This split is required whenever a booklet pairs a coated 200–300 gsm cover with an uncoated 80–120 gsm interior. Three conditions change how you apply it:
- Coated interior stock: If the interior pages use coated matte or gloss text stock instead of uncoated paper, convert both cover and interior with the matching coated profile, keeping total ink coverage conservative on lighter text weights.
- Uncoated cover stock: If both the cover and interior run on uncoated paper, apply the uncoated CMYK profile to both files so shared artwork and neutral tones stay consistent across the binding.
- Dark artwork with anti-scuff matte: When a coated cover uses heavy dark solids and an anti-scuff matte finish, keep rich black within C40–60 M30–40 Y30–40 K100 and stay within the 280%–300% total area coverage (TAC) ceiling so ink dries cleanly before finishing.
For general separation rules across other print components, see CMYK conversion.
Paper Stocks, Profiles, and Ink Limits
Coated covers and uncoated interior pages absorb ink differently on press. Coated stock seals the surface so halftone dots stay sharp, whereas porous uncoated fibers absorb ink and swell the dots (dot gain), darkening midtones and shadows. Converting both components through the right profile during CMYK conversion adjusts ink curves before plates are made.
Note that US paper weights use different basis sheet sizes for covers and text pages: Cover LB is measured on a 20 × 26 in (508 × 660 mm) basis sheet, while Text LB is measured on a 25 × 38 in (635 × 965 mm) basis sheet.
| Specification | Booklet Cover (Coated) | Interior Pages (Uncoated) |
|---|---|---|
| Stock weight | 200–300 gsm (approx. 74–111 lb Cover, 20 × 26 in / 508 × 660 mm basis) | 80–120 gsm (approx. 54–81 lb Text, 25 × 38 in / 635 × 965 mm basis) |
| Sheet caliper | Varies by board/cover grade | Approx. 0.08–0.13 mm (0.003–0.005 in) per sheet |
| CMYK profile type | Coated CMYK profile | Uncoated CMYK profile (pulls back midtones/shadows for dot gain) |
| Total Area Coverage (TAC) | ≤280%–300% | ≤280%–300% ceiling (uncoated profiles naturally cap lower) |
| Rich black (large solids) | C40–60 M30–40 Y30–40 K100 | Avoid heavy rich black on thin sheets; keep under-color light |
| Fine text and rules | 100% K only | 100% K only |
| Bleed and safety | 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) safety | 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) safety |
| File standard and resolution | PDF/X-1a or PDF/X-4, ≥300 DPI | PDF/X-1a or PDF/X-4, ≥300 DPI |
Booklet binding also governs file layout. Bound signatures run in multiples of four pages: saddle stitch suits 12–40 pages, perfect binding suits 28+ pages, and sewn binding is recommended for 80–100+ pages.
Prepress Separation and File Setup
- Split cover and interior files: Export the cover and interior as separate print-ready PDFs rather than one combined document. Deliver the interior as sequential single pages in a multiple of four, and deliver the cover as a 4-page cover (for saddle stitch) or a full outer wrap with the calculated spine width (for perfect or sewn binding).
- Convert artwork with separate CMYK profiles: Convert cover images and graphics from RGB or working space into the coated CMYK profile. Convert interior graphics into the uncoated CMYK profile so the separation reduces midtone and shadow dot values to offset ink spread on uncoated fibers.
- Lock black ink and TAC: Set all body copy, captions, and thin rules to 100% K only with overprint enabled so small type prints on a single plate. For large dark fills on a coated cover, build rich black at C40–60 M30–40 Y30–40 K100, and verify in separation preview that no pixel exceeds 280%–300% TAC.
- Isolate spot layers and multilingual black plates: Place specialty finishes—such as spot varnish, foil, or Pantone brand inks—on separate named spot layers rather than flattening them into CMYK. For multilingual runs, keep all translated text on the 100% K plate so only the black plate swaps between languages while the CMYK artwork plates remain unchanged.
- Export to PDF/X with bleed and fonts: Export using PDF/X-1a or PDF/X-4 (AI, PDF, or PSD source workflows), keeping raster artwork at ≥300 DPI, 3 mm (0.118 in) bleed on all trim sides, and all fonts embedded or outlined.
Sign-Off Criteria Before Printing
- Two separate files: Cover PDF and interior PDF are delivered separately, with the interior page count in a multiple of four matching the chosen binding method (12–40 pages saddle stitch, 28+ perfect bound, or 80–100+ sewn).
- Correct profile assignment: Coated output intent is applied to the cover PDF and uncoated output intent is applied to the interior PDF, with no uncalibrated RGB elements left in either file.
- Ink and black-plate checks: TAC measures ≤280%–300% across all separations, fine text reads 100% K only (0% C/M/Y), and any multilingual text sits strictly on the K plate.
- Geometry and asset integrity: All pages include 3 mm (0.118 in) bleed per side, ≥3 mm (0.118 in) safety margin from trim, ≥300 DPI effective image resolution, embedded or outlined fonts, and isolated spot layers where applicable.
Concrete Failure Modes
- Plugged shadows on uncoated interior pages: Converting interior pages with a coated CMYK profile leaves excess cyan, magenta, and yellow in 70%–95% tones; on 80–120 gsm uncoated paper, dot gain fills in the paper grain, turning dark illustrations muddy and shifting neutral grays warm or brownish.
- Visible color shift between cover and text pages: Using identical CMYK numbers across the 200–300 gsm coated cover and the uncoated interior causes shared backgrounds or icons to print crisp and saturated on the cover but flat and overly dark inside.
- Set-off and show-through on thin sheets: Pushing ink density near 280%–300% TAC on 80–120 gsm (0.08–0.13 mm / 0.003–0.005 in) uncoated stock slows drying, transferring wet ink onto the facing page during folding and stacking or showing dark graphics through from the reverse side.
- Fuzzy type and broken black-plate swaps: Leaving body text in 4-color process black instead of 100% K introduces color fringing from minor press misregistration and forces full 4-plate remakes for every language version instead of a single black-plate swap.
- Scuffing on dark coated covers: High-ink dark artwork on a coated cover marks easily during trimming and binding if an anti-scuff matte coating is omitted.
Parent guide CMYK Color Conversion and Output Profiles