This approach changes based on three production conditions:
- Unchanged reprint vs. expansion pack: A straight reprint reuses the original prepress plates and imposition, whereas an expansion pairs new card faces with the archived card-back file and requires fresh plate verification against the base run.
- Paper mill or finish continuity: Switching paper mills, core constructions, or surface coatings alters the sheet's white point, specular glare, and thickness, requiring wet press proofing on the replacement stock rather than relying on digital proofs.
- Bordered vs. full-bleed card backs: Bordered backs expose minor die-cut or registration drift in a shuffled stack and require at least 4–5 mm (0.157–0.197 in) safety margins, compared to 3 mm (0.118 in) for full-bleed layouts.
For broader stage gates and initial first-edition sign-offs, see the proofing overview.
Matching Specifications and Tolerance Targets
Standard offset card runs start at 200 decks (with usual production tiers at 200, 300, 500, and 1,000+ decks). To keep repeat runs and expansions visually and physically uniform when shuffled into an existing base game, lock these specifications to the archived job ticket:
| Parameter | Target Specification | Matching Requirement |
|---|---|---|
| Prepress & Color | AI/PDF/PSD exported as PDF/X-1a or PDF/X-4; ≥300 DPI; CMYK with separate spot layers | Lock the archived card-back separation; keep fine text at 100% K, rich black at C40–60 M30–40 Y30–40 K100, and total area coverage (TAC) ≤280%–300%. |
| Stock & Caliper | 300 gsm art/blue core: 0.28–0.31 mm (0.0110–0.0122 in) 310 gsm black-core linen: 0.30–0.32 mm (0.0118–0.0126 in) 330 gsm black core: 0.32–0.34 mm (0.0126–0.0134 in) 350 gsm art stock: 0.34–0.38 mm (0.0134–0.0150 in) 400 gsm: 0.40–0.44 mm (0.0157–0.0173 in) PVC: 0.30 mm (0.0118 in) |
Match exact gsm and core type. When referencing US paper weights, distinguish US Text LB (25 × 38 in basis sheet) from US Cover LB (20 × 26 in basis sheet) instead of matching pound numbers across different basis sizes. |
| Surface Finish | Double-sided film adds 0.03–0.05 mm (0.0012–0.0020 in) per card | Keep coating chemistry identical; anti-scuff matte suits dark artwork, while thick lamination conflicts with gilded edges. |
| Bleed & Die-Cut | 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) safety (≥4–5 mm / 0.157–0.197 in for bordered backs); R3–R3.5 mm (R0.118–R0.138 in) corners | Maintain identical trim dimensions and corner-die radius so mixed cards do not protrude when squared. |
Job-Specific Proofing and Approval Steps
- Retrieve the base-edition golden sample and job ticket. Pull uncirculated cards from the original production run (stored away from UV light and high humidity) along with the archived PDF/X-1a or PDF/X-4 press files, stock gsm, core type, finish spec, and corner-die record.
- Lock the card-back master file. For expansion packs, place new card-face artwork onto the layout while keeping the original card-back CMYK values, spot layers, and outlined or embedded fonts untouched.
- Pull wet press proofs on the production stock. Digital inkjet proofs do not reproduce offset dot gain, core tint, or film sheen. Evaluate press sheets printed on the exact target stock and coated with the specified varnish or double-sided film.
- Run a blind mix test under neutral lighting. Shuffle cut press samples face-down into the archived base-edition deck under neutral D50/D65 light. Inspect card-back hue, sheen angle, border centering, and corner alignment from both flat and raking angles.
- Measure caliper and archive the new golden sample. Record micrometer readings across multiple finished cards and verify total deck stack height against existing box clearances (1.5–2.5 mm / 0.059–0.098 in across width and height, and 1.5–3 mm / 0.059–0.118 in for stack height). Seal approved samples from the repeat or expansion run for future reorders.
Sign-Off Criteria
Approve the repeat run or expansion press sample only when all three conditions hold:
- Face-down invisibility: Shuffled expansion or reprint cards show no detectable hue shift, sheen mismatch, or border asymmetry against the base-edition golden sample.
- Caliper and stack parity: Single-card thickness (base stock plus any 0.03–0.05 mm / 0.0012–0.0020 in double-sided film) falls within the archived base stock's tolerance band so combined decks fit existing boxes and trays.
- Edge and corner alignment: Trimmed edges and R3–R3.5 mm (R0.118–R0.138 in) corners sit flush in a squared deck with no stepped overhang.
Concrete Failure Modes
- Approving from a digital contract proof: Digital proofing paper lacks the tint of blue-core or black-core card stock and the specular response of matte or linen finishes, masking color shifts that appear on press.
- Re-separating card-back artwork: Re-exporting the card back through a different CMYK ICC profile or altering rich black (C40–60 M30–40 Y30–40 K100) changes ink density on dark backs, effectively marking expansion cards in a shuffled deck.
- Swapping finish or film thickness mid-series: Moving from a press varnish to double-sided film adds 0.03–0.05 mm (0.0012–0.0020 in) per card, changing card stiffness, surface friction, and total stack height.
- Tight safety margins on bordered backs: Leaving less than 4–5 mm (0.157–0.197 in) safety on a bordered card back turns normal die-cut variance into visible uneven borders when mixed with base-edition cards.
- Mismatched corner-cutting dies: Cutting an expansion within a slightly different R3–R3.5 mm (R0.118–R0.138 in) die profile than the base run leaves sharp corner steps along the edges of a squared deck.
Parent guide Production Proofs and Sample Approval