Complete Bill of Materials and Stabilization Specifications
Card Deck Press produces custom shaped-contour puzzles through specialist offset and tabletop manufacturing partners. Boxed games and custom tooling—including the outer silhouette knife, irregular internal cut grid, and fitted insert die—follow project and component minimums rather than standard deck tiers.
| Component | Material & Caliper / Weight | Key Dimensional & Print Specs | Role in Finished Product |
|---|---|---|---|
| Puzzle Backing Board | Greyboard: 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in) |
Thicker 2.5–3 mm (0.098–0.118 in) board reinforces narrow perimeter peninsulas |
Prevents edge-piece warping and tab breakage during stripping |
| Puzzle Face Sheet | Offset-printed art paper, mounted to greyboard | CMYK + separate spot layers, ≥300 DPI, TAC ≤280%–300%, rich black C40–60 M30–40 Y30–40 K100, 100% K fine text |
Carries artwork; anti-scuff matte lamination suits dark artwork |
| Outer Box (Rigid) | Greyboard 1.5–3 mm (0.059–0.118 in) with printed wrap |
Wrap margin 15–20 mm (0.591–0.787 in); interior sized to insert + reference sheet |
Protects irregular pieces inside a retail-friendly rectangular footprint |
| Fitted Box Filler Insert | Die-cut paperboard or corrugated E-flute | 1.5–2.5 mm (0.059–0.098 in) X/Y clearance; 1.5–3 mm (0.059–0.118 in) stack-height clearance |
Immobilizes bagged pieces away from empty box corners |
| Irregular Reference Sheet | 80–120 gsm (0.08–0.13 mm / 0.003–0.005 in per sheet; 55–80 lb US Text LB on a 25 x 38 in basis sheet) or 200–300 gsm (75–110 lb US Cover LB on a 20 x 26 in basis sheet) |
Flat card or 4/6/8-panel folded leaflet; 3 mm (0.118 in) bleed per side |
Shows the exact silhouette border and edge-piece orientation |
| Inner Piece Bag | Heat-sealed or resealable poly/paper bag | Sized to compressed loose-piece volume inside the insert cavity | Keeps irregular edge pieces contained and dust-free |
Note on paper weights: always specify paper in gsm alongside the US grade, because US Text LB (25 x 38 in basis sheet) and US Cover LB (20 x 26 in basis sheet) use different basis sheet sizes and do not convert at the same ratio.
Perimeter Die and Bleed Registration (Summary)
On a shaped-contour puzzle, the outer silhouette knife cuts through the mounted board along a custom vector path rather than a straight guillotine edge. Extend artwork 3 mm (0.118 in) beyond the outer silhouette vector on all sides, and keep critical edge details at least ≥3 mm (0.118 in) inside the contour (≥4–5 mm / 0.157–0.197 in if the reverse side carries a bordered pattern). For full internal grid geometry, bridge placement, and die-knife tolerances, see shaped-contour puzzle cut patterns.
Irregular Reference Sheet and Box Stabilization
Because a rectangular box lid cannot show a 1:1 rectangular crop without misrepresenting the outer border, the reference sheet must display the complete silhouette outline inside its frame.
- Flat vs. folded reference: Use
200–300 gsmcover stock (20 x 26 inbasis) for a flat reference card when the box interior is large enough to hold it flat with1.5–2.5 mm(0.059–0.098 in) lateral clearance. Use80–120 gsmtext stock (25 x 38 inbasis) for4,6, or8-panel folded leaflets when the box footprint is smaller than the readable reference scale. - Insert geometry: Size the filler insert cavity to match the settled volume of the bagged pieces, leaving
1.5–2.5 mm(0.059–0.098 in) across width and height and1.5–3 mm(0.059–0.118 in) for stack height. In master cartons packed up to15–20 kg(33.1–44.1 lb), an unstabilized bag shifts toward box corners and crushes protruding perimeter tabs.
Production Steps
- Prepress and Dieline Separation: Prepare print files in
AI,PDF, orPSDexported asPDF/X-1aorPDF/X-4with outlined or embedded fonts. Place the outer silhouette trim knife, internal puzzle cut grid, and box/insert dielines on separate non-printing spot layers. - Sheet Printing, Lamination, and Mounting: Print the puzzle face sheet, reference sheet, and box wrap in CMYK (
≥300 DPI,TAC ≤280%–300%). Apply anti-scuff matte lamination to dark puzzle faces before mounting onto1.5–3 mm(0.059–0.118 in) greyboard, then allow adhesive moisture to stabilize before cutting. - Contour Die-Cutting and Waste Stripping: Die-cut the mounted board. Strip the outer perimeter waste matrix carefully so narrow edge-piece knobs and concavities do not tear or delaminate from the greyboard backing.
- Bagging, Insert Seating, and Box Assembly: Seal the stripped pieces in the inner bag, seat the bag inside the fitted filler insert within the wrapped rigid box (
15–20 mm/0.591–0.787 inwrap margin), and lay the irregular reference sheet on top before closing the lid.
Sign-Off Criteria and Regulatory Records
Pre-Production and Press Sign-Off
Verify these physical tolerances on the wet proof and cut white/printed dummy before full run release:
- Perimeter registration: Zero unprinted paper slivers along concave or convex outer silhouette edges (
3 mm/0.118 inbleed intact). - Edge-piece integrity: No backing-board splitting or face-sheet lift on narrow perimeter tabs.
- Box and insert fit: Bagged pieces sit flush inside the filler cavity without forcing the lid up, maintaining
1.5–2.5 mm(0.059–0.098 in) X/Y clearance and1.5–3 mm(0.059–0.118 in) Z clearance. - Reference accuracy: The reference sheet displays the exact outer silhouette contour and matches the orientation of the finished cut puzzle.
Conditional Regulatory and Packaging Records
Depending on target markets and age grading, maintain the applicable compliance records alongside the bill of materials:
- EN 71 (EU Toy Safety): When a shaped-contour puzzle is marketed as a toy or intended for children in the EU, EN 71 assessment and testing apply, documented through age-grading justification, small-parts evaluation, and accredited lab test reports. See the European Commission Toy Safety overview.
- VerpackG (Germany): Placing packaged puzzles on the German market triggers packaging registration and material-weight data reporting covering the rigid box, inner bag, and paperboard filler insert. See the ZSVR Verpackungsregister.
- Triman (France): Distribution into France requires Triman sorting instructions on the outer packaging, specifying disposal streams for the box, insert, and inner bag. See the French Ministry Info-Tri guidance.
Concrete Failure Modes
- White slivers on concave borders: Caused by omitting
3 mm(0.118 in) perimeter bleed along tight inward curves or placing high-contrast borders inside the3 mm(0.118 in) safety zone. Fix by expanding the bleed path uniformly outward from the silhouette vector. - Broken or bent perimeter tabs in transit: Caused by packing loose bagged pieces directly into a standard rectangular box without a filler insert, or using
1.5 mm(0.059 in) greyboard on long, narrow outer projections. Fix by stepping up to2.5–3 mm(0.098–0.118 in) greyboard and adding a fitted insert that pins the bag away from box walls. - Scuffed dark edge pieces: Caused by greyboard dust abrading uncoated or standard-varnish dark ink during stripping and bagging. Fix by applying anti-scuff matte lamination and capping ink coverage at
TAC ≤280%–300%. - Misleading reference sheet: Caused by printing a rectangular detail crop instead of the true silhouette outline, leaving assemblers unable to identify edge pieces. Fix by placing the exact outer trim vector on the
80–120 gsm(55–80 lbUS Text LB) or200–300 gsm(75–110 lbUS Cover LB) reference sheet.