Specifications
Standard offset card runs start at 200 decks (usual tiers: 200, 300, 500, and 1,000+ decks), while custom hang-tab tuck box tooling follows project and component minimums. Because US paper weights differ by basis sheet size—Cover LB is measured on a 20 × 26 in sheet, whereas Text/Book LB is measured on a 25 × 38 in sheet—specify all card, box, and insert stocks in gsm alongside caliper in mm and inches.
| Component | Default Specification | Caliper / Allowance |
|---|---|---|
| Game Cards | 300 gsm art/blue core; 310 gsm black-core linen; 330 gsm black core; 350 gsm art stock; 400 gsm board; or 0.30 mm (0.0118 in) PVC | 300 gsm: 0.28–0.31 mm (0.0110–0.0122 in) 310 gsm: 0.30–0.32 mm (0.0118–0.0126 in) 330 gsm: 0.32–0.34 mm (0.0126–0.0134 in) 350 gsm: 0.34–0.38 mm (0.0134–0.0150 in) 400 gsm: 0.40–0.44 mm (0.0157–0.0173 in) Double-sided film adds 0.03–0.05 mm (0.0012–0.0020 in) per card |
| Card Corners | Rounded die-cut corners | R3–R3.5 mm (0.118–0.138 in) |
| Hang-Tab Tuck Box | 350–400 gsm tuck board with extended euro-slot top header and double-ply glued option | 350 gsm: 0.34–0.38 mm (0.0134–0.0150 in) 400 gsm: 0.40–0.44 mm (0.0157–0.0173 in) |
| Box Internal Clearance | Derived from the chosen card trim and total stack thickness | Width/height: +1.5–2.5 mm (+0.059–0.098 in) Stack height: +1.5–3 mm (+0.059–0.118 in) |
| Folded Leaflet (Optional) | 4-, 6-, or 8-panel insert on 80–120 gsm interior Text stock | 0.08–0.13 mm (0.0031–0.0051 in) per sheet |
| Tamper-Evident Seals | Clear or printed security seals across box opening seams | Placed clear of the euro-slot neck, barcode, and compliance marks |
Sizing the Box Without a Fixed Trim
Derive the tuck box dieline directly from the project's chosen card trim rather than assuming a universal card size:
- Box inner width and height (mm) = Card trim dimension (mm) + 1.5 to 2.5 mm (0.059 to 0.098 in)
- Box inner depth (mm) = (Card count × Single-card caliper in mm) + Folded leaflet thickness (mm) + 1.5 to 3 mm (0.059 to 0.118 in)
Laminated Hang-Tab Header Reinforcement & Deck-Weight Limits
The euro-slot neck is the highest-stress point on a retail hang-tab box. Standard pegboard hooks concentrate the entire deck weight onto a narrow bridge of paperboard above the slot.
Header Construction & Lamination
- Single-ply extended header (350–400 gsm): Viable only for low-card-count, lightweight decks where total hanging mass stays low and transit cartons support the headers upright.
- Double-folded glued header (recommended default): Extending the rear panel upward and folding it back down behind the euro-slot—glued face-to-face before die-cutting—doubles the board thickness at the hook bearing surface and resists tearing from repeated customer handling.
- Film lamination: Exterior or double-sided film lamination adds tensile strength across the euro-slot neck and prevents fiber splitting along score lines. Use anti-scuff matte lamination when box artwork has dark solids. Note that thick lamination on cards themselves can conflict with gilded edges; keep heavy protective film on the outer tuck box if cards use edge gilding.
Calculating & Capping Deck Weight
Total hanging mass determines whether a tuck-box hang tab will hold up in retail aisles. Calculate total hanging weight in kilograms (kg) and pounds (lb) before locking the box dieline:
Card stack mass (g) = (Card width in mm * Card height in mm / 1,000,000) * Card gsm * Card count
Total hanging mass (kg) = (Card stack mass in g + Tuck box mass in g + Leaflet mass in g) / 1,000
Total hanging mass (lb) = Total hanging mass (kg) * 2.2046
If high card counts, 400 gsm card stock, or multi-panel booklets push the deck into heavier mass tiers—or make the box depth wide enough that the center of gravity pulls forward off the peg hook—replace the tuck-box hang tab with a reinforced glued header insert or transition to a rigid two-piece retail box with a separate hanging sleeve.
