This choice changes under four physical conditions:

  • Structural load vs. punchability: Heavy game boards or large rigid boxes often require 2.5 mm (0.098 in) or 3 mm (0.118 in) greyboard to resist warping, whereas dense punchboards with small tokens cut cleaner on 1.5 mm (0.059 in) or 2 mm (0.079 in) board.
  • Shuffle durability vs. rigid dividers: Playing cards that are shuffled repeatedly need core-stock snap—such as 300 gsm blue core, 310 gsm black-core linen, or 330 gsm black core—while static reference cards and dividers can share 350 gsm or 400 gsm art stock without core opacity.
  • Edge finishing conflicts: Thick film lamination adds 0.03–0.05 mm (0.001–0.002 in) per card and can conflict with gilded edges, so gilded decks cannot share the same heavy lamination pass as un-gilded dividers or reference sheets.
  • Box volume and freight limits: Stepping all greyboard parts up to a thicker caliper increases total stack height and carton mass in kg (lb), which can force a deeper box or push a shipment across a weight tier.

For broader component-grouping strategies beyond material selection, see Shared Parts and Consolidation.


Substrate, Caliper, and Coating Specifications

Specify all paper stocks in grams per square meter (gsm) rather than US pound weights alone. US Text LB is measured on a 25 × 38 in (635 × 965 mm) basis sheet, whereas US Cover LB is measured on a 20 × 26 in (508 × 660 mm) basis sheet; an identical pound rating represents a substantially heavier and thicker sheet in Cover LB than in Text LB. Using gsm alongside target caliper prevents stock mismatches when unifying cards, dividers, booklet covers, and board wraps.

Paper Stock and Caliper Reference

Component Group Material / Grade Weight (gsm) Approximate Caliper Typical Consolidation Role
Standard cards Art / blue core 300 gsm 0.28–0.31 mm (0.011–0.012 in) Main decks and reference cards
Textured cards Black-core linen 310 gsm 0.30–0.32 mm (0.012–0.013 in) Linen-embossed decks and player aids
Heavy core cards Black core 330 gsm 0.32–0.34 mm (0.013 in) High-opacity decks and dividers
Rigid flat cards Art stock 350 gsm 0.34–0.38 mm (0.013–0.015 in) Reference cards, dividers, thin inserts
Extra-rigid flat cards Art stock 400 gsm 0.40–0.44 mm (0.016–0.017 in) Thick dividers and heavy tuck/cardboard inserts
Plastic cards PVC — 0.30 mm (0.012 in) Waterproof decks (cannot share paper gang runs)
Booklet interior Uncoated / matte text 80–120 gsm 0.08–0.13 mm (0.003–0.005 in) per sheet Rulebooks (saddle stitch 12–40 pp, perfect 28+, sewn 80–100+ pp) and 4/6/8-panel leaflets
Booklet covers Cover / art stock 200–300 gsm ~0.20–0.31 mm (0.008–0.012 in) Self-cover or shared wrap/insert press sheet

Double-sided film lamination adds 0.03–0.05 mm (0.001–0.002 in) per card. Anti-scuff matte lamination suits dark artwork where surface rubbing would otherwise show scuff marks during packing and play.

Greyboard and Mounting Specifications

Parameter Standard Range (mm) Inch Equivalent (in) Consolidation Constraint
Greyboard calipers 1.5 / 2 / 2.5 / 3 mm 0.059 / 0.079 / 0.098 / 0.118 in Boards, punchboards, and rigid box walls
Board wrap margin 15–20 mm 0.591–0.787 in Paper wrap allowance per edge around greyboard
Punchboard die gap 3–4 mm 0.118–0.157 in Minimum spacing between die-cut tokens/tiles
Box width/height clearance 1.5–2.5 mm 0.059–0.098 in Internal room around unified component stacks
Box stack-height clearance 1.5–3 mm 0.059–0.118 in Vertical allowance for combined boards, tiles, and decks

Prepress and Tolerance Standards

  • File formats and color: Supply AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 with fonts outlined or embedded. Build artwork in CMYK with separate spot layers for specialty finishes.
  • Resolution and ink density: Use ≥300 DPI raster assets. Set fine text to 100% K, rich black solids to C40–60 M30–40 Y30–40 K100, and keep Total Area Coverage (TAC) at ≤280%–300%.
  • Bleed, safety, and corners: Allow 3 mm (0.118 in) bleed per side, ≥3 mm (0.118 in) safety margin (≥4–5 mm / 0.157–0.197 in for bordered backs), and R3–R3.5 mm (0.118–0.138 in) corner radii on standard rounded cards.
  • Stack-height and weight formulas:
    • Total Stack Height (mm) = (Card Count × (Base Caliper + Lamination Allowance)) + (Board Count × Greyboard Caliper)
    • Total Stack Height (in) = Total Stack Height (mm) / 25.4
    • Target Inner Box Depth (mm) = Total Stack Height (mm) + 1.5 to 3.0 mm
    • Master Carton Weight (lb) = Master Carton Weight (kg) × 2.20462

