Several job conditions shift where you set total ink within that range:

  • Sheet stacking and uncoated or textured surfaces: Keep Total Area Coverage (TAC) near the lower 280% cap on heavy ink-coverage sheets where wet ink sits in the delivery pile before curing.
  • Laminated dark backs: Anti-scuff matte lamination supports rich black up to 300% TAC once cured and hides rub marks on dark full-bleed backs. Double-sided film adds 0.03–0.05 mm (0.0012–0.0020 in) per card.
  • Gilded edges: Avoid combining heavy ink buildup at the trim line with thick lamination, because thick lamination can conflict with gilded-edge adhesion.
  • Fine text and thin knockouts: Use 100% K (C0 M0 Y0 K100) instead of rich black for small type and thin rules so minor plate shift does not create color fringes.

For general CMYK ink-density rules across other print components, see the rich black setup guide.

Full-Bleed Card Back Specifications

Parameter Specification Notes
Rich black CMYK mix C40–60 M30–40 Y30–40 K100 Balanced neutral-to-cool black
Total Area Coverage (TAC) <= 280%–300% Formula: C + M + Y + K <= 280% to 300%
Fine text / thin rules 100% K (C0 M0 Y0 K100) Prevents registration haloing
Bleed per side 3 mm (0.118 in) Extends rich black past trim on all four sides
Safety margin (borderless) >= 3 mm (0.118 in) Keeps key art clear of trim
Safety margin (bordered backs) >= 4–5 mm (0.157–0.197 in) Prevents uneven border appearance
Corner radius R3–R3.5 mm (R0.118–R0.138 in) Standard rounded card corners
Color mode & resolution CMYK + separate spot layers, >= 300 DPI No RGB elements
File format & fonts AI, PDF, or PSD as PDF/X-1a or PDF/X-4 Fonts outlined or embedded
Protective finish Anti-scuff matte lamination Suits dark full-bleed artwork

Prepress Setup Steps

  1. Build the background swatch and cap TAC. Set solid dark card backs to C40–60 M30–40 Y30–40 K100 (for example, C50 M40 Y40 K100 = 230% TAC). If the card back includes gradients, vignettes, or raster textures, verify that shadow peaks never exceed C + M + Y + K <= 280%–300%. Convert any R0 G0 B0 blacks to CMYK before export so the RIP does not output 340%+ four-color black.
  2. Isolate fine text and specialty spot layers. Assign small type and fine linework to 100% K only. Place metallic inks, foil stamps, or spot UV on separate spot layers rather than stacking them over full four-color rich black.
  3. Extend bleed and clear the corners. Run the rich black fill 3 mm (0.118 in) past the trim box on all four edges. Keep logos, borders, and critical graphics inside the >= 3 mm (0.118 in) safety margin—or >= 4–5 mm (0.157–0.197 in) on bordered backs—and check that R3–R3.5 mm (R0.118–R0.138 in) corner rounding does not clip corner elements.
  4. Export and inspect separations. Export PDF/X-1a or PDF/X-4 with fonts outlined or embedded and raster artwork at >= 300 DPI. Check the ink-coverage / separation preview across the trim and bleed zones before releasing the file to plating.

File Sign-Off Criteria

Confirm every item below before approving full-bleed dark card backs for press:

  • Separation preview shows C + M + Y + K <= 280%–300% across the entire card back and 3 mm (0.118 in) bleed zone.
  • Zero RGB blacks (R0 G0 B0) or 400% registration blacks appear anywhere in the artwork.
  • Fine text is 100% K only; specialty finishes sit on dedicated spot layers.
  • Bleed extends 3 mm (0.118 in) past trim on all four sides, and all interior elements respect the >= 3 mm (0.118 in) safety margin (>= 4–5 mm / 0.157–0.197 in for bordered backs) and R3–R3.5 mm (R0.118–R0.138 in) corners.
  • Output is PDF/X-1a or PDF/X-4 compliant at >= 300 DPI with all fonts outlined or embedded.

Concrete Failure Modes

  • Stack setoff on press sheets: Exceeding 300% TAC—most commonly from unconverted RGB black—leaves excess wet ink on the sheet surface. Under the weight of the delivery stack, wet ink from the card back transfers onto the face of the sheet underneath.
  • Edge chipping along cut edges and corners: Over-saturated ink forms a brittle layer along the trim path. When the cutting die or trimmer slices through 300–400 gsm card stock or 0.30 mm (0.012 in) PVC, thick ink fractures along the straight edges and R3–R3.5 mm (R0.118–R0.138 in) corners, exposing light paper core flecks.
  • Scuffing on unlaminated dark backs: Full-bleed dark backs without a protective film show bright rub streaks from press handling, collation, and shuffling. Anti-scuff matte lamination prevents surface abrasion on dark solids.
  • Color fringing on small reverse text: Using four-color rich black for fine type or placing dense four-color builds right against micro-knockouts produces visible cyan, magenta, or yellow halos if plates shift slightly on press.
  • Gilded-edge adhesion conflict: Heavy ink coverage at the trim edge paired with thick lamination (0.03–0.05 mm / 0.0012–0.0020 in double-sided film) can interfere with edge gilding adhesion.