Mask and Wrap Specifications

Parameter Specification Notes
File formats AI, PDF, PSD (PDF/X-1a or PDF/X-4) Outlined or embedded fonts; ≥300 DPI for raster elements
Color & separations CMYK + separate spot mask layer Set spot mask to 100% solid on an overprinting spot channel
Wrap sheet bleed 3 mm (0.118 in) per side Applies to CMYK wrap artwork on the outer perimeter
Turn-in wrap margin 15–20 mm (0.591–0.787 in) Keep holographic transfer masks completely out of turn-ins
Panel safety & fold clearance ≥3 mm (0.118 in) from fold/trim Step masks back from 90-degree fold lines and corner-fold tabs
Greyboard core thickness 1.5 / 2 / 2.5 / 3 mm (0.059 / 0.079 / 0.098 / 0.118 in) Thicker board increases wrap fold radius and corner-tab bulk
Black & ink density 100% K fine text; rich black C40–60 M30–40 Y30–40 K100 Total area coverage (TAC) ≤280%–300%

Keep holographic transfer film off 90-degree creases and 15–20 mm (0.591–0.787 in) turn-ins because bending the cured transfer layer at sharp wrap angles stresses the film and adhesive bond. See Holographic Transfers for Rigid Boxes and Booster Packs for the full finishing behavior at folds and turn-ins.

Preparation Steps

  1. Lock the rigid box wrap dieline first. Confirm the greyboard caliper—1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in)—so the 90-degree fold lines, corner-fold cutouts, and 15–20 mm (0.591–0.787 in) turn-in margins match the final board-wrapping geometry.
  2. Isolate the holographic mask on a dedicated spot layer. Place all holographic elements as 100% solid vector shapes on a named spot channel separate from CMYK, white ink, or other specialty masks. Set the spot layer to overprint so underlying CMYK ink does not knock out and expose paper edges under registration tolerance.
  3. Apply corner-fold and edge clearances. Offset the holographic mask inward by at least 3 mm (0.118 in) from every 90-degree fold line and keep all mitered corner-fold tabs and 15–20 mm (0.591–0.787 in) turn-ins 100% clear of transfer coverage.
  4. Align pattern orientation across lid and side panels. On flat-sheet wraps where a directional holographic pattern (linear, brushed, or grating) spans the top lid and adjacent side aprons, mark the primary grain or pattern direction on a non-printing guide layer. Keep the lid and side-panel artwork oriented consistently relative to the sheet feed direction so folded side walls do not display mismatched light refraction.
  5. Preflight and export. Confirm 3 mm (0.118 in) outer bleed on the CMYK wrap artwork, ≥300 DPI on any raster art, 100% K for fine text, rich black at C40–60 M30–40 Y30–40 K100, and TAC ≤280%–300%. Export as PDF/X-1a or PDF/X-4 with fonts outlined or embedded.

Sign-Off Criteria

  • The holographic transfer mask resides on a single, clearly named spot vector layer set to overprint, separate from CMYK and white-ink plates.
  • Every mask shape sits strictly inside the flat lid or side-panel face with ≥3 mm (0.118 in) clearance from 90-degree fold lines, corner-fold tabs, and 15–20 mm (0.591–0.787 in) turn-in margins.
  • Pattern orientation across the lid and any side-apron panels is locked and documented on the dieline layer.
  • PDF/X-1a or PDF/X-4 separation previews show clean spot separation, 3 mm (0.118 in) outer wrap bleed, ≥300 DPI raster resolution, and TAC ≤280%–300%.

Concrete Failure Modes

  • Seam splitting at 90-degree folds: Extending the holographic mask across a score line causes the transfer layer to fracture or peel along the box edge when wrapped around 1.5–3 mm (0.059–0.118 in) greyboard.
  • Corner-tab and turn-in delamination: Allowing transfer film into the 15–20 mm (0.591–0.787 in) turn-in or mitered corner folds interferes with wrap adhesive bonding to the board, lifting the corner flaps.
  • Mismatched shimmer across folded aprons: Rotating side-panel artwork 90 degrees on the flat wrap sheet without accounting for directional holographic patterns produces uneven visual contrast between the lid face and side walls.
  • Registration haloing around spot art: Leaving the spot mask set to knockout instead of overprint exposes a thin white paper gap between the transfer edge and adjacent rich black (C40–60 M30–40 Y30–40 K100) backgrounds.