This baseline changes under four physical conditions:
- Shared vs. island artwork: Adjacent tokens with identical background colors can share a continuous bleed across the 3–4 mm (0.12–0.16 in) die gap. Pieces with contrasting colors or distinct borders require isolated (island) bleed of 1.5–2 mm (0.06–0.08 in) per piece so neighboring colors do not cross onto the wrong token during die-shift.
- Greyboard core thickness: Thicker cores at 2.5 mm (0.098 in) and 3 mm (0.118 in) deflect the die blade and draw the printed liner inward more than 1.5 mm (0.059 in) or 2 mm (0.079 in) boards, requiring the full 4 mm (0.16 in) die gap and 3 mm (0.12 in) safe zone.
- Sheet perimeter vs. internal gutter: Internal gutters between punched pieces use 1.5–2 mm (0.06–0.08 in) bleed, whereas the outer perimeter of the full punchboard sheet requires a 15–20 mm (0.59–0.79 in) wrap margin on the printed liner to fold cleanly around the greyboard edge.
- Mechanical features: Standee base tabs, interlocking slots, and dial rivet holes add localized crush and radial tolerance, requiring the 2.5–3 mm (0.10–0.12 in) safe zone around every internal cutout as well as the outer perimeter.
For standard flat-trimmed components that do not use internal die-cut gutters, see Bleed and Safe Zones, which covers the standard 3 mm (0.118 in) outer bleed per side.
Punchboard, Standee, and Dial Layout Specifications
| Parameter | Specification | Notes & Conditions |
|---|---|---|
| Internal die gap (gutter) | 3–4 mm (0.12–0.16 in) | Minimum spacing between adjacent cut paths in the waste skeleton |
| Internal piece bleed | 1.5–2 mm (0.06–0.08 in) | Plain-text rule: Internal bleed per piece <= Die gap / 2 |
| Edge & feature safe zone | ≥ 2.5–3 mm (0.10–0.12 in) | Measured inward from cut lines, standee tab necks, and dial rivet holes |
| Outer sheet wrap margin | 15–20 mm (0.59–0.79 in) | Extended liner artwork around the outer greyboard sheet perimeter |
| Greyboard core thickness | 1.5 / 2 / 2.5 / 3 mm (0.059 / 0.079 / 0.098 / 0.118 in) | Use 4 mm (0.16 in) gap and 3 mm (0.12 in) safe zone on 2.5–3 mm boards |
| File format & PDF standard | AI, PDF, PSD; PDF/X-1a or PDF/X-4 | Fonts outlined or embedded; ≥300 DPI raster resolution |
| Color & ink limits | CMYK + separate spot layers; TAC ≤ 280%–300% | Fine text in 100% K; rich black C40–60 M30–40 Y30–40 K100 |
| Dark artwork finish | Anti-scuff matte lamination | Recommended when dark rich-black solids extend across die-cut edges |
Shared vs. Island Bleed in the Die Gap
The 3–4 mm (0.12–0.16 in) strip between punched pieces is discarded as a waste skeleton after die-cutting. How you fill that strip depends on adjacent piece contrast:
- Island bleed (default for mixed sheets): Extend each piece's edge art outward by 1.5–2 mm (0.06–0.08 in) and leave a clean break or neutral tone in the center of the die gap. Because
1.5 mm + 1.5 mm = 3 mm(0.06 in + 0.06 in = 0.12 in), a 1.5 mm (0.06 in) island bleed prevents adjacent pieces from overlapping inside a 3 mm (0.12 in) gap, while a 2 mm (0.08 in) island bleed fits a 4 mm (0.16 in) gap. - Shared bleed (uniform backgrounds): When a sheet holds identical tokens or tiles with a matching solid color or continuous texture, flood the entire 3–4 mm (0.12–0.16 in) die gap with that shared background. This eliminates visible white or neutral slivers if the die shifts slightly toward one side of the gutter.
