This configuration sits within the folding board games family and pairs a folding game board, one or more die-cut punchboards, and loose components (cards, booklets, and partner-sourced game pieces) inside a custom-molded PET blister tray and rigid outer box. Choose a formed PET tray when the finished bill of materials (BOM) has multiple token shapes or mixed component sizes that need separated wells after punch-out and a flat upper ledge to support heavy board layers during transit. Because thermoformed PET requires custom mold tooling, boxed games using formed trays follow project and component minimums rather than the 200-deck starting tier used for standard offset card-only runs (200/300/500/1,000+ decks). If a game contains minimal loose pieces or low unit volume that cannot justify mold tooling, a folded paperboard insert or partitioned box is the simpler alternative.

Finished BOM Specifications and Stack Geometry

Every component in a formed-tray set shares the same rigid box cavity, so material calipers, film thickness, and tray wall geometry must be locked together before tooling starts.

BOM Component Standard Material & Caliper Key Dimensional & Print Constraints
Outer Rigid Box Greyboard: 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in) Wrap margin 15–20 mm (0.591–0.787 in); inner clearance 1.5–2.5 mm (0.059–0.098 in) on width/height and 1.5–3 mm (0.059–0.118 in) on stack height
Folding Board & Punchboards Greyboard: 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in) Punchboard die gap 3–4 mm (0.118–0.157 in) between tokens to maintain sheet rigidity before punch-out
Thermoformed PET Tray Custom-molded PET insert Upper perimeter/stepped ledges support intact punchboards and folding board; lower wells house sorted tokens, cards, and partner-sourced dice/pawns
Card Decks 300 gsm art/blue core: 0.28–0.31 mm (0.011–0.012 in); 310 gsm black-core linen: 0.30–0.32 mm (0.012–0.013 in); 330 gsm black core: 0.32–0.34 mm (0.013 in); 350 gsm art stock: 0.34–0.38 mm (0.013–0.015 in); 400 gsm: 0.40–0.44 mm (0.016–0.017 in); PVC: 0.30 mm (0.012 in) Double-sided film adds 0.03–0.05 mm (0.001–0.002 in) per card; R3–R3.5 mm (0.118–0.138 in) corners; size tray card wells to the job's finished card trim and deck height
Booklets & Leaflets Interior stock: 80–120 gsm, about 0.08–0.13 mm (0.003–0.005 in) per sheet; covers: 200–300 gsm Leaflets use 4/6/8 panels; bound signatures use multiples of 4 (saddle stitch 12–40 pages, perfect binding 28+ pages, sewn binding 80–100+ pages recommended)

When specifying paper weights for booklets or box wraps in imperial units alongside gsm, distinguish US Text LB (based on a 25 x 38 in / 635 x 965 mm basis sheet) from US Cover LB (based on a 20 x 26 in / 508 x 660 mm basis sheet), as identical LB numbers represent different gsm densities across the two basis sizes.

Prepress and Print Specifications

  • File formats and color: Supply AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 in CMYK with separate spot layers, at >=300 DPI, with all fonts outlined or embedded.
  • Bleed and safety: Include 3 mm (0.118 in) bleed per side, >=3 mm (0.118 in) safety margin, and >=4–5 mm (0.157–0.197 in) safety for bordered card backs.
  • Black ink and coverage: Use 100% K for fine text, rich black C40–60 M30–40 Y30–40 K100 for solid dark areas, and keep total area coverage (TAC) at <=280%–300%.
  • Surface finish: Apply anti-scuff matte lamination on dark artwork for rigid box wraps, folding boards, and card surfaces to prevent rub marks during tray insertion and shipping.

Stack-Height and Box-Clearance Calculations

Size the rigid box and PET tray together using plain-text stack math rather than estimating from unmounted sheet counts:

Total Stack Height (mm) = Folding Board Thickness + Intact Punchboard Stack + Booklet Thickness + Formed Tray Overall Height
Box Inner Depth (mm) = Total Stack Height + 1.5 to 3.0 mm (0.059 to 0.118 in)
Box Inner Width or Length (mm) = Tray Outer Width or Length + 1.5 to 2.5 mm (0.059 to 0.098 in)

Account for total packed component mass in kg (lb) when setting greyboard thickness and tray support ribs: heavier stacks of 2.5–3 mm (0.098–0.118 in) boards and dense partner-sourced dice or wooden pieces place greater downward load on the PET tray rim during palletized transit.

