Technical Specifications & Material Compatibility
Liquid soft-touch coating cures directly onto the printed sheet as an inline or offline flood varnish rather than bonding a separate plastic layer.
| Parameter | Liquid Soft-Touch Coating (UV / Aqueous) | Double-Sided Soft-Touch BOPP Film (Comparison) |
|---|---|---|
| Added Caliper per Card | 0 mm (0 in) film thickness | 0.03–0.05 mm (0.0012–0.0020 in) |
| Edge Behavior | Zero film-edge peeling or delamination | Film edge can lift under heavy corner wear |
| Tear & Moisture Resistance | Relies entirely on underlying paperboard | Higher tear strength and moisture barrier |
| Surface Burnishing | Burnishes faster to semi-gloss under friction | Higher abrasion resistance before burnishing |
| Gilded Edge Compatibility | Compatible; no plastic film edge to interfere | Thick lamination can conflict with gilded edges |
| Offset Card Minimums | 200 decks (usual tiers: 200/300/500/1,000+) | 200 decks (usual tiers: 200/300/500/1,000+) |
Stock Weights, Caliper, and Box Clearance
When specifying substrates for velvet varnish, distinguish paper weights by gsm alongside US basis weights—US Cover LB (measured on a 20 × 26 in basis sheet) and US Text LB (measured on a 25 × 38 in basis sheet)—because the same pound number represents a much lighter sheet in Text LB than in Cover LB:
- Card Stocks (Cover LB equivalents):
- 300 gsm art / blue-core stock: 0.28–0.31 mm (0.0110–0.0122 in)
- 310 gsm black-core linen stock: 0.30–0.32 mm (0.0118–0.0126 in)
- 330 gsm black-core stock: 0.32–0.34 mm (0.0126–0.0134 in)
- 350 gsm art stock: 0.34–0.38 mm (0.0134–0.0150 in)
- 400 gsm art stock: 0.40–0.44 mm (0.0157–0.0173 in)
- PVC card stock: 0.30 mm (0.0118 in)
- Booklet & Box Component Stocks:
- Booklet interiors use 80–120 gsm Text LB stocks, about 0.08–0.13 mm (0.0031–0.0051 in) per sheet, while booklet covers use 200–300 gsm Cover LB stocks.
- Rigid boxes and boards use 1.5 mm, 2 mm, 2.5 mm, or 3 mm (0.059 in, 0.079 in, 0.098 in, or 0.118 in) greyboard with a 15–20 mm (0.591–0.787 in) wrap margin.
- Stack Height & Box Clearance: Because liquid soft-touch coating adds 0 mm (0 in) of film caliper, a 54-card or 78-card deck keeps its bare-stock stack height. Maintain 1.5–2.5 mm (0.059–0.098 in) box clearance across width and height and 1.5–3 mm (0.059–0.118 in) for stack height.
Prepress & Ink Limits
- File Setup: Supply AI, PDF, or PSD files in PDF/X-1a or PDF/X-4 format with outlined or embedded fonts and ≥300 DPI raster assets.
- Color & Ink Density: Build artwork in CMYK with separate spot layers for any foil or spot UV masks. Keep fine text at 100% K, use rich black at C40–60 M30–40 Y30–40 K100, and cap Total Area Coverage (TAC) at ≤280%–300% so liquid varnish wets and cures evenly over heavy ink coverage.
- Bleed, Safety & Corners: Provide 3 mm (0.118 in) bleed per side, ≥3 mm (0.118 in) safety margin (≥4–5 mm / 0.157–0.197 in for bordered backs), and R3–R3.5 mm (0.118–0.138 in) rounded corners.
Production & Cure Workflow
Specialist offset and tabletop manufacturing partners apply liquid soft-touch coating as a controlled liquid film rather than a heat- or pressure-bonded laminate:
- Ink Drying & Cure Window: Offset CMYK inks must oxidize or UV-cure sufficiently before liquid soft-touch application. Applying aqueous velvet varnish over wet offset ink causes mottling or ink-transfer blocking in the delivery pile.
- Flood Coating Application: The press applies either a water-based aqueous soft-touch dispersion (dried via heated air knives and IR lamps) or a UV-curable soft-touch resin (cross-linked instantly under UV lamps) via anilox or blanket roller.
- Pile Weight & Cure Stabilization: Freshly coated press sheets are stacked in controlled lifts—typically keeping lift weights moderate (around 10–15 kg / 22–33 lb per rack tray during thermal off-gassing) so bottom sheets do not press tacky varnish into adjacent backs before full cross-linking.
- Post-Coat Finishing & Die-Cutting: Because there is no plastic BOPP skin, steel-rule dies and corner-rounding punches cut cleanly through the coated paperboard without stretching film at the perimeter. If pairing with gilded edges or spot UV, the zero-thickness coating avoids edge ridges; for dark artwork exposed to heavy handling, anti-scuff matte formulations or film lamination are evaluated against the deck's expected shuffle wear.
- Format Decisions: Standard card decks and custom-sized tabletop cards follow the same liquid-coat cure sequence, while boxed games and custom tooling follow project and component minimums.
Sign-Off Criteria
Production sign-off checks physical cure, surface friction, and edge integrity before bulk collation:
- Tactile & Gloss Uniformity: The sheet shows a consistent, dead-flat velvet matte sheen across both unprinted paper margins and dense rich-black solids, with no glossy streaks or orange-peel texture from uneven anilox transfer.
- Cure & Rub Resistance: A firm finger or dry-cloth rub test across C40–60 M30–40 Y30–40 K100 dark solids leaves no ink smear, varnish lift, or immediate shiny burnish track.
- Zero Blocking: Stacked cards and press sheets separate cleanly without fiber tearing or varnish picking between face and back.
- Clean Die-Cut Perimeter: Rounded corners (R3–R3.5 mm / 0.118–0.138 in) and trimmed edges show crisp paperboard fibers with zero flaking or peeling.
- Regulatory & Material Records: Where finished games or card decks fall under children's product rules, coating formulations and cured samples undergo applicable assessment and testing under EU Toy Safety (EN 71) with retained lab documentation.
Concrete Failure Modes & Remedies
| Failure Mode | Physical Cause | Production Remedy |
|---|---|---|
| Rapid Surface Burnishing | High-friction shuffling or card-on-card rubbing polishes the soft-touch resin peaks flat, creating shiny scuff marks—most visible on dark artwork. | Switch heavy-play decks to anti-scuff matte or soft-touch BOPP film; keep liquid soft-touch for lower-friction cards, collector tuck boxes, or rigid box wraps. |
| Tacky Feel or Sheet Blocking | Excessive ink density (TAC >300%), insufficient UV lamp output, or stacking heavy lifts (>15 kg / 33 lb) before aqueous moisture evaporates. | Cap TAC at ≤280%–300%, extend IR/UV cure dwell, and rack sheets in shallower lifts during cooling. |
| Edge Cracking on Folded Tuck Boxes | Thick liquid UV resin bridges tightly scored creases on 300–400 gsm Cover LB stock and fractures along the fold line. | Use flexible aqueous soft-touch dispersion on scored packaging, widen score channels, or switch folded tuck boxes to flexible BOPP film. |
| Coating Crawling / Pinholes | Residual press spray powder or silicone contamination on ink surfaces repels the liquid varnish. | Minimize anti-set-off spray powder before offline coating and verify surface tension compatibility between ink set and varnish. |
Parent guide Protective Coatings and Laminates