Cured UV resin—especially high-build raised UV—is rigid and brittle compared to flexible BOPP film and paperboard fibers. When a sheet is scored, folded 90 degrees around greyboard, or creased 180 degrees along a tuck flap or booklet hinge, any UV resin sitting inside the fold zone fractures, whitens, or lifts away from the BOPP surface.
Two conditions change how tight you can run UV near a fold or edge:
- Flat spot UV vs. raised UV: Standard flat spot UV lays down a thin varnish layer that tolerates minor flex near a 2 mm (0.079 in) offset, whereas raised UV cures into a thick, tactile dome that requires the full 3 mm (0.118 in) clearance from any crease, hinge, or wrap turn-in.
- Lamination film type: Dark solid artwork (such as rich black C40–60 M30–40 Y30–40 K100) should use anti-scuff matte BOPP rather than standard matte BOPP so handling marks do not dull the contrast around gloss UV elements. For broader film-selection rules and surface-energy requirements, see BOPP lamination and spot UV compatibility.
Specifications and Knockout Clearances
Design the UV spot layer as a separate vector mask in 100% K inside your AI, PDF, or PSD layout (exported as PDF/X-1a or PDF/X-4 at ≥300 DPI with outlined or embedded fonts). Keep total area coverage (TAC) at ≤280%–300% and use 100% K for fine text so the underlying ink dries cleanly before BOPP lamination.
In US paper weights, distinguish Cover LB (20 × 26 in basis sheet) from Text LB (25 × 38 in basis sheet): a 200–300 gsm cover stock equals approximately 74–111 lb Cover (equivalent to 135–203 lb Text), while 80–120 gsm booklet interior sheets equal approximately 54–81 lb Text.
| Component | Typical Stock & Construction | Minimum UV Knockout Clearance | Bleed & Geometry Notes |
|---|---|---|---|
| Tuck boxes | 300–400 gsm (111–148 lb Cover) art or folding board; 0.28–0.44 mm (0.011–0.017 in) base caliper | 2–3 mm (0.079–0.118 in) from all score and crease lines | Hold UV back from dust-flap hinges, side-seam glue flaps, and thumb-notch cuts; account for 1.5–2.5 mm (0.059–0.098 in) width/height box clearance. |
| Rigid-box wraps | Printed wrap laminated with BOPP and mounted over 1.5, 2.0, 2.5, or 3.0 mm (0.059, 0.079, 0.098, or 0.118 in) greyboard | 2–3 mm (0.079–0.118 in) from all 90-degree box edges and corners | Keep raised UV off the 15–20 mm (0.591–0.787 in) wrap turn-in margin so wraps seat flat inside the greyboard corners. |
| Folding boards | BOPP-laminated wrap mounted onto hinged greyboard panels | 3 mm (0.118 in) on both sides of every fold channel | Do not bridge UV across panel hinges; keep ≥3 mm (0.118 in) safety from outer board trim and 3 mm (0.118 in) bleed on full-bleed wraps. |
| Booklet covers | 200–300 gsm (74–111 lb Cover) cover over 80–120 gsm (54–81 lb Text; 0.08–0.13 mm / 0.0031–0.0051 in per sheet) interiors | 2–3 mm (0.079–0.118 in) from spine scores and fold hinge | Applies to saddle-stitch (12–40 pages), perfect-bound (28+ pages), and sewn (80–100+ pages recommended) spines in 4-page signature multiples. |
Note on film thickness: Double-sided BOPP film adds 0.03–0.05 mm (0.0012–0.0020 in) to a sheet; single-sided box and cover lamination adds roughly half that amount (0.015–0.025 mm / 0.0006–0.0010 in) and must be factored into tight slipcase or tuck-flap tolerances.
Production Steps and Sign-Off Criteria
- Knock out the UV mask against the dieline: Overlay the final structural dieline (creases, scores, spine width, and wrap turn-ins) on the 100% K spot UV layer and subtract a 2–3 mm (0.079–0.118 in) buffer around every fold or corner line.
- Print and cure CMYK ink: Run offset CMYK with TAC capped at ≤280%–300% and allow adequate drying time so residual solvents do not interfere with BOPP adhesion.
- Apply UV-receptive BOPP film: Laminate the printed press sheet with matte or anti-scuff matte BOPP formulated for secondary UV adhesion.
- Apply and cure spot or raised UV: Register the UV plate or digital UV pass to the laminated sheet, keeping fine UV details clear of fold zones and glue areas.
- Die-cut, crease, wrap, or bind: Score and fold tuck boxes, wrap 15–20 mm (0.591–0.787 in) margins onto greyboard, or score and bind 200–300 gsm (74–111 lb Cover) booklet covers.
Sign-off criteria before full-run production:
- Spot and raised UV edges align cleanly with underlying artwork with no visible haloing or shift into the 2–3 mm (0.079–0.118 in) crease buffer.
- Folding a finished tuck box, rigid-box wrap corner, board hinge, or booklet cover to its full operating angle produces zero resin cracking, whitening, or edge lifting.
- Glued side seams on tuck boxes and 15–20 mm (0.591–0.787 in) wrap margins on rigid boxes sit completely free of UV resin so adhesives bond directly to the board or BOPP surface.
Concrete Failure Modes
- Resin cracking and flaking along creases: Spot or raised UV placed within 2 mm (0.079 in) of a tuck-box score or booklet spine snaps during folding, leaving jagged white fracture lines and loose resin flakes.
- Corner lifting on rigid-box wraps: Raised UV extending into a 90-degree box corner or 15–20 mm (0.591–0.787 in) turn-in resists wrapping over 1.5–3.0 mm (0.059–0.118 in) greyboard, causing the wrap to spring back or delaminate at the corner.
- Hinge splitting on folding boards: UV cured across a board hinge tears the BOPP surface or cracks along the fold channel the first time the board opens flat.
- UV beading or peeling on BOPP: Applying UV over low-surface-energy BOPP or uncured high-TAC ink (>300%) prevents proper wetting and causes the cured UV layer to peel off under light fingernail pressure.
- Scuffing around gloss UV on dark covers: Using standard matte BOPP under rich black artwork shows burnished rub marks beside high-gloss UV domes; switch to anti-scuff matte BOPP for dark backgrounds.