The exact allowance depends on greyboard caliper, hinge count, and whether the component is wrapped or die-cut from a mounted sheet. Thicker 2.5 to 3 mm (0.098 to 0.118 in) greyboard requires the upper end of the 15 to 20 mm (0.59 to 0.79 in) wrap margin and wider fold gutters than 1.5 mm (0.059 in) board, while double-sided punchboards require full horizontal mirroring of the back-sheet dieline. For general prepress checks covering color profiles, resolution, and ink limits, see the parent guide on approving PDF proofs.
Structural and Prepress Specifications
Partner PDF proofs for wrapped and die-cut board components must satisfy both structural dieline tolerances and offset prepress baselines.
| Parameter | Specification (mm / in) | Application |
|---|---|---|
| Greyboard caliper | 1.5, 2, 2.5, or 3 mm (0.059, 0.079, 0.098, or 0.118 in) | Game boards, rigid box walls, punchboards |
| Wrap turn-in margin | 15 to 20 mm (0.59 to 0.79 in) | Outer perimeter past board edge on wrapped items |
| Rigid box clearance (W x H) | 1.5 to 2.5 mm (0.059 to 0.098 in) | Lid-to-base fit across width and height |
| Rigid box stack clearance | 1.5 to 3 mm (0.059 to 0.118 in) | Internal depth allowance above stacked contents |
| Punchboard die gap | 3 to 4 mm (0.118 to 0.157 in) | Minimum spacing between adjacent token cut lines |
| Bleed allowance | 3 mm (0.118 in) per side | Outer trim and internal die-cut edges |
| Safety margin | >=3 mm (0.118 in) | Distance from text/icons to trim, creases, and cuts |
| PDF standard & resolution | PDF/X-1a or PDF/X-4, >=300 DPI | Partner soft-proof export |
| Color & ink limits | CMYK + separate spot layers; TAC <=280%–300% | Rich black C40–60 M30–40 Y30–40 K100; 100% K fine text |
When dark solid artwork wraps around board edges or box corners, anti-scuff matte lamination prevents rubbing marks during wrapping and transit.
Job-Specific Proofing Steps
1. Verify Wrap-Allowance and Turn-In Geometry
Wrapped game boards and rigid boxes use printed liner sheets mounted over greyboard and folded around the edges.
- Confirm the printed wrap artwork extends 15 to 20 mm (0.59 to 0.79 in) past the outermost greyboard score or trim line on all sides.
- Check that corner miters or notched flaps on rigid box dielines leave clean overlap without exposing bare greyboard corners when folded.
- Keep borders, rules, and logos at least 3 mm (0.118 in) inside the finished board face or box panel edge so wrap tension does not pull graphics onto the side wall.
2. Check Fold-Hinge and Crease-Line Clearances
Folding game boards and rigid box walls bend along scored channels where the liner paper bridges a gap between greyboard panels.
- Toggle the separate spot-color dieline layer on and inspect every crease and hinge line at high zoom.
- Confirm all text, small icons, and thin keylines sit at least 3 mm (0.118 in) clear of hinge lines.
- On two-piece rigid boxes, verify that side-panel graphics align with the 90-degree fold lines and that the box dimensions include 1.5 to 2.5 mm (0.059 to 0.098 in) width/height clearance and 1.5 to 3 mm (0.059 to 0.118 in) stack-height clearance.
3. Audit Front-to-Back Die Mirroring
Double-sided game boards and punchboards are printed as separate front and back sheets before mounting and die-cutting.
- Compare the front-sheet proof and back-sheet proof with the dieline spot layer visible on both.
- Confirm the back-sheet dieline is horizontally mirrored relative to the front-sheet dieline so asymmetrical tokens, thumb notches, and board hinges register when the sheet is flipped.
- Verify that 3 mm (0.118 in) bleed extends past every token cut line and outer perimeter on both the front and back sheets.
4. Inspect Die Spacing and Nick-Mark Placement
Punchboards rely on steel-rule dies to cut tokens through mounted greyboard while leaving small uncut paper bridges (nicks) that hold pieces in the frame until punched out.
- Measure the waste skeleton between adjacent token cut lines and confirm a 3 to 4 mm (0.118 to 0.157 in) gap throughout the sheet.
- Locate nick-mark indicators on the dieline layer and confirm they sit on straight edges or low-detail areas rather than sharp corners or fine text.
- Verify that large or heavy tokens have balanced nick placement on opposing sides so pieces do not drop loose during packing and freight.
Sign-Off Criteria
Approve the partner PDF proof only when all structural and prepress checks pass:
- PDF/X-1a or PDF/X-4 file opens with all fonts outlined or embedded, >=300 DPI raster art, and TAC <=280%–300%.
- Dielines, crease lines, and finishing effects sit on separate, overprint-enabled spot-color layers rather than flattened into CMYK.
- Wrap turn-in allowances measure 15 to 20 mm (0.59 to 0.79 in) beyond the greyboard perimeter.
- Text and critical graphics maintain >=3 mm (0.118 in) clearance from all creases, hinges, and cut lines.
- Back-sheet dielines on double-sided boards and punchboards are horizontally mirrored to match the front sheet, with 3 mm (0.118 in) bleed around every cut.
- Punchboard tokens maintain 3 to 4 mm (0.118 to 0.157 in) die spacing with nick marks positioned off corners and typography.
Concrete Failure Modes
- Exposed greyboard corners and edges: Wrap turn-ins narrower than 15 mm (0.59 in) or undersized for 2.5 to 3 mm (0.098 to 0.118 in) greyboard pull short during wrapping, leaving raw board visible along box edges or board backs.
- Cracked ink and warped text at hinges: Placing dense rich black above 280%–300% TAC or small typography within 3 mm (0.118 in) of a board fold causes ink cracking and visible distortion across the hinge channel.
- Mirrored back-sheet misregistration: Failing to mirror the dieline on the reverse sheet shifts asymmetrical punchboard tokens and double-sided board art off-center, slicing into reverse-side borders or icons.
- Crushed waste matrix or torn token faces: Die gaps narrower than 3 mm (0.118 in) collapse the greyboard skeleton under steel-rule pressure; nicks placed on sharp corners tear the printed liner when punched out, whereas omitted nicks let tokens fall out during transit.
Parent guide PDF Proof Review and Sign-Off