This setup applies to exported folding board wraps prepared for mounting over rigid greyboard. The exact layer structure shifts under two conditions:
- Specialty finishes included: Add a dedicated named spot separation for spot UV or foil masks rather than nesting them inside the CMYK or structural guide layers.
- PDF/X-1a vs. PDF/X-4 export: PDF/X-1a flattens transparency before plate output, which can accidentally merge or knock out un-overprinted strokes; PDF/X-4 preserves live spot layers and overprint attributes through RIP processing.
For broader plate, imposition, and file-acceptance rules across all components, see the Separations and Layers Preflight overview.
Wrapping and Separation Specifications
| Parameter | Specification | Notes |
|---|---|---|
| File formats | AI, PDF, or PSD (PDF/X-1a or PDF/X-4) | Fonts outlined or embedded |
| Raster resolution | >= 300 DPI | Measured at final 1:1 print scale |
| Greyboard core thickness | 1.5 / 2 / 2.5 / 3 mm (0.059 / 0.079 / 0.098 / 0.118 in) | Dictates hinge channel width and wrap allowance |
| Wrap / turn-in margin | 15–20 mm (0.591–0.787 in) | Artwork must extend across the full turn-in |
| Bleed | 3 mm (0.118 in) per side | Added beyond the outer cut edge of the wrap |
| Safety margin | >= 3 mm (0.118 in) | Keep text and critical graphics clear of folds and edges |
| Fine text | 100% K | Prevents registration halos on small type |
| Rich black | C40–60 M30–40 Y30–40 K100 | Used for large dark fills |
| Total Area Coverage (TAC) | <= 280%–300% | Anti-scuff matte film suits dark artwork |
Required Separation Structure
- CMYK Artwork (Printing): Contains all process-color graphics, rich black backgrounds, and 100% K fine text. Extends continuously through the 15–20 mm (0.591–0.787 in) turn-in margin and 3 mm (0.118 in) bleed.
- Crease and Dieline Guides (Non-Printing Spot): Assigned a distinct named spot swatch (such as
CreaseorDieline) with Overprint Stroke enabled. Excluded from final CMYK plate output. - Spot Finish Mask (Separate Spot): Assigned its own named spot swatch (100% solid tint) for foil or spot UV, kept separate from both CMYK plates and structural dielines.
Job-Specific Preflight Steps
- Verify export standard and resolution: Open the exported PDF/X-1a or PDF/X-4 file in your prepress viewer. Confirm all fonts are outlined or embedded and placed raster art meets >= 300 DPI at 100% scale.
- Isolate the crease and dieline separation: Open the Output Preview / Separations panel and turn off the Cyan, Magenta, Yellow, and Black plates. Confirm that all fold-crease lines, hinge guides, and board-edge dielines remain visible as a single named spot color. If any guide line disappears when CMYK is turned off, it was flattened into process ink.
- Check for knockouts beneath guides: Turn the structural spot separation off while keeping CMYK active. Inspect every fold line and board edge at high zoom to verify that the underlying CMYK artwork is continuous with no white hairline gaps where the guide line sat.
- Measure turn-in and safety boundaries: Confirm that wrap artwork extends 15–20 mm (0.591–0.787 in) past the board edge (plus 3 mm / 0.118 in bleed) to wrap cleanly around the 1.5–3 mm (0.059–0.118 in) greyboard core. Verify that logos, rules, and text stay at least 3 mm (0.118 in) inside fold creases and outer board edges.
- Audit specialty finish plates and ink density: Toggle any spot UV or foil separation on and off to confirm it registers to the CMYK art without merging into process plates. Run an ink-coverage check over dark backgrounds to confirm TAC stays at or below 280%–300% and rich black uses C40–60 M30–40 Y30–40 K100.
Sign-Off Criteria
- Turning off CMYK plates leaves only named non-printing structural spot guides and intentional spot finish masks visible.
- Turning off the crease/dieline spot plate leaves continuous, un-notched CMYK artwork across every fold and board edge.
- Outer wrap art covers the full 15–20 mm (0.591–0.787 in) turn-in margin plus 3 mm (0.118 in) bleed.
- Critical elements clear all fold lines and board edges by >= 3 mm (0.118 in).
- Total area coverage does not exceed 280%–300%, and fine text separates cleanly onto 100% K only.
Concrete Failure Modes
- Crease lines converted to 4-color black: Exporting RGB strokes or flattening transparency without preserving spot swatches bakes fold guides onto C, M, Y, and K plates, printing visible dark lines across the board hinges.
- Un-overprinted dielines knocking out CMYK: Leaving a spot dieline stroke set to knockout removes CMYK ink directly beneath the line, exposing white paper along the fold or board edge during mounting.
- Insufficient turn-in margin for greyboard thickness: Applying a standard 3 mm (0.118 in) bleed instead of the 15–20 mm (0.591–0.787 in) wrap margin leaves raw 1.5–3 mm (0.059–0.118 in) greyboard edges exposed on the underside of the board.
- Spot finish flattened into CMYK: Leaving a spot UV or foil layer as a process tint or RGB object prints the mask as ink on the paper rather than generating a separate finishing plate.
- Excessive TAC on dark wraps: Exceeding 280%–300% total ink density under dark artwork delays drying and increases ink cracking or scuffing along folding hinges, even when paired with anti-scuff matte lamination.
Parent guide Layers, Spot Channels, and Overprint Separation Preflight
Related guides
- Separation and Glue-Mask Preflight for Dual-Layer Boards
- Separation and Die-Layer Preflight for Punchboards
- Separation and Finish-Layer Preflight for Rigid Box Wraps
- Separation and Plate-Count Preflight for Bound Booklets
- Separation and Finish-Mask Preflight for Custom Cards
- White-Ink Underbase and Metallic Separation Preflight for Foil Boosters