Required Component Files and Naming
Dual-layer player boards combine a punched upper greyboard sheet mounted onto a solid lower greyboard base. Because the top and bottom layers are printed, wrapped, and die-cut in separate operations before lamination, every physical layer needs its own production file tied together by a shared board identifier and revision tag.
| Component | Purpose in Production | Recommended Filename Pattern | Condition |
|---|---|---|---|
| Top cutout wrap | Prints the upper face, outer edge turn-ins, and cutout bleed | <job>_<board-id>_top-wrap_v<n>.pdf |
Always required |
| Top underside / liner | Lines the back of the top layer or full board back | <job>_<board-id>_top-liner_v<n>.pdf |
Required when top layer is double-wrapped or back-lined |
| Bottom recessed-well wrap | Prints the base artwork visible inside the wells and outer back | <job>_<board-id>_bottom-base_v<n>.pdf |
Always required |
| Die-cut template | Defines outer trim, crease lines, and window cutouts | <job>_<board-id>_dieline_v<n>.pdf |
Always required |
| Composite alignment PDF | Flattened visual proof showing top windows over bottom art | <job>_<board-id>_composite-proof_v<n>.pdf |
Always required |
| Specialty finish mask | Separates spot UV, foil, or tactile varnish areas | <job>_<board-id>_spot-<finish>_v<n>.pdf |
Required when spot finishes are specified |
Use ASCII characters, lowercase letters, hyphens, and underscores in filenames. Avoid generic labels such as final, print, or layer1, which cause top and bottom wraps to be swapped during imposition.
Specifications and Technical Tolerances
All production print files must be supplied in AI, PDF, or PSD source format—exported as PDF/X-1a or PDF/X-4—with fonts outlined or embedded and raster artwork at 300 DPI or higher.
- Board thickness and wrap margins: Standard greyboard cores run 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in) per layer. Outer wraps require a 15–20 mm (0.591–0.787 in) wrap margin beyond the finished board edge to turn cleanly over the greyboard sides.
- Cutout bleed and safety: Extend top-wrap artwork 3 mm (0.118 in) into every cutout window so paper wrapping or die shift does not expose bare greyboard. Keep critical text, icons, and track numbers at least 3 mm (0.118 in) inside window edges and outer trim lines.
- Die gap between windows: Maintain at least 3–4 mm (0.118–0.157 in) of solid greyboard between adjacent recessed wells. Narrower bridges crush or tear during punching and fail to bond flat against the base layer.
- Color and ink limits: Build print layers in CMYK with separate spot-color layers for die-lines and specialty masks. Set fine text and small track numbers to 100% K, use rich black (C40–60 M30–40 Y30–40 K100) for solid dark backgrounds, and keep Total Area Coverage (TAC) at or below 280%–300%. Anti-scuff matte lamination suits dark artwork on heavily handled boards.
Job-Specific Delivery Steps
- Lock a shared artboard origin: Place the die-cut template at the exact same X/Y coordinates across the top wrap, bottom base, and specialty mask files so every layer aligns to one reference corner.
- Extend wrap and window bleeds: Pull the top-wrap background across the 15–20 mm (0.591–0.787 in) outer wrap margin and 3 mm (0.118 in) into all cutout openings. Extend the bottom recessed-well artwork 3 mm (0.118 in) beyond every window perimeter so slight mounting variance stays covered.
- Separate non-printing geometry: Place cut, crease, and window-knockout paths on dedicated spot-color layers set to overprint, or keep them strictly in the standalone die-cut template file rather than flattened into CMYK art.
- Generate the composite alignment PDF: Export a flattened, non-production reference PDF that places the top-wrap layer—with its window cutouts knocked out—directly over the bottom recessed-well wrap.
- Verify folder completeness: Group the production PDFs, die-cut template, specialty masks, and composite proof into a single versioned directory before upload.
Sign-Off Criteria
Prepress clears the package for plating when all of the following conditions are verified:
- All five core files (plus any required specialty masks) are present in the same versioned folder with matching
<board-id>and<n>revision numbers. - Top wrap, bottom wrap, and die-cut template share identical trim dimensions and registration origin.
- Outer wrap margins measure 15–20 mm (0.591–0.787 in), window bleeds measure 3 mm (0.118 in), and adjacent cutouts maintain a 3–4 mm (0.118–0.157 in) gap.
- Die-lines and specialty masks sit on named spot layers set to overprint, with CMYK TAC at or below 280%–300%.
- The composite alignment PDF confirms that bottom-layer icons, numbers, and wells sit centered inside the top-layer cutouts.
Failure Modes
- Missing composite alignment PDF: Without a flattened proof showing the top cutouts over the bottom art, prepress cannot confirm whether recessed-well graphics were intended to center inside windows or align to an edge, delaying plate approval.
- Trim bleed used instead of wrap margin: Supplying only a 3 mm (0.118 in) bleed on the outer perimeter instead of a 15–20 mm (0.591–0.787 in) wrap margin leaves raw greyboard exposed along the edges and corners of the finished board.
- Die-line flattened into CMYK: Merging the cut template into the CMYK artwork prints visible hairline cut marks around every window or creates white knockout halos if the stroke is not set to overprint.
- Narrow bridges between wells: Spacing recessed cutouts closer than 3–4 mm (0.118–0.157 in) causes the greyboard strip between wells to tear during die-cutting or delaminate during board mounting.
- Mismatched file revisions: Pairing a revised die-cut template (
v2) with an older top or bottom wrap (v1) shifts window openings off the printed well graphics and forces a full reprint of the affected wrap sheet.
Parent guide Delivery Package Completeness and File Naming
Related guides
- Package Completeness and Naming for Folding Game Boards
- Package Completeness and Naming for Bound Booklets and Leaflets
- Package Completeness and Naming for Custom Card Decks
- Package Completeness and Naming for Foil Boosters
- Package Completeness and Naming for Jigsaw Puzzles
- Package Completeness and Naming for Punchboards