The structural choice hinges on two physical states: factory pack-out (flat, unpunched hex sheets stacked above or beside the insert) and post-opening storage (loose punched hexes, sleeved or unsleeved cards, and wooden tokens). Because a rigid box must close flush at retail before tiles are punched—and still organize loose tiles afterward—the insert cavity depth and footprint must be calculated for both volumes simultaneously. Standard offset card runs start at 200 decks (usual tiers of 200, 300, 500, and 1,000+), while boxed games, custom punchboard dies, and multi-cavity inserts follow project and component minimums through specialist offset and tabletop manufacturing partners.

Bill of Materials and Component Specifications

Component Material / Stock Options Caliper / Thickness (mm / in) Key Structural & Clearance Rules
Rigid Box & Lid Greyboard 1.5 / 0.059, 2.0 / 0.079, 2.5 / 0.098, 3.0 / 0.118 15–20 mm (0.591–0.787 in) wrap margin; 1.5–2.5 mm (0.059–0.098 in) width/height clearance
Hex Punchboards Wrapped greyboard 1.5 / 0.059 to 3.0 / 0.118 3–4 mm (0.118–0.157 in) die gap between hexes and sheet border
Card Decks Art, blue-core, black-core, PVC 0.28–0.44 / 0.0110–0.0173 (+film) R3–R3.5 mm (0.118–0.138 in) corners; 1.5–3 mm (0.059–0.118 in) stack clearance
Wooden Tokens Partner-sourced hardwood Project-defined Seated in dedicated insert wells without fabric draw pouches
Rulebook / Leaflet 80–120 gsm interior; 200–300 gsm cover 0.08–0.13 / 0.0031–0.0051 per interior sheet 4/6/8-panel leaflet or multiples of 4 pages (12–40 saddle stitch; 28+ perfect; 80–100+ sewn)

Card Stock, Caliper, and Deck Well Sizing

Card trim dimensions are defined by the game's table footprint and insert layout rather than a single default format. When specifying paper weight, distinguish US Text LB from Cover LB by basis sheet size rather than treating pound ratings as interchangeable; use gsm alongside caliper for exact stack-height math.

  • 300 gsm art / blue core: 0.28–0.31 mm (0.0110–0.0122 in)
  • 310 gsm black-core linen: 0.30–0.32 mm (0.0118–0.0126 in)
  • 330 gsm black core: 0.32–0.34 mm (0.0126–0.0134 in)
  • 350 gsm art stock: 0.34–0.38 mm (0.0134–0.0150 in)
  • 400 gsm stock: 0.40–0.44 mm (0.0157–0.0173 in)
  • PVC: 0.30 mm (0.0118 in)
  • Double-sided film lamination: adds 0.03–0.05 mm (0.0012–0.0020 in) per card

Anti-scuff matte film is suited to dark artwork on card backs and box wraps. If the deck specifies gilded edges, avoid thick lamination because thick film can conflict with edge gilding.

Use the following plain-text formulas to size the card well inside the insert:

  • Deck stack height (mm) = Card count * (Base card caliper + Film thickness)
  • Deck stack height (in) = Deck stack height (mm) / 25.4
  • Minimum card well depth (mm) = Deck stack height (mm) + 1.5 to 3.0 mm (0.059 to 0.118 in)

Hex Punchboards, Wooden Tokens, and Box Depth

Hex tiles require a 3–4 mm (0.118–0.157 in) die gap between adjacent hexes and from the outer sheet edge so the cutting rules do not crush neighbouring tiles or strip the printed wrap. Because unpunched sheets retain this 3–4 mm (0.118–0.157 in) waste skeleton around every tile, the full sheet footprint is larger than the loose tiles alone.

