On dual-layer boards, the top sheet is printed, laminated, and spot-UV coated as a flat wrap before steel-rule die-cutting punches out the recessed wells and mounts the top layer onto the solid base board. Placing UV resin across a die-cut line causes the blade to fracture the cured coating, while placing UV on the base sheet interferes with adhesive bonding in the lamination zones.
Conditions that change this approach:
- Dark or high-ink artwork: Pair flat spot UV with an anti-scuff matte film base rather than standard gloss laminate so the varnish retains visual contrast and dark backgrounds resist rubbing during assembly.
- Full-wrap vs. flush-cut edges: If the top printed sheet wraps around the greyboard edge, stop the spot UV mask before the outer fold line so cured varnish does not crack along the 90-degree crease.
- Recessed floor graphics: Leave the base-layer cutout floors in matte or uncoated finish rather than spot UV; varnish inside small wells creates uneven friction for tokens and tiles.
Specifications and Tolerances
For general spot-varnish channel rules, see spot UV masks. Dual-layer boards add cutout and glue-zone clearances to those baseline prepress specs.
| Parameter | Specification | Notes |
|---|---|---|
| File format | PDF/X-4 or PDF/X-1a (from AI, PDF, or PSD) |
Fonts outlined or embedded; dieline on a non-printing spot layer |
| Image resolution | >=300 DPI |
Applies to all raster CMYK artwork beneath the mask |
| Color & ink limits | CMYK + 100% K spot plate (Spot_UV) |
Fine text 100% K; rich black C40–60 M30–40 Y30–40 K100; TAC <=280%–300% |
| Spot UV mask geometry | Pure vector, 100% solid fill, overprint on |
No gradients, soft feathers, or halftones |
| Bleed & safety | 3 mm (0.118 in) bleed per side; >=3 mm (0.118 in) safety |
Keep fine UV details inside the safety zone |
| Greyboard & wrap margin | 1.5 / 2 / 2.5 / 3 mm (0.059 / 0.079 / 0.098 / 0.118 in) board; 15–20 mm (0.591–0.787 in) wrap margin |
Keep spot UV completely out of the wrap margin and fold creases |
| Cutout & glue-zone clearance | Pulled back from all internal cutout dielines and base contact faces | Prevents die-cut chipping and glue-bond failure |
Production Steps for Dual-Layer Spot UV Files
- Separate top and base artboards: Export the top-layer face and the base-layer sheet as distinct print files aligned to the same master dieline.
- Isolate the
Spot_UVlayer on the top file only: Create a dedicated top-level layer using a single spot-color swatch namedSpot_UV(100%tint) and set every mask object to Overprint Fill (and Overprint Stroke, if any strokes remain). - Pull back from cutout windows and fold lines: Offset all
Spot_UVshapes inward away from every internal cutout window path and away from the outer trim or15–20 mm(0.591–0.787 in) wrap crease so the die blade only cuts through paper and laminate. - Clear the base-layer file: Remove all
Spot_UVobjects from the base-layer artboard so the entire lamination glue zone remains bare paper or laminate-free board surface for clean adhesive penetration. - Flatten and export: Convert any stroked mask paths to closed compound shapes, verify that the dieline layer is set to non-printing, and export as
PDF/X-4orPDF/X-1a.
Prepress Sign-Off Criteria
Before releasing the job to plate and screen/digital UV setup, inspect the exported PDF in Output Preview (separation view):
- Single spot plate: Only one
Spot_UVseparation appears alongside CMYK (plus the non-printing dieline). - Overprint verified: Toggling
Spot_UVoff leaves the underlying CMYK artwork continuous with zero white knockout shapes beneath the varnish. - Clean cutout and wrap zones: Zooming into every recessed window dieline and outer wrap fold shows a clear gap between the
Spot_UVedge and the cut/fold path. - Base layer clear: The base-layer PDF contains zero
Spot_UVink anywhere on the sheet. - Color compliance: CMYK totals remain at
TAC <=280%–300%, fine text separates cleanly on the100% Kplate, and all fonts are outlined or embedded.
Failure Modes
- Chipped varnish around cutout windows: Extending
Spot_UVto or across a recessed window path causes the steel-rule die to crush and flake the cured resin, leaving jagged edges around token wells. Pull the mask back from every internal cutout line. - Top-to-base delamination: Placing spot UV on the base layer's bonding surface blocks glue from penetrating the paper fibers, causing the top layer to bubble or lift around cutouts. Keep
Spot_UVstrictly off the base-layer file and glue zones. - White halos around glossy elements: Leaving
Spot_UVset to knockout instead of overprint punches a white hole in the CMYK plates, exposing unprinted paper if UV registration shifts. Set allSpot_UVobjects to overprint. - Cracked UV on board edges: Running the mask into the
15–20 mm(0.591–0.787 in) wrap margin forces cured UV resin to bend 90 degrees around the greyboard edge, cracking the coating during wrapping. Stop the mask before the outer fold crease. - Soft edges or scuffed dark areas: Exporting rasterized masks or applying UV over standard gloss film instead of anti-scuff matte laminate produces fuzzy edges and visible rub marks on dark boards. Use sharp vector shapes over an anti-scuff matte base.
Parent guide Flat Spot UV Varnish Mask Setup