Choose this configuration over the folding-carton or single-pad formats covered in the roll-and-write games guide when the finished bill of materials (BOM) includes multiple distinct pad designs, solid partner-sourced dice and pencils that exceed flat-pack depth, or heavy paper stacks that would crush a standard tuck box. Standard offset cards start at 200 decks (usual tiers 200/300/500/1,000+), whereas boxed games with rigid greyboard tooling, partitioned inserts, and custom dice engraving molds follow project and component minimums.
Finished-Product BOM and Specifications
| Component | Material & Basis Weight | Dimensions, Caliper & Clearance | Production Notes |
|---|---|---|---|
| Two-Piece Rigid Box | 1.5, 2, 2.5, or 3 mm (0.059, 0.079, 0.098, or 0.118 in) greyboard wrapped in coated art paper | 15–20 mm (0.591–0.787 in) wrap margin; 1.5–2.5 mm (0.059–0.098 in) width/height clearance; 1.5–3 mm (0.059–0.118 in) stack height clearance | Use 2–2.5 mm (0.079–0.098 in) greyboard when multi-pad sets reach 0.5–1.5 kg (1.1–3.3 lb) to prevent lid bowing; anti-scuff matte lamination suits dark artwork |
| Partitioned Insert | Die-cut paperboard or laminated greyboard dividers | Cavity walls matched to tallest loose item; 1.5–2.5 mm (0.059–0.098 in) per-cavity width/length clearance | Separates engraved dice and wooden pencils from scorepad faces and reference cards |
| Glued Scorepad Blocks | 80–120 gsm uncoated interior sheets (~54–80 lb US Text, 25 × 38 in / 635 × 965 mm basis sheet); 200–300 gsm backer (~74–111 lb US Cover, 20 × 26 in / 508 × 660 mm basis sheet) | 0.08–0.13 mm (0.003–0.005 in) per interior sheet | Top-edge padding glue over a rigid backer; uncoated stock gives pencil graphite reliable bite |
| Reference Cards | 300 gsm art/blue core, 310 gsm black-core linen, 330 gsm black core, or 350 gsm art stock | 300 gsm: 0.28–0.31 mm (0.011–0.012 in); 310 gsm: 0.30–0.32 mm (0.012–0.013 in); 330 gsm: 0.32–0.34 mm (0.013 in); 350 gsm: 0.34–0.38 mm (0.013–0.015 in); double-sided film adds 0.03–0.05 mm (0.001–0.002 in) per card; R3–R3.5 mm (0.118–0.138 in) corners | Size card trim to share a partition well with a pad block or sit in its own recessed card well |
| Rulebook / Leaflet | 80–120 gsm interior (~54–80 lb US Text); 200–300 gsm cover (~74–111 lb US Cover) | 0.08–0.13 mm (0.003–0.005 in) per interior sheet | Leaflets use 4/6/8 panels; bound booklets use multiples of 4 pages (saddle stitch 12–40 pages, perfect binding 28+, sewn binding 80–100+ recommended) |
| Custom Engraved Dice & Pencils | Partner-sourced resin/acrylic/wood dice; wooden pencils | Sized to dedicated tray recesses | Pencil channel length and dice diameter establish the minimum interior box footprint and depth |
Basis Weight and Stack-Height Sizing
Distinguish US Text LB (25 × 38 in / 635 × 965 mm basis sheet) from US Cover LB (20 × 26 in / 508 × 660 mm basis sheet) when specifying scorepads and booklets. Ordering a 100 lb Text sheet for a pad backer or rulebook cover yields flexible paper rather than rigid cover stock.
Size the rigid box interior from the worst-case cumulative caliper of all stacked paper plus the tallest rigid component:
Pad Stack Height = (Sheet Count * Max Sheet Caliper) + Backer Caliper + Glue Film
Interior Box Height = Max(Total Pad Stack Height, Dice + Tray Height) + 1.5 to 3 mm (0.059 to 0.118 in)
Cavity Width or Length = Component Width or Length + 1.5 to 2.5 mm (0.059 to 0.098 in)
If multiple pad designs have different sheet counts or footprints, either trim all pads to a shared outer footprint with stepped partition floors or assign each pad design its own walled cavity.