To fit both states without draw pouches:

  1. Size the inner box length and width to the unpunched sheet footprint plus 1.5–2.5 mm (0.059–0.098 in) clearance.
  2. Partition the lower insert into a card well, loose hex-tile wells, and wooden-token wells, leaving the upper cavity clear for the stacked unpunched punchboard sheets and rulebook at initial pack-out.
  3. Calculate total internal box height using: Total internal box height (mm) = Max(Lower insert height, Loose tile + token stack height) + Unpunched sheet stack height + Rulebook thickness + 1.5 to 3.0 mm (0.059 to 0.118 in)

Set Weight and Carton Planning

Heavy greyboard punchboards, dense card stacks, and hardwood tokens increase shipping mass quickly. Track unit and master-carton weight in both kg and lb during structural sign-off so greyboard thickness (1.5–3.0 mm / 0.059–0.118 in) and insert walls can support the load without bowing:

  • Total set weight (kg) = Sum of component weights (kg)
  • Total set weight (lb) = Total set weight (kg) * 2.205

Prepress and Print File Specifications

Prepare all print-ready artwork for cards, punchboard wraps, rigid box wraps, and rulebooks to the following standards:

  • File formats: AI, PDF, or PSD, exported as PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
  • Colour space and ink limits: CMYK with separate spot layers for die-lines and specialty finishes; 100% K for fine text; rich black at C40–60 M30–40 Y30–40 K100; total area coverage (TAC) at or below 280%–300%.
  • Resolution: Minimum 300 DPI at final print size.
  • Bleed and safety margins: 3 mm (0.118 in) bleed per side; minimum 3 mm (0.118 in) safety margin from trim or die-cut lines, increasing to 4–5 mm (0.157–0.197 in) on bordered card backs.
  • Box and punchboard wraps: Allow 15–20 mm (0.591–0.787 in) wrap margin on all four sides of rigid box greyboard wraps.

Job-Specific Production Steps and Sign-Off Criteria

  1. Structural White-Sample Sign-Off: Assemble an unprinted dummy using the exact greyboard thickness (1.5–3.0 mm / 0.059–0.118 in), insert geometry, card stack, and wooden tokens. Verify 1.5–2.5 mm (0.059–0.098 in) lateral clearance and 1.5–3.0 mm (0.059–0.118 in) vertical clearance with the unpunched sheets stacked on top, then punch the sample sheets and verify that all loose hexes fit the lower wells without lid lift.
  2. Prepress and Die-Line Overlay Review: Superimpose the hex die-line onto the punchboard artwork to confirm the 3–4 mm (0.118–0.157 in) die gap, 3 mm (0.118 in) bleed, and ≥3 mm (0.118 in) safety margin on every tile face and back. Confirm spot layers are separated from CMYK and TAC stays within 280%–300%.
  3. Offset Printing, Lamination, and Die-Cutting: Print card sheets, box wraps, punchboard wraps, and booklets. Apply anti-scuff matte film where dark artwork is used, die-cut cards with R3–R3.5 mm (0.118–0.138 in) corners, and die-cut hex punchboards with calibrated nicking so tiles stay in the sheet during transit but punch cleanly by hand.
  4. Wooden Token Inspection and Pack-Out: Inspect partner-sourced wooden pieces for dimensional consistency against the insert wells, then pack lower insert cavities (cards and tokens), stack unpunched hex sheets and the rulebook on top, and verify flush lid closure.

Regulatory and Market Compliance Records

Depending on target distribution markets and age grading, maintain applicable assessment and packaging records rather than assuming coverage:

Concrete Failure Modes

  • Lid lift or crushed box corners: Caused by omitting the 1.5–3.0 mm (0.059–0.118 in) vertical clearance above stacked unpunched sheets and rulebooks, or by selecting 1.5 mm (0.059 in) greyboard on a heavy multi-sheet set where 2.5–3.0 mm (0.098–0.118 in) is needed for the total kg/lb load.
  • Hex tile edge tearing or bleed contamination: Caused by setting punchboard die gaps below 3–4 mm (0.118–0.157 in), which prevents clean die-rule seating and pulls wrap paper across adjacent tile faces.
  • Card well binding or bowed decks: Caused by calculating well depth from base paper caliper alone without adding 0.03–0.05 mm (0.0012–0.0020 in) per card for double-sided film lamination, or by exceeding 2.5 mm (0.098 in) lateral clearance so cards shift and dog-ear.
  • Token migration in transit: Caused by oversized wooden-token wells without a flat unpunched punchboard sheet or rulebook resting directly over the insert top to hold pieces in their cavities.
  • Scuffing or gilded-edge flaking: Caused by specifying standard varnish instead of anti-scuff matte on dark card backs and box wraps, or pairing thick lamination with gilded card edges.