Tamper-Seal Placement
Retail hang-tab decks require tamper-evident sealing that secures the cards without damaging box graphics or interfering with pegboard hanging:
- Bottom tuck flap (primary seal): Place a single tamper seal centered across the bottom tuck flap seam onto the back panel. This keeps the top euro-slot header free of adhesive stress and avoids peeling when hooks slide in and out.
- Top flap (secondary seal, if required): If the top flap opens independently of the glued hang-tab header, place a small seal on the front-to-top tuck seam, well below the euro-slot cutout.
- Keep clear zones unobstructed: Never bridge a tamper seal over the euro-slot, UPC/EAN barcode quiet zone, or mandatory recycling/safety markings.
Job-Specific Production & Prepress Steps
- Prepress & File Setup: Supply print-ready files in AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 with all fonts outlined or embedded. Build artwork in CMYK at ≥300 DPI with separate spot layers for any foil, spot UV, or die/crease lines.
- Bleed & Safety Margins: Extend all full-bleed card and box artwork 3 mm (0.118 in) past the trim/cut line on every side. Keep text and critical graphics at least 3 mm (0.118 in) inside trim lines, and ≥4–5 mm (0.157–0.197 in) inside trim for bordered card backs. Keep all box copy clear of the euro-slot punch zone and fold creases.
- Ink & Black Builds: Set fine body text to 100% K only. For deep solid black backgrounds, use rich black (C40–60 M30–40 Y30–40 K100) and keep Total Area Coverage (TAC) at ≤280%–300% to prevent set-off and cracking on box folds.
- Print, Laminate & Die-Cut: Print sheets, apply exterior film (anti-scuff matte for dark designs), and die-cut both the box perimeter/creases and the euro-slot in a single registered pass so the slot sits square to the top edge.
- Fold, Glue & Pack: Glue the double-ply header and side seam, collate the R3–R3.5 mm (0.118–0.138 in) corner-rounded cards and any 4/6/8-panel leaflet, insert into the tuck box, and apply tamper seals. Pack finished decks in master cartons with dividers or flat-stacked orientation so extended headers are not bent or crushed in transit.
Retail Compliance & Labeling (Conditional)
Where retail distribution includes regulated jurisdictions, build required markings into the back or bottom box panel during prepress and maintain supporting compliance records:
- EU Toy Safety (EN 71): If the card game is marketed as a toy or intended for children, arrange third-party assessment and testing against applicable EN 71 parts and retain technical documentation per the European Commission Toy Safety framework.
- Germany (VerpackG / LUCID): Retail packaging placed on the German market requires producer registration and packaging-volume data reporting through the LUCID Packaging Register.
- France (Triman / Info-tri): Consumer-facing retail packaging sold in France requires sorting instructions and the Triman symbol formatted according to Info-tri guidelines.
Sign-Off Criteria
Before approving the press proof and physical white/printed dummy for mass production, verify:
- Header & Slot Integrity: Double-ply header glue bond is uniform with no edge lift; euro-slot punch is clean with no jagged board fibers or delaminated film.
- Fit & Clearance: Card stack plus any 80–120 gsm leaflet slides cleanly into the tuck box within the 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) stack-height clearances without bulging the front panel.
- Prepress & Color: PDF/X-1a or PDF/X-4 passes preflight with TAC ≤280%–300%, 100% K fine text, 3 mm (0.118 in) bleed, and ≥4–5 mm (0.157–0.197 in) safety on bordered card backs.
- Tamper-Seal & Label Check: Seals adhere cleanly to the laminated surface without lifting ink, and barcodes/compliance marks remain completely unobstructed.
Concrete Failure Modes
- Euro-Slot Tearing in Aisles: Using unreinforced single-ply board or unlaminated stock for heavy decks causes the hook slot to split vertically under pegboard load or transit vibration.
- Header Creasing & Box Bowing: Packing hang-tab boxes loosely in master cartons bends the extended header, while under-sizing stack depth (<1.5 mm / 0.059 in clearance) bows the tuck box and pops the bottom flap open.
- Score-Line Cracking: Folding 350–400 gsm board with heavy ink coverage (TAC >300%) or without exterior lamination cracks the printed surface along the hang-tab fold and side seams.
- Tamper-Seal Lift or Surface Tear: Applying high-tack seals over uncoated stock tears box fibers on opening, whereas low-tack seals can peel off anti-scuff matte film during cold-chain or humid transit.
- Bordered Card-Back Clipping: Leaving less than 4–5 mm (0.157–0.197 in) safety on bordered backs exposes uneven border widths after R3–R3.5 mm (0.118–0.138 in) die-cutting.
Parent guide Standard Card Game Deck Printing