In offset and specialty tabletop printing with manufacturing partners, white ink is laid down as a separate opaque spot layer before CMYK passes. Because sheet-fed and flatbed presses have finite mechanical registration tolerance between the white pass and the CMYK passes, any unchoked white underbase aligned 1:1 with the artwork edge will shift into view as a sharp white halo against metallic foil or transparent stock. For broader color trapping rules across standard paperboard, see trapping and chokes.

Conditions That Change the Choke

  • Opaque color vs. metallic or clear show-through: Areas that must look solid and true to CMYK color require a choked white underbase underneath them. Areas intended to flash metallic foil or remain see-through on clear PVC or acrylic must have zero white ink in the spot channel.
  • Substrate stability: Flexible clear PVC (0.30 mm / 0.012 in), foil-laminated card stocks, and rigid acrylic game pieces expand and feed differently through presses. Less stable substrates or multi-pass runs require a slightly deeper inward choke than rigid, dimensionally stable sheets.
  • Fine text and thin linework: Thin strokes and small 100% K text cannot withstand a heavy inward choke because contracting both sides of a narrow stroke erases the white core entirely. Either thicken the graphic so a continuous white core remains, or omit the white underbase under 100% K text so black ink prints directly onto the foil or clear surface.
  • Full-bleed edges: Artwork that runs to the edge of a card needs 3 mm (0.118 in) bleed per side. When a foil border or clear edge is desired, stop the white underbase inside the safety zone rather than extending it into the bleed.

Prepress and File Specifications

Parameter Specification
Accepted formats AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4
Color separation CMYK process layers plus a separate named spot layer for white ink
Resolution >=300 DPI for all raster artwork and white spot masks
Fonts Outlined or embedded
Black ink 100% K for fine text; rich black C40–60 M30–40 Y30–40 K100
Total Area Coverage (TAC) <=280%–300%
Bleed and safety 3 mm (0.118 in) bleed per side; >=3 mm (0.118 in) safety (>=4–5 mm / 0.157–0.197 in for bordered backs)
Card corners and PVC caliper R3–R3.5 mm (R0.118–0.138 in) corners; clear PVC at 0.30 mm (0.012 in); double-sided film adds 0.03–0.05 mm (0.0012–0.0020 in) per card

Production Steps for White Underbase Choking

  1. Map opaque and open zones: Split the design into regions that need an opaque white backing and regions that stay bare foil or transparent.
  2. Isolate the white spot layer: Duplicate the opaque artwork silhouettes onto a dedicated spot-color layer or channel, keeping it separate from CMYK and any additional specialty foil or varnish masks.
  3. Contract the white perimeter inward: Apply an inward choke (negative offset) to the white spot shapes so every outer edge of the white underbase sits slightly inside the CMYK boundary.
  4. Set overprint behavior: Configure the CMYK artwork to overprint the white spot layer rather than knocking it out, so CMYK inks print directly on top of the white base and overlap its choked edge onto the substrate.
  5. Inspect separations before export: Check the file in overprint preview to verify that the white spot channel is present, properly choked, and free of accidental knockouts, then export as PDF/X-1a or PDF/X-4.

Sign-Off Criteria Before Printing

  • Single dedicated spot channel: White ink exists as one clearly labeled spot layer separate from CMYK.
  • Verified inward offset: Overprint preview shows CMYK edges extending past the white underbase perimeter on every opaque shape.
  • Intact fine details: Thin rules and small 100% K text either hold a continuous white core or intentionally omit the white underbase.
  • Clean transparent and foil zones: Intended metallic or clear areas show 0% white spot coverage and do not carry unintended CMYK background tints.
  • Preflight compliance: Bleed (3 mm / 0.118 in), safety (>=3 mm / 0.118 in, or >=4–5 mm / 0.157–0.197 in on bordered backs), >=300 DPI resolution, and TAC <=280%–300% pass without flattening errors.

Concrete Failure Modes

  • Bright white halo around artwork: Pushing the white mask outward (spreading) or leaving it at a 1:1 edge with CMYK causes normal press registration shift to expose a bright white outline around dark or colored graphics on foil and clear stock.
  • White shapes knocking out CMYK: Leaving the white spot layer set to knock out underlying channels erases the CMYK artwork on top, leaving blank white silhouettes instead of colored graphics.
  • Washed-out or broken thin strokes: Applying an aggressive inward choke to hairline rules or small type collapses the white underbase in the center, leaving CMYK ink translucent against metallic foil or clear PVC.
  • Cloudy foil or blocked transparency: Flattening spot channels into CMYK or leaving low-percentage white tint in open areas turns intended mirror-foil highlights or clear acrylic windows dull and milky.