Job-Specific Production Steps

  1. Lock the complete BOM and component mass: Confirm the exact greyboard thickness for the box, folding board, and punchboards, card stock plus double-sided film caliper, booklet page count, and dimensions of all partner-sourced game pieces, along with total packed unit mass in kg (lb).
  2. Engineer the dual-state PET tray CAD: Design upper stepped ledges to hold the intact punchboards and folding board flat during shipping, and sculpt lower cavities with finger-pull notches for post-punch tokens, finished decks (sized to the exact card trim without assuming a default format), and dice.
  3. Verify the tooling sample with physical dummies: Produce a thermoformed PET sample from the blister mold and test-pack unprinted dummy boards, punchboards, laminated cards, and partner-sourced pieces inside a white-sample rigid box.
  4. Finalize prepress and plates: Preflight all box wrap, folding board, punchboard, card, and booklet PDF/X-1a or PDF/X-4 files for 3 mm (0.118 in) bleed, safety margins, 100% K fine text, TAC <=280%–300%, and separate spot layers.
  5. Run production and collate: Print and laminate sheets, mount greyboard with 15–20 mm (0.591–0.787 in) wrap margins, die-cut punchboards with 3–4 mm (0.118–0.157 in) die gaps, thermoform the PET trays, and assemble the finished BOM.

Sign-Off Criteria

  • Pre-punch shipping fit: Intact punchboards and the folding board rest flat on the PET tray's upper support ledges without bowing into empty lower wells, and the box lid seats flush within the 1.5–3 mm (0.059–0.118 in) stack-height clearance.
  • Post-punch storage fit: Punched tokens, partner-sourced pieces, and full card decks (including 0.03–0.05 mm / 0.001–0.002 in per card for double-sided film) sit completely below the tray's board-support ledge so the folding board does not pinch components.
  • Die-cut and wrap integrity: Punchboard tokens remain intact in the matrix across the 3–4 mm (0.118–0.157 in) die gaps until pushed out, and rigid box wraps turn cleanly over the greyboard edges within the 15–20 mm (0.591–0.787 in) wrap margin.
  • Print proof verification: Press or digital proofs confirm >=300 DPI detail, >=4–5 mm (0.157–0.197 in) safety on bordered card backs, clean 100% K fine text, and anti-scuff matte finish on dark surfaces.

Regulatory and Packaging Compliance Records

Because formed-tray sets combine paperboard, greyboard, inks/coatings, thermoformed PET plastic, and partner-sourced game pieces, market-specific compliance depends on product classification and destination:

  • Toy Safety (EN 71): Where a board game is intended for children or falls under EU toy-safety scope, EN 71 assessment and testing apply to the physical components, chemical/ink compliance, and small-part hazards of punched tokens and partner-sourced pieces. Maintain technical documentation and test records in accordance with the European Commission Toy Safety framework.
  • Packaging EPR Registration and Sorting Marks: Pairing a greyboard/paper rigid box with a thermoformed PET plastic tray introduces multi-material packaging streams. For distribution into Germany, verify producer registration and packaging-weight data reporting under VerpackG (LUCID Packaging Register). For distribution into France, verify applicable sorting-instruction markings for paperboard and plastic tray elements under Triman / Info-tri.

Concrete Failure Modes

  • Punchboard sag and premature pop-out: Leaving wide unsupported spans above deep token wells allows intact punchboards to flex under carton weight (kg / lb) during transit, popping tokens loose before unboxing.
  • Card well binding after film lamination: Calculating card well depth from raw paper caliper without adding 0.03–0.05 mm (0.001–0.002 in) per card for double-sided film causes the deck to sit proud of the tray well and lift the folding board.
  • Box lid lift or internal rattle: Neglecting the 1.5–3 mm (0.059–0.118 in) stack-height clearance or 1.5–2.5 mm (0.059–0.098 in) width/height clearance results in either a lid that cannot close fully or an insert that shifts and scuffs the inner box wrap.
  • Punchboard matrix tearing: Narrowing the die gap below 3–4 mm (0.118–0.157 in) weakens the waste bridge between tokens, causing adjacent pieces to tear or delaminate during die-cutting or handling.
  • Scuffing on dark inner surfaces: Omitting anti-scuff matte lamination on rich-black (C40–60 M30–40 Y30–40 K100) or high-TAC artwork leaves visible abrasion tracks where the PET tray flange or folding board rubs against the box interior.