For overall layer structure and finish selection, see the finish masks overview. The exact alignment and trapping rules depend on three job conditions:

  • Clear vs. opaque finishes: Clear spot coats (spot UV, spot varnish) sit over printed CMYK ink and require overprint, whereas opaque finishes (metallic foil, opaque white ink) interact directly with the substrate and require explicit knockout or underprint trapping.
  • Interior vs. full-bleed placement: Interior finish elements stay inside the safety margin, while edge-crossing finishes must extend through the full 3 mm (0.118 in) bleed.
  • Bordered backs and edge treatments: Bordered card backs require wider safety clearance (≥4–5 mm / 0.157–0.197 in) so minor die-cut movement does not make an aligned finish look off-center, and builds with gilded edges cannot pair with thick lamination.

Alignment and Registration Specifications

Parameter Specification Production Rule
Artboard & Trim Origin Identical (0, 0) origin and trim box across all layers Base CMYK and every spot mask share the exact same artboard dimensions.
Bleed 3 mm (0.118 in) per side Extend any edge-crossing finish mask to the outer bleed edge.
Safety Margin (Standard) ≥3 mm (0.118 in) inward from trim Keep non-bleed spot elements inside this boundary.
Safety Margin (Bordered Backs) ≥4–5 mm (0.157–0.197 in) inward from trim Prevents visible asymmetry between borders and finish masks after die cutting.
Corner Radius Clearance R3–R3.5 mm (0.118–0.138 in) Keep corner-adjacent spot elements clear of the rounded die path unless full-bleed.
File Format & Color Space AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 CMYK base with separate 100% spot-color layers or channels for each finish; ≥300 DPI for raster elements.
Ink Density Limits Fine text 100% K; rich black C40–60 M30–40 Y30–40 K100; TAC ≤280%–300% Prevents ink set-off and adhesion issues beneath finishes; use anti-scuff matte on dark artwork.
Registration Allowance Supplied trap / choke / spread value Apply along shared boundaries between opaque finishes and adjacent CMYK ink.

Knockout vs. Overprint Rules

Set knockout and overprint attributes by finish opacity so the base press run does not leave unintended holes or double-inked mud:

  • Clear finishes over CMYK (spot UV, gloss/matte varnish): Set the spot mask object or layer to overprint. The underlying CMYK artwork prints continuously across the sheet, and the clear coat applies on top in registration.
  • Opaque white ink underprint: Place opaque white on its own spot separation. Where CMYK prints on top of white, set the CMYK objects to overprint the white plate; apply the supplied registration allowance (choking the white underprint slightly inside the CMYK edge, or spreading per the job spec) so white edges do not peek out around colored artwork.
  • Metallic foil and opaque spot masks: Set the underlying CMYK to knock out where bare stock is required for adhesion, or overprint where the spec calls for foil over ink. Apply the supplied registration allowance so adjacent CMYK ink overlaps or clears the foil edge without leaving an unprinted halo.

Job-Specific Preparation Steps

  1. Lock the base artboard: Finalize the base CMYK artwork with the exact trim dimensions, R3–R3.5 mm (0.118–0.138 in) corner awareness, and 3 mm (0.118 in) bleed per side before building any mask. For non-standard deck formats, match the custom trim box provided for the job rather than forcing a generic frame.
  2. Duplicate coordinates to spot layers: Create one separate spot-color layer or channel per finish using the exact same artboard origin and bleed box as the base artwork. Do not crop mask files to the bounding box of the finish graphic.
  3. Assign overprint or knockout: Set clear finish masks to overprint and configure opaque white or foil masks per the finish spec. Check TAC ≤280%–300% on the base CMYK layer, keeping fine text at 100% K and rich black at C40–60 M30–40 Y30–40 K100.
  4. Apply the supplied registration allowance: Add the specified choke or spread along every boundary where an opaque finish meets printed CMYK. Verify that full-bleed masks extend the entire 3 mm (0.118 in) past trim and interior masks respect the ≥3 mm (0.118 in) safety zone (or ≥4–5 mm / 0.157–0.197 in on bordered backs).
  5. Export and inspect separations: Outline or embed all fonts and export as PDF/X-1a or PDF/X-4. Open the exported PDF in separation and overprint preview to verify that toggling each spot plate leaves the base CMYK intact where expected and aligned 1:1 with the trim box.

Sign-Off Criteria

  • Base CMYK and all finish mask plates share identical trim box and 3 mm (0.118 in) bleed box coordinates with zero X/Y offset.
  • Separation preview confirms every finish sits on its own dedicated spot plate, with overprint active on clear finishes and no unintended CMYK knockouts.
  • Supplied registration allowance is applied at all opaque-finish-to-ink boundaries, and safety margins (≥3 mm / 0.118 in standard, ≥4–5 mm / 0.157–0.197 in bordered backs) are clear.
  • Fonts are outlined or embedded, raster resolution is ≥300 DPI, and total ink coverage stays at TAC ≤280%–300% in a valid PDF/X-1a or PDF/X-4 export.

Concrete Failure Modes

  • Cropped mask artboard: Exporting a mask sized only to the finish graphic's bounding box instead of the full trim-plus-bleed artboard shifts the entire finish out of alignment on press.
  • Accidental knockout under spot UV: Leaving a clear finish mask set to knock out removes the CMYK ink underneath, exposing bare card stock around the edge of the gloss area if registration shifts.
  • Zero-allowance butt fit on foil or white ink: Stopping adjacent CMYK ink at the exact vector line of an opaque foil or white mask without the supplied registration allowance leaves a visible bare gap during normal press or die movement.
  • Short bleed or tight border clearance: Stopping a full-bleed mask at the trim line or placing spot accents inside the ≥4–5 mm (0.157–0.197 in) bordered-back safety zone results in un-coated edges or visibly skewed borders after R3–R3.5 mm (0.118–0.138 in) corner die cutting.
  • Excessive ink load or lamination conflict: Running TAC above 280%–300% beneath heavy spot finishes causes poor surface bonding or scuffing on dark artwork without anti-scuff matte, while pairing thick lamination with gilded edges causes edge-finishing defects.