Conditions that change the setup:
- Board thickness: Standee slot widths and minimum bridge clearances must match the selected greyboard core caliper—1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in)—plus any surface wrap or film thickness.
- Multi-layer assemblies: Stacked dials and slotted standees require separate through-cut paths for removable pieces and half-cut or score paths for folding tabs, with every die stroke set to overprint so it never knocks out underlying artwork.
- General dieline conventions: Follow the layer naming and spot-color separation rules in Dieline and Markings before adding punchboard-specific geometry.
Specifications and Geometry Rules
| Parameter | Specification | Purpose |
|---|---|---|
| Greyboard core calipers | 1.5 / 2 / 2.5 / 3 mm (0.059 / 0.079 / 0.098 / 0.118 in) | Determines structural rigidity and standee slot width |
| Punchboard die gap | 3–4 mm (0.118–0.157 in) minimum | Keeps greyboard webs intact between adjacent cuts |
| Wrap margin (wrapped sheets) | 15–20 mm (0.591–0.787 in) | Covers board edges cleanly during mounting |
| Artwork bleed | 3 mm (0.118 in) per cut edge | Prevents white edges on tokens, slots, and dial windows |
| Safety margin | ≥3 mm (0.118 in) inside cut lines | Protects text, borders, and dial numerals from trim shift |
| Raster & color setup | CMYK + separate spot layers, ≥300 DPI | Ensures clean plate separations and sharp print detail |
| Black & ink limits | 100% K fine text; rich black C40–60 M30–40 Y30–40 K100; TAC ≤280%–300% | Prevents ink setoff and muddy registration |
| Export formats | AI, PDF, or PSD as PDF/X-1a or PDF/X-4 (fonts outlined or embedded) | Preserves vector die paths and spot separations |
Through-Cuts, Half-Cuts, and Score Lines
Place all cutting and creasing vectors on one top-level, non-printing layer. Assign a separate spot swatch to each rule type—such as Cut_Through for full-depth token and window cutouts, Cut_Half for partial-depth kiss-cuts or peel tabs, and Crease_Score for fold lines. Keep all die strokes set to Overprint Stroke with no fill so the rip excludes them from CMYK printing plates without creating white knockouts.
Die Nick Bridge Markers
Die nicks are small uncut bridges that hold punched tokens inside the waste frame during packing and shipping. Mark nick positions only where the manufacturing template specifies them, using a dedicated indicator or gap marker on the die layer. Do not interrupt the underlying CMYK artwork bleed at nick points.
Standee Slots and Tabs
Draw standee base slots as closed vector paths sized to the finished board thickness (core greyboard caliper plus wrap/film). Maintain the 3–4 mm (0.118–0.157 in) die gap between the slot cutout and the outer perimeter of the base so the surrounding board does not tear when the standee is inserted.
Coaxial Dial Windows and Rivet Holes
For rotating dials, the top cover sheet, viewing window cutout, center-rivet hole, and underlying rotating wheel must share one exact X/Y center coordinate.
- Rivet holes: Draw the center hole as a closed through-cut circle centered on the rotation axis across every stacked layer of the dial.
- Viewing windows: Position the window arc or cutout radially from that same center point, keeping dial numerals ≥3 mm (0.118 in) clear of the window edge and outer wheel trim.
Prepress Production Steps
- Build the layer stack: Create a locked artwork stack for CMYK print layers and place a single
Dielinelayer at the top, following Dieline and Markings. - Draw and join die paths: Construct closed, continuous vector outlines for all tokens, standee slots, dial wheels, and viewing windows. Merge overlapping anchor points so the die-maker receives clean single-stroke paths.
- Assign spot swatches and overprint: Color-code through-cuts, half-cuts, and scores with distinct named spot colors and enable Overprint Stroke on every path.
- Place template nick markers: Add nick position indicators at the exact coordinates specified by the punchboard template.
- Lock coaxial dial geometry: Snap the center-rivet hole, wheel perimeter, and viewing window on front and back spreads to the exact same center coordinates.
- Verify bleed and ink limits: Extend 3 mm (0.118 in) bleed into all waste areas, interior dial windows, and standee slots. Confirm fine text is 100% K, rich black stays within C40–60 M30–40 Y30–40 K100, and total area coverage is ≤280%–300%.
- Export and inspect separations: Export as PDF/X-1a or PDF/X-4 with fonts outlined or embedded, then toggle off the spot die layer in separation preview to confirm no white knockout gaps appear beneath the die lines.
Sign-Off Criteria
- Every through-cut, half-cut, and score line uses a distinct named spot color on the top dieline layer with Overprint Stroke active.
- All adjacent through-cut paths maintain a 3–4 mm (0.118–0.157 in) die gap.
- Die nick markers match the template layout and do not obscure critical token edges.
- Dial center-rivet holes, wheel perimeters, and viewing windows share identical X/Y center coordinates across all paired layers.
- Bleed extends 3 mm (0.118 in) past all outer and interior cut edges, and critical graphics sit ≥3 mm (0.118 in) inside cut lines.
- Exported PDF/X-1a or PDF/X-4 files contain outlined or embedded fonts, ≥300 DPI raster assets, and TAC ≤280%–300%.
Concrete Failure Modes
- White hairline knockouts around tokens: Leaving die strokes in CMYK or failing to enable overprint on spot die colors knocks out underlying ink, leaving visible white borders on punched edges.
- Crushed webs or premature token fallout: Spacing through-cut paths closer than the 3–4 mm (0.118–0.157 in) die gap collapses the greyboard bridge during die-cutting.
- Torn printed faces when punching: Omitting template nick markers or placing nicks across delicate edge artwork causes tokens to detach loose in transit or rip the surface wrap on removal.
- Jamming or misaligned dials: Shifting the center-rivet coordinate between the top viewing plate and the rotating wheel causes the dial to bind against the rivet or clip printed values inside the window.
- Wobbly or split standees: Drawing standee slots without matching the selected greyboard caliper—1.5, 2, 2.5, or 3 mm (0.059, 0.079, 0.098, or 0.118 in)—produces slots that are either too loose to hold the figure upright or too tight to insert without delaminating the edge.
Parent guide Vector Cut, Crease, Fold, Wrap, and Nick Markings
Related guides
- Cut Contour and Corner-Radius Markings for Standard and Shaped Cards
- Cut, Fold, and Cavity-Outline Markings for Inserts, Dividers, and EVA/Formed Trays
- Kiss-Cut, Perforation, and Reference-Grid Markings for Stickers, Postcards, and Puzzles
- Cut, Score, Perforation, and Glue-Area Markings for Tuck Boxes and Sleeves
- Crimp-Zone, Tear-Notch, and Eye-Mark Markings for Booster Wrappers
- Greyboard Score, Wrap-Trim, and Miter Markings for Rigid Boxes and Boards