Conditions that change this choice:
- Standard non-foil runs: If metallic shine-through is not required, use standard custom trading card specifications on 300 gsm art/blue-core or 310 gsm black-core linen stock to avoid PET film and white-ink pass overhead.
- Dark artwork vs. high-gloss finishes: Choose anti-scuff matte over gloss varnish when artwork relies on dark solids or rich black, as gloss shows handling marks rapidly.
- Gilded edges: Avoid thick film lamination when specifying gilded card edges, because thick lamination can conflict with edge gilding adhesion at the cut line.
- Higher rigidity or waterproof needs: Step up to 350–400 gsm art stock for stiffer display cards without a black core, or 0.30 mm (0.0118 in) PVC when moisture resistance is required.
- Order volume: Standard offset card runs start at 200 decks (usual tiers: 200, 300, 500, and 1,000+), while custom foil tooling, holographic patterns, and boxed sets follow project and component minimums.
Finished Card Bill of Materials and Foil-Substrate Stack
Card stock weight is specified in gsm rather than US Cover LB or Text LB, because Cover LB and Text LB are calculated on different basis sheet sizes and cannot be compared directly by pound number alone.
| Layer | Material / Specification | Caliper Contribution | Role in Stack |
|---|---|---|---|
| Core substrate | 330 gsm black-core paperboard | 0.32–0.34 mm (0.0126–0.0134 in) | Opaque center layer; prevents light show-through and provides snap |
| Foil / holographic layer | Metallic or rainbow PET film | +0.03–0.05 mm (0.0012–0.0020 in) for double-sided film | Creates reflective metallic or diffractive holographic base |
| Underbase | Selective opaque white ink (spot layer) | Negligible | Blocks PET reflection under solid graphics; knocked out where foil shows |
| Color & detail inks | CMYK process + optional spot layers | Negligible | Renders artwork; fine text set to 100% K |
| Topcoat | Anti-scratch matte or UV coating | Included in film/finish tolerance | Protects ink from abrasion and balances front/back sheet tension |
When double-sided film is applied to 330 gsm black-core stock, total finished card caliper increases to approximately 0.35–0.39 mm (0.0138–0.0154 in).
Prepress, White-Ink Masking, and Anti-Curl Specifications
File Setup and Color Limits
- Accepted formats: AI, PDF, or PSD exported to PDF/X-1a or PDF/X-4.
- Resolution and fonts: Minimum 300 DPI for all raster elements; all fonts outlined or embedded.
- Ink limits: Total Area Coverage (TAC) ≤280%–300%. Use 100% K for fine text and rich black (C40–60 M30–40 Y30–40 K100) for deep dark fills.
- Bleed, safety, and corners: Supply artwork at the project's assigned trim dimensions with 3 mm (0.118 in) bleed per side, ≥3 mm (0.118 in) safety margin (≥4–5 mm / 0.157–0.197 in for bordered backs), and R3–R3.5 mm (0.118–0.138 in) rounded corners.
White-Ink Masking Requirement
- Build the opaque white underbase as a dedicated, named spot-color layer separate from CMYK channels.
- Set 100% spot white behind every graphic, text block, or frame that must appear opaque and non-metallic.
- Leave 0% white (knockout) wherever the metallic or rainbow PET film should reflect through CMYK tints or remain bare foil.
- Keep mask edges sharp and vector-clean; feathered or rasterized masks create cloudy transitions at foil boundaries.
Anti-Curl Coating Balance
PET film laminated to one face introduces asymmetric surface tension against the paperboard core as sheets cure. Balance the front PET layer with either a matching back-side film or a calibrated anti-scratch matte or UV coating across both faces so sheets remain flat through die-cutting and collation.
Production Steps and Sign-Off Criteria
- Prepress separation check: Verify PDF/X-1a or PDF/X-4 compliance, ≥300 DPI resolution, TAC ≤280%–300%, bleed/safety margins, and clean spot-channel separation for the white-ink mask.
- PET film lamination: Bond metallic or rainbow PET film to 330 gsm black-core press sheets.
- White-ink underbase and CMYK pass: Print the selective opaque white-ink layer first, followed by CMYK process and any additional spot layers.
- Anti-scratch coating and conditioning: Apply anti-scratch matte or UV coating to protect ink and equalize sheet tension before cutting.
- Die-cutting and collation: Die-cut cards with R3–R3.5 mm (0.118–0.138 in) corners and collate into scratch-safe inner wraps or boxes.
Sign-Off Criteria
- Mask registration: White-ink underbase aligns cleanly beneath CMYK artwork with no visible white halo along foil-to-opaque edges.
- Sheet flatness: Finished cards sit flat on a level surface without edge lift or bowing after coating cure.
- Caliper accuracy: Measured card thickness matches the 330 gsm + film stack range (0.35–0.39 mm / 0.0138–0.0154 in for double-sided film) so deck height fits the box specification.
- Surface durability: Dark artwork and rich-black solids show no visible scuffing after collation handling.
Scratch-Safe Packaging, Box Clearance, and Regulatory Records
Scratch-Safe Handling and Box Sizing
Foil and dark-ink surfaces abrade easily if cards shift loosely in transit. Pair anti-scratch matte or UV topcoats with snug inner packs (boosters or wraps) and size outer boxes using finished-card caliper rather than bare board caliper:
- Width and height clearance: 1.5–2.5 mm (0.059–0.098 in) over card trim dimensions.
- Stack height clearance: 1.5–3 mm (0.059–0.118 in) over the total deck stack height, calculated from the filmed card caliper (including the +0.03–0.05 mm / 0.0012–0.0020 in per-card film allowance).
- Rigid box construction (when used): 1.5, 2, 2.5, or 3 mm (0.059, 0.079, 0.098, or 0.118 in) greyboard with a 15–20 mm (0.591–0.787 in) wrap margin.
Conditional Regulatory Steps
Depending on target age grading and distribution region, maintain the corresponding compliance and packaging records before shipment:
- Children's products (EU): EU Toy Safety (EN 71) assessment and testing documentation where cards are marketed for children.
- Packaging registration (Germany): VerpackG registration and data reporting for packaged goods placed on the German market.
- Sorting labeling (France): Triman sorting information on retail packaging distributed in France.
Failure Modes
- Sheet curl after cutting: Applying PET film to only the card face without a compensating back-side film or balanced UV/matte coating causes cards to bow.
- White-ink haloing or dull foil: Misregistered or soft-edged white-ink spot masks bleed into metallic zones, leaving pale fringes around opaque graphics or muting rainbow refraction.
- Scuffing on dark backgrounds: Omitting anti-scratch matte or UV protection on rich-black fills (C40–60 M30–40 Y30–40 K100) leads to visible rub marks during collation and shipping.
- Tight or crushed deck boxes: Calculating box depth from bare 330 gsm caliper (0.32–0.34 mm / 0.0126–0.0134 in) instead of filmed caliper (+0.03–0.05 mm / 0.0012–0.0020 in per card) consumes the 1.5–3 mm (0.059–0.118 in) stack clearance and binds the deck.
- Edge peeling on gilded decks: Combining thick lamination with gilded edges prevents clean edge adhesion and causes delamination along the trim.
Parent guide Custom Trading Card Printing