Switch away from anti-scratch matte lamination under two conditions:

  • Gilded edges: Thick lamination can conflict with metallic edge gilding adhesion and edge smoothness.
  • Tight box stack-height clearance: Because double-sided film adds 0.03–0.05 mm (0.0012–0.0020 in) per card, high-card-count decks require recalculating tuck or two-piece box depth to maintain 1.5–3 mm (0.059–0.118 in) of stack-height clearance.

For the broader finish overview, see anti-scratch matte lamination. For a full side-by-side breakdown against standard film, see anti-scratch matte lamination vs. standard matte lamination.


Card Performance and Caliper Specifications

Specify card stocks in gsm rather than US Text LB or Cover LB, because US Text LB and Cover LB are measured against different basis sheet sizes and do not convert directly at equal weights.

Specification Anti-Scratch Matte Lamination Effect Production Target / Range
Added caliper (double-sided) Increases single-card thickness +0.03–0.05 mm (+0.0012–0.0020 in) per card
Scuff resistance Resists white shuffle scratches on dark ink Suited for dark artwork and rich-black fields
Stiffness Adds slight edge and snap rigidity Slightly crisper than standard matte film
Shuffle glide Reduces surface drag between faces Smoother slide than standard matte film
Edge finish compatibility Thick film interferes with edge foil Avoid combining with gilded edges

Combined Card Caliper by Base Stock

Total laminated card caliper follows: Total laminated caliper = Base stock caliper + 0.03 to 0.05 mm (0.0012 to 0.0020 in)

Base Card Stock Unlaminated Caliper Laminated Caliper (Double-Sided Film)
300 gsm art / blue core 0.28–0.31 mm (0.0110–0.0122 in) 0.31–0.36 mm (0.0122–0.0142 in)
310 gsm black-core linen 0.30–0.32 mm (0.0118–0.0126 in) 0.33–0.37 mm (0.0130–0.0146 in)
330 gsm black core 0.32–0.34 mm (0.0126–0.0134 in) 0.35–0.39 mm (0.0138–0.0154 in)
350 gsm art stock 0.34–0.38 mm (0.0134–0.0150 in) 0.37–0.43 mm (0.0146–0.0169 in)
400 gsm art stock 0.40–0.44 mm (0.0157–0.0173 in) 0.43–0.49 mm (0.0169–0.0193 in)
PVC (0.30 mm) 0.30 mm (0.0118 in) 0.33–0.35 mm (0.0130–0.0138 in)

Stack Thickness and Box Clearance

Calculate total laminated stack height before finalizing box dielines: Added stack height = Card count * 0.03 to 0.05 mm (0.0012 to 0.0020 in) Total stack height = (Card count * Base stock caliper) + Added stack height

Box cavities require 1.5–2.5 mm (0.059–0.098 in) clearance across width and height, and 1.5–3 mm (0.059–0.118 in) clearance for stack height.


Prepress and Production Steps

Card Deck Press coordinates offset card printing and finishing through specialist manufacturing partners. Each job follows four film-specific production stages:

  1. Prepress and ink-limit preparation: Supply files in AI, PDF, or PSD (PDF/X-1a or PDF/X-4) with outlined or embedded fonts, CMYK plus separate spot layers, and ≥300 DPI raster artwork. Include 3 mm (0.118 in) bleed per side, ≥3 mm (0.118 in) safety margin (≥4–5 mm / 0.157–0.197 in for bordered backs), 100% K for fine text, rich black at C40–60 M30–40 Y30–40 K100, and Total Area Coverage (TAC) ≤280%–300%.
  2. Double-sided thermal/adhesive lamination: Apply anti-scratch matte film evenly across both press-sheet faces after ink curing so dark solids do not lift or delaminate during cutting.
  3. Sheet slitting and corner rounding: Die-cut cards to the job's assigned trim format and round corners to R3–R3.5 mm (0.118–0.138 in) with sharp tooling to prevent film lipping along the perimeter.
  4. Deck collation and box-fit verification: Collate decks to the target card count and verify stack height against box clearance before final packing.

Sign-Off Criteria

  • Visual surface check: Dark and rich-black fields show uniform matte diffusion without white scuff streaks after repeated card-to-card rubbing.
  • Edge and corner integrity: Die-cut edges and R3–R3.5 mm (0.118–0.138 in) corners show clean film adhesion with no lifting, bubbling, or frayed film overhang.
  • Shuffle and snap check: Cards glide smoothly in riffle and overhand shuffles and return flat without excessive curl.
  • Stack-height fit: Completed deck stack fits inside the box with 1.5–3 mm (0.059–0.118 in) height clearance and 1.5–2.5 mm (0.059–0.098 in) width/height clearance.

Concrete Failure Modes

  • Box bind from uncounted film thickness: Sizing a tuck or two-piece box from unlaminated stock caliper omits 0.03–0.05 mm (0.0012–0.0020 in) per card, consuming the 1.5–3 mm (0.059–0.118 in) stack-height allowance and causing tight insertion or lid bowing.
  • Gilded-edge conflict: Applying metallic edge gilding over thick double-sided lamination leads to poor foil transfer, uneven edge sheen, or peeling along the card edge.
  • Edge delamination on high-TAC dark borders: Exceeding 280%–300% TAC or laminating before ink dries weakens film bond at the cut line, causing the film to lift along dark bleeds during die-cutting and R3–R3.5 mm (0.118–0.138 in) corner rounding.
  • Asymmetric curl from single-sided application: Laminating only one face creates uneven surface tension across the sheet, warping the card body during storage and play.