Prepress and Job-Specific Production Steps
Prepress File Requirements
- Format and color: Supply AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 at ≥300 DPI in CMYK, with separate spot layers for box die-lines, partition scores, and dice engraving artwork.
- Text and ink limits: Outline or embed all fonts. Set fine scorepad grids, numbers, and body text in 100% K. Use rich black C40–60 M30–40 Y30–40 K100 for solid dark box wraps, keeping total area coverage (TAC) at ≤280%–300%.
- Bleed, safety, and wrap: Apply 3 mm (0.118 in) bleed per side and ≥3 mm (0.118 in) safety margin (≥4–5 mm / 0.157–0.197 in for bordered card backs). Extend rigid box wrap artwork across the full 15–20 mm (0.591–0.787 in) turn-in margin.
Production Sequence
- Lock BOM dimensions: Confirm pad sheet counts, paper calipers, dice dimensions, and pencil length before cutting rigid box and partition dies.
- Print paper components: Run offset sheets for box wraps, reference cards, rulebooks, and each scorepad design; collate and pad-glue each scorepad block onto its 200–300 gsm backer.
- Produce partner-sourced pieces: Manufacture custom engraved dice and wooden pencils in parallel with print finishing.
- Convert box and insert: Wrap 1.5–3 mm (0.059–0.118 in) greyboard shells with laminated wraps and die-cut the partitioned insert.
- Assemble and pack: Seat each pad block, card stack, pencil, and die into its assigned cavity, confirm lid closure without compression, and pack into master cartons.
Sign-Off Criteria
- Cavity and lid fit: Every component drops into its partition within 1.5–2.5 mm (0.059–0.098 in) lateral clearance, and the lid closes flush with 1.5–3 mm (0.059–0.118 in) vertical clearance.
- Pad tear-off: Top-edge padding glue holds the block together during handling while allowing single sheets to tear cleanly without ripping the grid or lifting the backer.
- Line legibility: Fine scorepad tables and reference card text print in 100% K with crisp edges and no multi-plate registration haloing.
- Wrap adhesion: Laminated box wraps fold cleanly around the 15–20 mm (0.591–0.787 in) turn-ins with no corner cracking, particularly on dark anti-scuff matte finishes.
Concrete Failure Modes
- Dice or pencils bruising scorepads: Unpartitioned wells or low divider walls let hard dice and pencil points dent top scorepad sheets during transit; match divider height to the tallest loose piece.
- Lid hang-up or bowing: Ignoring per-sheet caliper tolerance (0.08–0.13 mm / 0.003–0.005 in per sheet across multiple pads) consumes the 1.5–3 mm (0.059–0.118 in) stack clearance, while 1.5 mm (0.059 in) greyboard bows under sets weighing 1 kg (2.2 lb) or more; calculate maximum caliper stack-up and step up to 2–2.5 mm (0.079–0.098 in) greyboard.
- Smeared or skipped pencil marks: Specifying coated art paper or varnish on scorepad interiors prevents graphite transfer; keep scorepad interiors uncoated at 80–120 gsm.
- Plugged scorepad grids: Building thin grid rules in four-color rich black or exceeding 280%–300% TAC causes ink spread and muddy lines; restrict fine linework to 100% K.
Regulatory and Packaging Compliance Records
When distributing rigid-box sets with small components such as dice or pencil end-caps, verify applicable safety assessment, testing, and packaging reporting records for each destination market:
- Toy safety assessment and testing (EU): Where age grading or play patterns bring the set under toy safety rules, maintain technical documentation and EN 71 assessment and testing records per the European Commission Toy Safety framework.
- Packaging registration and reporting (Germany): Register packaging weights and material streams (greyboard box, paperboard insert, inner wraps) under VerpackG via Zentrale Stelle Verpackungsregister (VerpackG).
- Sorting signage (France): Place required Triman sorting instructions on the rigid box and applicable packaging layers per French Ministry of Ecological Transition Info-Tri (Triman).