- Double-sided alignment: On two-sided tokens, standees, and dials, mirror the dieline on the back sheet and match the bleed strategy on both faces so front-to-back registration tolerance does not expose unprinted liner stock.
Prepress Layout Steps
- Separate the dieline and specialty masks: Place all outer cut paths, standee tab contours, dial rivet holes, and any specialty finish masks on dedicated spot color layers set to overprint. Keep every cut path at least 3–4 mm (0.12–0.16 in) away from neighboring cut paths.
- Build internal bleed and outer wrap margins: Extend each punched piece's artwork by 1.5–2 mm (0.06–0.08 in) into the die gap (or flood shared backgrounds across matching pieces). Extend the full-sheet background 15–20 mm (0.59–0.79 in) beyond the greyboard trim edge for wrapping.
- Enforce safe zones around tabs and holes: Inset all icons, text, numeric tracks, and inner keylines at least 2.5–3 mm (0.10–0.12 in) from punched perimeters, standee slot shoulders, and dial center holes. Account for the physical rivet head diameter when placing dial pointer windows or inner rings.
- Set ink and export standards: Convert fine labels to 100% K, cap rich black at C40–60 M30–40 Y30–40 K100, and keep total area coverage (TAC) at or below 280%–300%. Export as PDF/X-1a or PDF/X-4 at ≥300 DPI with all fonts outlined or embedded.
File Acceptance and Sign-Off Criteria
Before releasing punchboard, standee, or dial files to plate-making and die tooling, verify the following conditions:
- Dieline separation: Cut, crease, and rivet-hole vectors sit on named spot layers set to overprint, not flattened into CMYK artwork.
- Minimum gutter clearance: All adjacent punched pieces maintain a 3–4 mm (0.12–0.16 in) gap with no overlapping island bleeds.
- Safe-zone clearance: No critical text, icon, standee foot detail, or dial numeral sits closer than 2.5–3 mm (0.10–0.12 in) to any cut path or rivet hole.
- Wrap margin integrity: Outer punchboard sheets include the full 15–20 mm (0.59–0.79 in) wrap margin on both top and back liners where applicable.
- Print-ready separations: Raster art is ≥300 DPI, TAC is ≤280%–300%, fine type is 100% K, and fonts are outlined or embedded in PDF/X-1a or PDF/X-4.
Concrete Failure Modes
- Bleed crossover on contrasting tokens: Extending island bleed beyond 2 mm (0.08 in) inside a 3–4 mm (0.12–0.16 in) die gap causes adjacent piece colors to bleed onto neighboring tokens whenever the die shifts laterally.
- Clipped rim borders and dial numbers: Placing thin frame borders or radial dial values within 2.5 mm (0.10 in) of a punched edge leads to uneven borders or sliced characters, amplified on 2.5–3 mm (0.098–0.118 in) greyboard where blade beveling pulls the top liner inward.
- Standee tab and rivet obstruction: Graphics placed near standee slot necks scuff or tear during assembly, and dial labels placed too close to the center hole get covered by the rivet flange.
- Exposed greyboard on sheet edges: Omitting the 15–20 mm (0.59–0.79 in) outer wrap margin leaves raw board visible along the sheet perimeter or causes liner lift at the corners.
- Printed dielines: Leaving cut paths in CMYK or failing to set the dieline spot layer to overprint prints visible hairlines around every token and knocks out underlying ink.
Parent guide Trim, Bleed, and Safe Zone Setup by Deliverable
Related guides
- Bleed and Edge-Piece Safe Zones for Jigsaw Puzzles, Stickers, and Postcards
- Outer Bleed and Gutter Safe Zones for Booklets and Art Books
- Bleed and Safe Zones for Standard Rectangular Cards
- Inner Well Bleed and Safe Zones for Dual-Layer Recessed Boards
- Wrap Bleed and Hinge Safe Zones for Folding Boards and GM Screens
- Oversized Bleed and Stitched-Border Safe Zones for Neoprene Mats