Job-Specific Consolidation Steps

  1. Audit component roles against physical requirements. Separate parts that must flex and shuffle (decks) from parts that must stay flat and rigid (boards, punchboards, dividers, box trays). Keep decks on a single core stock (300–330 gsm) and group static reference cards or dividers onto the same sheet if they share the deck's trim and finish.
  2. Lock one shared greyboard caliper where tolerances align. Select 2 mm (0.079 in) greyboard as the baseline when unifying game boards and punchboard tokens, or 1.5 mm (0.059 in) when small, intricate token dies dominate. Only split to 2.5 mm (0.098 in) or 3 mm (0.118 in) if an oversized folding board or heavy rigid box wall requires extra stiffness.
  3. Align paper wraps, booklet covers, and inserts. Match board wrap sheets and box wraps to the same coated art stock and lamination finish (such as anti-scuff matte for dark designs) so press makeready and coating runs are shared. If a booklet cover uses 200–300 gsm stock, align it with existing flat-insert runs when quantities match.
  4. Gang layouts and verify die and box clearances. Check that punchboard layouts maintain a 3–4 mm (0.118–0.157 in) die gap and that wrapped boards retain a 15–20 mm (0.591–0.787 in) wrap margin. Recalculate total stack height with lamination included and confirm 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) stack-height clearance inside the box.
  5. Validate prepress and compliance test groupings. Confirm all unified sheets obey TAC ≤280%–300%, 100% K fine text, and separate spot layers. Where products require toy-safety assessment and testing under EN 71, consolidating onto fewer distinct paper stocks, greyboard calipers, and coatings reduces the number of separate substrate and finish combinations documented for laboratory testing.

Sign-Off Criteria

Before releasing unified files to production, verify the following on physical white dummies and press/digital proofs:

  • Caliper and stack-height fit: Measure a full assembled stack of laminated cards, punchboards, and folded boards with a micrometer or caliper gauge; confirm the stack fits inside the box with 1.5–3 mm (0.059–0.118 in) vertical clearance and 1.5–2.5 mm (0.059–0.098 in) lateral clearance.
  • Punchboard release and edge integrity: Test die-cut tokens on the chosen greyboard caliper to confirm clean punch-out without tearing the 3–4 mm (0.118–0.157 in) bridges or delaminating the 15–20 mm (0.591–0.787 in) wrap edges.
  • Finish and color consistency: Inspect dark-ink panels under anti-scuff matte lamination and verify that shared stocks (such as 300 gsm cards and 300 gsm dividers) hold consistent ink density within TAC ≤280%–300% without set-off.
  • Lot-level AQL and carton weight check: Confirm final master carton gross weight in kg and lb against pallet and carrier limits before locking the packaging spec.

Concrete Failure Modes

  • Stack-height overflow from uncounted film: Calculating box depth from raw 300–350 gsm stock caliper alone and omitting the 0.03–0.05 mm (0.001–0.002 in) double-sided film allowance adds up to 3–5 mm (0.118–0.197 in) across a 100-card deck, eliminating the 1.5–3 mm (0.059–0.118 in) box clearance and causing lid lift.
  • Die-bridge tearing on oversized calipers: Running small, closely spaced punchboard tokens on 2.5–3 mm (0.098–0.118 in) greyboard with less than a 3–4 mm (0.118–0.157 in) die gap crushes the paper wrap and leaves ragged greyboard fibers when punched.
  • Gilded-edge delamination on laminated cards: Grouping gilded decks with heavily laminated dividers on the same thick film pass causes poor foil adhesion or edge peeling during gilding.
  • Ink set-off and scuffing on ganged runs: Combining heavy rich-black dark artwork (exceeding TAC 300%) with lighter uncoated or unlaminated inserts on a single press sheet leads to ink transfer in the pile and visible scuffing if anti-scuff matte lamination is omitted.
  • Basis-weight mismatch between US Text LB and Cover LB: Ordering "80 lb" stock across a rulebook interior and a divider without specifying gsm can mix 80 lb Text (~118 gsm) with 80 lb Cover (~216 gsm), breaking both signature folding (multiples of 4) and box stack height.